Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 2.80 g/cc | 0.101 lb/in³ | |
McDanel Advanced Ceramics MV-30 Mullite Information provided by McDanel Advanced Ceramic Technologies |
|||
Bulk Density | 2.80 - 2.90 g/cc | 0.101 - 0.105 lb/in³ | After drying at 110°C |
Gouda Vuurvast CURAS 85 PD Moldable Refractory Material Description: This material is supplied as a dry powder, it has to be mixed with potable water to the necessary consistency. This phosphate bonded material based on corundum and bauxite has a very go.. |
|||
Bulk Density | 2.80 - 2.90 g/cc | 0.101 - 0.105 lb/in³ | After drying at 110°C |
Gouda Vuurvast CURAS 90 PFM Moldable Refractory Material Description: Curas 90 PFM ramming mix has outstanding abrasion properties, (erosion loss acc. ASTM C704: 2-4 cm3). In addition, it has a good resistance against thermal shock and corrosive gasses. T.. |
|||
Bulk Density | 2.80 - 2.90 g/cc | 0.101 - 0.105 lb/in³ | After drying at 110°C |
Gouda Vuurvast FLUCON 150 Dense Self Flowing Refractory Castable Description: Flucon 150 is a self-flowing low cement castable based on sintered bauxite.Remarks: These values apply to cast products.Information provided by Gouda Vuurvast. |
|||
Bulk Density | 2.80 - 2.90 g/cc | 0.101 - 0.105 lb/in³ | After drying at 110°C |
Gouda Vuurvast VIBRON 135 Dense Vibrating Refractory Castable Description: Vibron 135 is a vibrating castable, specially fit for the production of prefab elements. The very low cement content (1%) and the abrasion resistant spinel grains give this material exc.. |
|||
Bulk Density | 2.80 - 2.90 g/cc | 0.101 - 0.105 lb/in³ | After drying at 110°C |
Gouda Vuurvast VIBRON 150 Al RAPID Dense Vibrating Refractory Castable Description: Vibron 150 Al Rapid is a vibrating low cement castable resistant to liquid aluminum metal. Due to a special additive a relatively high heating rate is possible.Remarks: These values app.. |
|||
Bulk Density | 2.80 - 2.90 g/cc | 0.101 - 0.105 lb/in³ | After drying at 110°C |
Gouda Vuurvast VIBRON 150 Dense Vibrating Refractory Castable Description: Vibron 150 is a low cement castable based on sintered bauxite.Remarks: Indicated values apply to vibrated products.Information provided by Gouda Vuurvast. |
|||
Bulk Density | 2.80 g/cc | 0.101 lb/in³ | |
Minelco MagnaDense 30 Coarse Aggregate MagnaDense is a high grade natural aggregate, manufactured from the iron oxide Magnetite. With its high density MagnaDense is used as loose ballast or as aggregate to produce high quality, high dens.. |
|||
Bulk Density | 2.80 - 2.90 g/cc | 0.101 - 0.105 lb/in³ | After drying at 110°C |
Gouda Vuurvast CURAS 85 PD GM Moldable Refractory Material Description: This material is supplied as a dry powder and can be gunned. This phosphate bonded material based on corundum and bauxite has a very good resistance against slag attack or liquid alumin.. |
|||
Bulk Density | 2.80 g/cc | 0.101 lb/in³ | |
Sharadaa Ceramics HA 80SD High Alumina Brick Services Offered: Retrofitting of Furnace, Installation of Castables/Bricks/Ceramic Fiber Modules, Castable Laying by Vibrocasting/Guiniting, Turnkey Installation Boiler/Chimney/Heater/Reformer/Rota.. |
|||
Bulk Density | 2.80 g/cc | 0.101 lb/in³ | After Drying at 110°C |
Sharadaa Ceramics PCF80 Precast Prefired Brick Features: Manufactured under controlled conditions under refractory engineers supervision; Measured Quantity/Temperature of water, mixing by Intensive counter current mixers, Forming by Vibro Castin.. |
|||
Bulk Density | >= 2.80 g/cc | >= 0.101 lb/in³ | Dried at 110°C |
Sharadaa Ceramics REFCAST A High Alumina Castables Description: We bring to our clients a qualitative range of Dense Alumina Castables that are conventional castable of medium purity. These castables cater to the application needs of various industr.. |
|||
Bulk Density | >= 2.80 g/cc | >= 0.101 lb/in³ | After Drying at 110°C |
Sharadaa Ceramics VELCRETE G403 Gunning Castables Description: Available from us a range of Gunning Castables that are made in compliance with the set industrial standards. These castables are widely used in refineries, foundries, boilers, rolling .. |
|||
Bulk Density | 2.80 g/cc | 0.101 lb/in³ | After Drying at 110°C |
Sharadaa Ceramics VELECRETE RC 104 Rodding Castables Description: The Rodding Castables offered by us are user friendly in nature and does not require high energy mixing machines and vibrators. Free flowing in nature, these castables are designed in c.. |
|||
Bulk Density | >= 2.80 g/cc | >= 0.101 lb/in³ | After Drying at 110°C |
Sharadaa Ceramics ZAP 003 Smart Cast Application Special Properties: Anti-repellent PropertiesIndustry: CementApplication: Cement Plant Smoke ChamberInformation provided by Sharadaa Ceramics Pvt. Ltd. |
|||
Bulk Density | 2.79 g/cc | 0.101 lb/in³ | Trowellable |
Stellar Canada CERAMITE® BKR-F Wear Resistant Castable Ceramite is a family of wear resistant castables with a unique combination of high wear resistance, thermal resistance and mechanical strength. Ceramite is produced and supplied to end users world w.. |
|||
Bulk Density | 2.79 g/cc | 0.101 lb/in³ | Self-flowing |
Stellar Canada CERAMITE® CSR-S Wear Resistant Castable Ceramite is a family of wear resistant castables with a unique combination of high wear resistance, thermal resistance and mechanical strength. Ceramite is produced and supplied to end users world w.. |
|||
Bulk Density | >= 2.80 g/cc | >= 0.101 lb/in³ | After Drying at 110°C |
Sharadaa Ceramics ZAP 012 Smart Cast Application Special Properties: Patching At Hot Conditions, Easy InstallationIndustry: All IndustryApplication: All type of Rotary Kilns, AL/CU Melting Furnaces, Rolling Mills, Forgoing Furnaces, IncineratorsIn.. |
|||
Bulk Density | 2.80 g/cc | 0.101 lb/in³ | Scott |
China Tungsten YG13 Tungsten Carbide Powder Information provided by China Tungsten |
|||
Bulk Density | 2.80 g/cc | 0.101 lb/in³ | Scott |
China Tungsten YG13X Tungsten Carbide Powder Information provided by China Tungsten |
|||
Bulk Density | 2.80 - 2.90 g/cc | 0.101 - 0.105 lb/in³ | |
Chosun Refractories BATN-8 Gas Purging Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Bulk Density | 2.80 - 2.90 g/cc | 0.101 - 0.105 lb/in³ | |
Chosun Refractories CSN-309NM,Insert Plate Brick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Bulk Density | 2.80 - 2.90 g/cc | 0.101 - 0.105 lb/in³ | |
Chosun Refractories CUN-810 Nozzle Brick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Bulk Density | 2.80 g/cc | 0.101 lb/in³ | |
Chosun Refractories SAL75Z(ACD) Special Alumina brick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Bulk Density | >= 2.80 g/cc | >= 0.101 lb/in³ | |
China-Yixing Longly Refractories Load Bearing Board Corundum-Mullite Products with high-purity fused alumina and fused mullite for raw materials, the use of high-tonnage press repression, from ultra-high-temperature sintering; high-purity, the main phase (or corundum.. |
|||
Bulk Density | >= 2.80 g/cc | >= 0.101 lb/in³ | |
China-Yixing Longly Refractories Push Slab Corundum-Mullite Our company's production of a variety of corundum mullite push slab (moved plate), corundum-mullite seggar, corundum mullite corrugated board and other kinds of the kiln furniture, high refractorine.. |
|||
Bulk Density | 2.80 - 3.10 g/cc | 0.101 - 0.112 lb/in³ | |
China-Yixing Longly Refractories Steatite Ceramics (High Frequency Porcelain) LONGLY's steatite ceramics (namely high frequency porcelain, strengthened porcelain, magnesia porcelain), molecular formula as MgO-SiO2, is pure white. Steatite is the appropriate option when good .. |
|||
Bulk Density | 2.80 g/cc | 0.101 lb/in³ | |
Chosun Refractories CER-80 Special Casting Block Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Bulk Density | 2.80 g/cc | 0.101 lb/in³ | Powder |
Ametek P409L P/M Stainless Steel, Sintered from 6.45 g/cc Green Density P409L is a ferritic, weldable grade of stainless steel with high compressibility, enhanced green strength and good sinterability. This stabilized grade provides excellent corrosion resistance and ha.. |
|||
Bulk Density | 2.80 g/cc | 0.101 lb/in³ | Powder |
Ametek P409L P/M Stainless Steel, Sintered from 6.60 g/cc Green Density P409L is a ferritic, weldable grade of stainless steel with high compressibility, enhanced green strength and good sinterability. This stabilized grade provides excellent corrosion resistance and ha.. |