KaMin KaMin® Tek 2001 Clay

Category Ceramic , Clay
Manufacturer KaMin LLC
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF KaMin KaMin® Tek 2001 Clay.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
The uniform, narrow particle size distribution and excellent color makes Kamin® TEK 2001 the preferred extender for gloss latex paints where optimum TiO2 spacing is desired without adverse effect on gloss.Industry: Paint & CoatingsUses: Architectural Coatings, Industrial Coatings, Wood Coatings, Satin, GlossInformation provided by KaMin LLC.
Physical Properties Metric English Comments
Specific Gravity 2.60 g/cc
2.60 g/cc
Bulk Density 0.801 - 0.897 g/cc
0.0289 - 0.0324 lb/in³
Loose
Solids Content 69.5 - 71 %
69.5 - 71 %
Slurry
Brightness 91 - 92.5 %
91 - 92.5 %
Reflectance (TAPPI)
Oil Absorption 34 %
34 %
Fineness >= 5
>= 5
Hegman Grind
Moisture Absorption at Equilibrium <= 1.5 %
<= 1.5 %
As Produced
Particle Size 0.250 µm
0.250 µm
Average Stokes Equivalent Diameter
0.620 µm
0.620 µm
Median (Malvern Laser)
Particle Mesh Size 325 Mesh
325 Mesh
0.005% Retained
pH 6 - 8
6 - 8
100 g/250 ml H2O Slurry
Specific Surface Area 20.0 m²/g
20.0 m²/g
BET
Brookfield Viscosity 500 cP

@Temperature 25.0 °C
500 cP

@Temperature 77.0 °F
20 RPM
Descriptive Properties Value Comments
Bulking Value 21.7 lb.gal
CAS Number 1332-58-7
Crystalline Silica (quartz) <0.1%
Physical Forms Dry, Slurry
Shipping Point Wrens, GA