Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | >= 0.50 µm | >= 0.50 µm | Primary Crystal Size |
Nabaltec NABALOX® NO 313 Ground Alumina NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula.. |
|||
Particle Size | 0.50 µm | 0.50 µm | 52% of particles less than |
Old Hickory 44-B Kentucky Ball Clay The 44-B clay is similar to 54-S and is a recommended selection where additional plasticity and strength are important. It is particularly recommended in extruded and plastic processed ceramic formu.. |
|||
Particle Size | 0.50 µm | 0.50 µm | 40% of particles less than |
Old Hickory FC-340 Tennessee Ball Clay The FC-340 clay is designed for all types of casting formulas ranging from low fire earthenware to vitreous composition. It has excellent response to deflocculation and a very good casting rate whil.. |
|||
Particle Size | 0.50 µm | 0.50 µm | 21.8% of partciles less than |
Old Hickory M&M Clays, Inc. Wilco-LPC Kaolin Clay Wilco LPC is the same selection as the SLU grade except it is in natural shredded or Airfloat (powdered) form. It offers the same benefits in a ceramic casting formulation discussed above for the SL.. |
|||
Particle Size | 0.50 µm | 0.50 µm | 43% of particles less than |
Old Hickory No. 28 Kentucky Ball Clay This is a kaolin grade with exceptional plasticity, dry and green strength, and low levels of carbon content. it can be utilized in extruded or pressed ceramic formulations and is a clay particularl.. |
|||
Particle Size | 0.50 µm | 0.50 µm | 56% of particles less than |
Old Hickory Taylor Blend Tennessee Ball Clay A highly plastic clay suitable for a variety of extruded, pressed, or casting ceramic formulations. It is a fine PSD clay with low carbon content and excellent fired brightness.Information provided .. |
|||
Particle Size | 0.50 µm | 0.50 µm | 29% of particles less than |
Old Hickory UltraCast Slurry PC-2000 Kentucky Ball Clay These popular slurry grades are shipped at 60% solids content and deflocculated with sodium silicate to maintain stable rheology characteristics. All the above grades are suitable for a variety of c.. |
|||
Particle Size | 0.50 µm | 0.50 µm | 52% of particles less than |
Old Hickory Volunteer Tennessee Ball Clay A versatile clay selection for casting, pressing, or plastic forming process methods. It is similar to M-23 in mineralogy with slightly more organic content. Volunteer has very good plasticity and i.. |
|||
Particle Size | 0.50 - 1.5 µm | 0.50 - 1.5 µm | D<sub>50</sub> |
NYC YT3CP Y2O3 Powder |
|||
Particle Size | 0.50 µm | 0.50 µm | 31% of particles less than |
Old Hickory UltraCast Slurry PC-2034 Kentucky Ball Clay These popular slurry grades are shipped at 60% solids content and deflocculated with sodium silicate to maintain stable rheology characteristics. All the above grades are suitable for a variety of c.. |
|||
Particle Size | 0.50 - 1.0 µm | 0.50 - 1.0 µm | D<sub>50</sub> |
NYC YT3WP Y2O3 Granules |
|||
Particle Size | 0.50 µm | 0.50 µm | 71.5% finer than |
Imerys Aftonâ„¢ Kaolin Afton is a fine-grained air floating kaolin which is widely used as an anit-caking agent in certain agricultural compounds.Information provided by Imerys |
|||
Particle Size | 0.50 µm | 0.50 µm | 71.5% finer than |
Imerys Aftonâ„¢ R Kaolin Afton is a fine-grained kaolin used asa a filler in hard rubber products, plastic products, adhesives, protective coatings and similar applications.Information provided by Imerys |
|||
Particle Size | 0.50 µm | 0.50 µm | 28% finer than |
Imerys Allenâ„¢ G Kaolin Allen G is an intermediate-grained kaolin used as a suspension aid in ceramic glazes.Information provided by Imerys |
|||
Particle Size | 0.50 µm | 0.50 µm | 28% finer than |
Imerys Allenâ„¢ R Kaolin Allen is an intermediate-grained kaolin suitable for use as a filler in soft rubber products, plastic compounds, adhesives, protective coatings and similar applications.Information provided by Imery.. |
|||
Particle Size | 0.50 µm | 0.50 µm | 72% finer than |
Imerys Amlockâ„¢ 321 Kaolin Information provided by Imerys |
|||
Particle Size | 0.50 µm | 0.50 µm | 45% finer than |
Imerys Carverâ„¢ Kaolin Information provided by Imerys |
|||
Particle Size | 0.50 µm | 0.50 µm | 27% finer than |
Imerys DB-Floatâ„¢ Kaolin Information provided by Imerys |
|||
Particle Size | 0.50 µm | 0.50 µm | 38% finer than |
Imerys Diamondâ„¢ Kaolin Diamond is an intermediate-grained montmorillonitc kaolin used primarily in plastic formed bodies. This kaolin is known for its good strength and white-firing characteristics.Information provided by.. |
|||
Particle Size | 0.50 µm | 0.50 µm | 23% finer than |
Imerys Kaolin Slurryâ„¢ Kaolin Slurry is a carefully controlled Kaolin-water suspension formulated for use in cermic castings.Information provided by Imerys |
|||
Particle Size | 0.50 µm | 0.50 µm | 30% finer than |
Imerys KT-Cast/Rogersâ„¢ Kaolin Information provided by Imerys |
|||
Particle Size | 0.50 µm | 0.50 µm | 72% finer than |
Imerys Mercapâ„¢ 100 Kaolin Information provided by Imerys |
|||
Particle Size | 0.50 µm | 0.50 µm | Mean |
Momentive Performance Materials AC6111 Boron Nitride (BN) Powder Agglomeration of submicron hexagonal turbostatic crystals. Used in paints, refractory coatings, mold/die release agents, nucleation aid, and lubricants. It is relatively non-wetting versus molten .. |
|||
Particle Size | 0.50 µm | 0.50 µm | |
Shin-Etsu Silicones X-52-2328 Fluid Information Provided by Shin-Etsu Silicones of America, Inc. |
|||
Particle Size | 0.50 - 1.0 µm | 0.50 - 1.0 µm | D50 Sedigraph |
Solvay Polishing Opaline™ Description: Polishing OPALINE® is a high quality cerium oxide powder developed high precision polishing. It has an excellent surface quality, very low roughness, and has quality consistency. The.. |
|||
Particle Size | 0.50 - 25 µm | 0.50 - 25 µm | PSD (d<sub>50</sub> |
Terio Corporation TZY-10 Yttria Stabilized Zirconia Information provided by TERIO Corporation. |
|||
Particle Size | 0.50 - 25 µm | 0.50 - 25 µm | PSD (d<sub>50</sub> |
Terio Corporation TZY-8 Yttria Stabilized Zirconia Information provided by TERIO Corporation. |
|||
Particle Size | 0.50 - 25 µm | 0.50 - 25 µm | PSD (d<sub>50</sub> |
Terio Corporation TCZA-20~80 CeO2-Al2O3-ZrO2 Information provided by TERIO Corporation. |
|||
Particle Size | 0.50 µm | 0.50 µm | |
Astro Met AmZirOx 86 Zirconia - Zirconium Oxide General Description:AmZirOx 86 zirconia (Astro Met Zirconium Oxide) is a yttria stabilized zirconia ceramic material which features high strength and toughness making it a candidate material for use.. |
|||
Particle Size | 0.50 µm | 0.50 µm | 55% of particles less than |
Old Hickory TI-21 Tennessee Ball Clay TI-21 is a very low carbon content clay specifically designed for plastic forming methods. It has excellent oxidation qualities particularly for dense volume stoneware or vitreous ceramic pieces. Th.. |