Material Notes:
NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insulationhigh mechanical strengthhigh temperature propertiesdimensional accuracyoptimized chemical resistanceRefractory Industry, Wear-resistant ceramics
Physical Properties Metric English Comments
Bulk Density 0.600 - 0.800 g/cc
0.0217 - 0.0289 lb/in³
Density 2.05 g/cc
0.0741 lb/in³
Green Density
3.67 g/cc
0.133 lb/in³
Sintered Density
3.90 g/cc
0.141 lb/in³
Loss On Ignition <= 1.00 %

@Temperature 20.0 - 1100 °C
<= 1.00 %

@Temperature 68.0 - 2010 °F
Particle Size >= 0.50 µm
>= 0.50 µm
Primary Crystal Size
2.0 µm
2.0 µm
Median Grain Diameter
Specific Surface Area 8.0 - 12 m²/g
8.0 - 12 m²/g
BET
Thermal Properties Metric English Comments
Shrinkage 20 %
20 %
Sintering Shrinkage
Component Elements Properties Metric English Comments
Al2O3 >= 99.6 %
>= 99.6 %
Fe2O3 0.030 %
0.030 %
Na2O 0.30 %
0.30 %
SiO2 0.030 %
0.030 %
Processing Properties Metric English Comments
Sintering Temperature 1750 °C
3180 °F
Descriptive Properties Value Comments
alpha-Al2O3-Content % 95