Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Gouda Vuurvast CURAS 85 PD GM Moldable Refractory Material

Category Ceramic , Oxide , Aluminum Oxide
Manufacturer Gouda Vuurvast
Trade Name CURAS
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Gouda Vuurvast CURAS 85 PD GM Moldable Refractory Material.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Description: This material is supplied as a dry powder and can be gunned. This phosphate bonded material based on corundum and bauxite has a very good resistance against slag attack or liquid aluminum. The mechanical strength of this product is just developed after heating above 150°C.Remarks: The stated chemical composition and physical properties represent average values.Information provided by Gouda Vuurvast.
Physical Properties Metric English Comments
Bulk Density 2.80 - 2.90 g/cc
0.101 - 0.105 lb/in³
After drying at 110°C
Thermal Properties Metric English Comments
Thermal Conductivity 0.890 - 0.990 W/m-K

@Temperature 100 °C
6.18 - 6.87 BTU-in/hr-ft²-°F

@Temperature 212 °F
0.970 - 1.17 W/m-K

@Temperature 600 °C
6.73 - 8.12 BTU-in/hr-ft²-°F

@Temperature 1110 °F
1.44 - 1.64 W/m-K

@Temperature 1600 °C
9.99 - 11.4 BTU-in/hr-ft²-°F

@Temperature 2910 °F
Maximum Service Temperature, Air 1650 °C
3000 °F
Shrinkage -1.50 - 1.50 %

@Temperature 1600 °C
-1.50 - 1.50 %

@Temperature 2910 °F
Permanent Linear Change
Component Elements Properties Metric English Comments
Al2O3 84 %
84 %
Fe2O3 <= 1.0 %
<= 1.0 %
SiO2 11 %
11 %
Descriptive Properties Value Comments
Bonding Type chemical/ceramic
Material Consumption per 1 m3 2800 kg
Segercone 37