Terio Corporation TZY-8 Yttria Stabilized Zirconia

Category Ceramic , Oxide , Zirconium Oxide
Manufacturer Terio Corporation
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Terio Corporation TZY-8 Yttria Stabilized Zirconia.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Information provided by TERIO Corporation.
Physical Properties Metric English Comments
Particle Size 0.50 - 25 µm
0.50 - 25 µm
PSD (d<sub>50</sub>
Specific Surface Area 6.0 - 15 m²/g
6.0 - 15 m²/g
Component Elements Properties Metric English Comments
Y2O3 13 - 14 %
13 - 14 %
ZrO2 86.5 %
86.5 %