Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 0.800 g/cc | 0.0289 lb/in³ | Loose |
Nyco NYAD G® WOLLASTOCOAT® Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Bulk Density | 0.800 g/cc | 0.0289 lb/in³ | Tapped |
Nyco NYGLOS® 20 Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Bulk Density | 0.800 - 1.00 g/cc | 0.0289 - 0.0361 lb/in³ | |
Nabaltec NABALOX® NO 105 Calcined Aluminum Oxide NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula.. |
|||
Bulk Density | 0.800 - 1.00 g/cc | 0.0289 - 0.0361 lb/in³ | |
Nabaltec NABALOX® NO 713-10 Reactive Alumina NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula.. |
|||
Bulk Density | 0.800 g/cc | 0.0289 lb/in³ | PEPL-10-W-67 |
Pearl Engineering PEPLPET D-101-SH Monofilament Resin Used in the paper industry as paper pulp nets. |
|||
Bulk Density | 0.800 - 0.900 g/cc | 0.0289 - 0.0325 lb/in³ | PEPL-10-W-67 |
Pearl Engineering PEPLPET B-103C PET Bottle Grade A co-polymer used for mineral water bottles |
|||
Bulk Density | 0.800 - 1.05 g/cc | 0.0289 - 0.0379 lb/in³ | |
Magyar Aluminum ALO-DF223 Alumina Alumina for Polishing |
|||
Bulk Density | 0.800 - 1.10 g/cc | 0.0289 - 0.0397 lb/in³ | |
Magyar Aluminum ALO-DFC Alumina Alumina for Polishing |
|||
Bulk Density | 0.800 g/cc | 0.0289 lb/in³ | Tap Density |
Momentive Performance Materials AC6001 Boron Nitride (BN) Powder Agglomerate of hexagonal BN crystals. AC6001 powders are granular with good flow and blend characteristics as well as high thermal conductivity and good lubrication qualities. Information provided.. |
|||
Bulk Density | 0.801 - 0.897 g/cc | 0.0289 - 0.0324 lb/in³ | Loose |
KaMin KaMin® Tek 2001 Clay The uniform, narrow particle size distribution and excellent color makes Kamin® TEK 2001 the preferred extender for gloss latex paints where optimum TiO2 spacing is desired without adverse effect.. |
|||
Bulk Density | 0.800 g/cc | 0.0289 lb/in³ | ISO 60 |
Lanxess Pocan® ECO T 3240 000000 PBT + PET, 45% Glass Fiber PBT + PET, 45% glass fibers, injection molding, improved surface finish, contains 25% post-consumer recycled material, increased temperature peak loadInformation provided by LANXESS. |
|||
Bulk Density | 0.800 g/cc | 0.0289 lb/in³ | ISO 60 |
Lanxess Pocan® T 7331 POS151 700226 PBT + PET, 30% Glass Fiber PBT + PET, 30% glass fibers, injection molding, improved surface finish, increased temperature peak load, UV stabilizedInformation provided by LANXESS. |
|||
Bulk Density | 0.800 g/cc | 0.0289 lb/in³ | ISO 60 |
Lanxess Pocan® B 1701 000000 PBT PBT, non-reinforced, extrusion, food contactInformation provided by LANXESS. |
|||
Bulk Density | 0.801 g/cc | 0.0289 lb/in³ | Dry |
Skamol Group Moler ROTOL Insulating Block SKAMOL Moler insulating bricks & blocks have the following characteristics: Max. service temperature: Up to 1000°C (1832°F)Back-up insulation Excellent insulating propertiesHigh mechanical str.. |
|||
Bulk Density | 0.801 g/cc | 0.0289 lb/in³ | Dry |
Skamol Group SKAMOLEX V-1100 (800) Customized Shape SKAMOLEX customized shapes have the following characteristics: Max. service temperature: Up to 1150°C (2102°F)Hot-face applications or back-up insulationA large variety of specialized and vers.. |
|||
Bulk Density | 0.800 g/cc | 0.0289 lb/in³ | ASTM D1895 |
Sumitomo Bakelite North America E 8354A-2 Short Glass Fiber Reinforced Epoxy E 8354A-2 is a fiberglass and mineral reinforced epoxy molding compound, with excellent dimensional stability, good electrical insulation properties, and good strength.Information provided by Sumito.. |
|||
Bulk Density | 0.800 g/cc | 0.0289 lb/in³ | Powder; ISO 60 |
Sumitomo Bakelite North America RX® 630 Fiberglass Reinforced Phenolic RX 630 is a fiberglass reinforced phenolic molding compound, with good dimensional stability and good strength at elevated temperatures. Information supplied by Sumitomo Bak North America. |
|||
Bulk Density | 0.800 g/cc | 0.0289 lb/in³ | ASTM D1895 |
Sumitomo Bakelite Sumikon® PM-9501 Glass-Filled Phenolic, Compression Grade Sumikon PM-9501 is a two stage glass fiber and mineral filled black phenolic special purpose molding compound. It is especially designed for applications requiring high strength and dimensional s.. |
|||
Bulk Density | 0.800 g/cc | 0.0289 lb/in³ | ASTM D1895 |
Sumitomo Bakelite North America E 16521A Electrical Encapsulation Grade Epoxy E-16521A is an encapsulation grade epoxy molding compound suitable for electrical applications such as coils.Information provided by Sumitomo Bak North America, Inc. |
|||
Bulk Density | 0.800 g/cc | 0.0289 lb/in³ | |
Solvay SUPRAGIL® RM/210 EI Polynaphthalenmethan-Sulphonate, Sodium Salt Description: Dispersing, non foaming agent.Identification: POLYNAPHTHALENMETHAN-SULPHONATE, SODIUM SALTCAS: 9084 – 06 – 4Solubility: Soluble in water. Insoluble in polar and aromatic solve.. |
|||
Bulk Density | 0.800 g/cc | 0.0289 lb/in³ | Size E (tapped) |
Vesta Ceramics SicoMill® Grade 4 Silicon Powder General Description:SicoMill® is a fine-grained silicon powder, specially developed for the ceramic industry. We have five standard grinding grades, but we can produce powders adapted to single cu.. |
|||
Bulk Density | 0.800 g/cc | 0.0289 lb/in³ | |
DuPont™ Nomex® 410 Paper, 3 mil Nominal Thickness Nomex® Type 410 is a calendared insulation paper which offers high inherent dielectric strength, mechanical toughness, flexibility, and resilience. It is the original form of Nomex® paper and is .. |
|||
Bulk Density | >= 0.800 g/cc | >= 0.0289 lb/in³ | |
Chosun Refractories LW-28 Special Insulating Firebrick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Bulk Density | 0.801 g/cc | 0.0289 lb/in³ | Dow Method |
Dow XU 32046.31 Barrier Polymer Excellent oxygen and water vapor barrier Information provided by Dow |
|||
Bulk Density | 0.800 g/cc | 0.0289 lb/in³ | DIN 53466 |
3M Dyneon™ PFA 6503PAZ Fluoroplastic Powder 3M™ Dyneon™ Fluoroplastic Powder PFA 6503PAZ is a fluorothermoplastic powder designed for use in thin film powder coatings. Typical applications include non-stick surfaces, chemical vessel and tan.. |
|||
Bulk Density | 0.800 - 0.900 g/cc | 0.0289 - 0.0325 lb/in³ | |
Addcomp ADD-VANCE® BA 401 Blowing agent Fields of application: Foamed products of Polyolefin and other polymers.Examples: Extruded sheets and foams in general as well as injection molded parts that require a foamed core.Mode of action and.. |
|||
Bulk Density | 0.800 g/cc | 0.0289 lb/in³ | Poured; ASTM D1895 |
Eastman VersaTray 12822 Plastic
(discontinued **) VersaTray plastic 12822 is a polyethylene terephthalate resin designed for use as a base resin for crystallized PET (CPET) food trays and other high temperature food packaging applications. CPET foo.. |
|||
Bulk Density | 0.800 g/cc | 0.0289 lb/in³ | Powder; ASTM D1895 |
Sumitomo Bakelite North America FM 4009 Fiberglass Reinforced Phenolic Novolac FM 4009 is a fiberglass reinforced phenolic novolac molding compound formulated for excellent wear resistance.Information supplied by Sumitomo Bak North America. |
|||
Bulk Density | 0.800 g/cc | 0.0289 lb/in³ | ASTM D1895 |
Sumitomo Bakelite North America RX® 647 Fiberglass Reinforced Phenolic RX 643 is a fiberglass reinforced, ammonia-free, phenolic resole compound, with good dimensional stability and good strength at elevated temperatures. Meets ASTM D-5948 Type GPI-10. RX 647 is a fibe.. |
|||
Bulk Density | 0.800 g/cc | 0.0289 lb/in³ | DIN 53466 |
3M Dyneon™ PFA 6503 B EPC Perfluoroalkoxy Fluorothermoplastic
(discontinued **) Dyneon PFA 6503 B EPC is a fluorothermoplastic powder for powder coating applications, and is designed for thin film applications where target film thickness is 25-40 micrometers per pass.non-stick .. |