Potters Industries Conduct-O-Fil® SA300S30 Silver-coated Aluminum Granules

Category Metal , Nonferrous Metal , Aluminum Alloy , Other Engineering Material , Additive/Filler for Polymer
Manufacturer Potters Industries
Trade Name Conduct-O-Fil®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Potters Industries Conduct-O-Fil® SA300S30 Silver-coated Aluminum Granules.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Applications:EMI shielding in contact with aluminumConductive adhesivesAerospace and marine applicationsAdvantages:Low density with high conductivityLow galvanic corrosion in contact with aluminumInformation provided by Potters Industries.
Physical Properties Metric English Comments
Particle Size 40 µm
40 µm
Average Diameter
Component Elements Properties Metric English Comments
Silver, Ag 30 %
30 %
by weight