Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 0.500 g/cc | 0.0181 lb/in³ | |
NanoScale NanoActive® Calcium Oxide NanoActive CaO is produced using proprietary processes to obtain high specific surface area (over 20 m²/g vs. 1-2 m²/g for standard CaO) with strong affinity towards carbon dioxide and hydrogen su.. |
|||
Bulk Density | 0.500 - 0.800 g/cc | 0.0181 - 0.0289 lb/in³ | |
Magyar Aluminum ALO-DF2 Alumina Alumina for Polishing |
|||
Bulk Density | 0.500 g/cc | 0.0181 lb/in³ | |
Isoflon Polyester Mesh Open mesh polyester, 1 x 1 mm, is used in a large number of industries such as food processing, textiles, packaging and electronics for single filtration or for drying ovens.Thanks to its great flex.. |
|||
Bulk Density | 0.500 g/cc | 0.0181 lb/in³ | Tap Density |
Momentive Performance Materials AC6103 Boron Nitride (BN) Powder Agglomerate of hexagonal BN crystals. AC6103 powders are granular with good flow and blend characteristics as well as high thermal conductivity and good lubrication qualities. Information provided.. |
|||
Bulk Density | 0.500 - 0.800 g/cc | 0.0181 - 0.0289 lb/in³ | |
Shandong Dongyue Polymer DF-21A PTFE Presintered Resin Usage: The presintered resin is suitable for continuously extruding of all types, pushing and pressing PTFE rod, tube and special shape.Packing: PTFE is packed in double layer PVC bags inside and in.. |
|||
Bulk Density | 0.500 g/cc | 0.0181 lb/in³ | |
Solvay SOPROPHOR® K/202 Surfactant Description: Multipurpose dispersing agent for SC formulationsIdentification: ABSORBED SURFACTANTSolubility: Dispersible in water. Insoluble in polar and aromatic solvents.Available in: Asia Pacific.. |
|||
Bulk Density | 0.500 - 0.600 g/cc | 0.0181 - 0.0217 lb/in³ | |
Borealis LE4201R Polyethylene Insulation Compound, Crosslinkable LE4201R is a crosslinkable natural polyethylene compound, specially designed for insulation applications. Applications LE4201R is intended for insulation of XLPE power cables with rated voltages up.. |
|||
Bulk Density | 0.500 g/cc | 0.0181 lb/in³ | Size E (apparent) |
Vesta Ceramics SicoMill® Grade 4 Silicon Powder General Description:SicoMill® is a fine-grained silicon powder, specially developed for the ceramic industry. We have five standard grinding grades, but we can produce powders adapted to single cu.. |
|||
Bulk Density | 0.500 g/cc | 0.0181 lb/in³ | |
Zircar Zirconia HfF-100 Hafnia Felt Insulation Our hafnia (HfO2) fibers and textiles are made by the same unique Zircar process used for manufacturing yttria-stabilized zirconia cloths and felts. Our high purity hafnia fiber and textiles are off.. |
|||
Bulk Density | >= 0.500 g/cc | >= 0.0181 lb/in³ | |
Chosun Refractories A-3 Insulating Firebrick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Bulk Density | 0.500 - 0.650 g/cc | 0.0181 - 0.0235 lb/in³ | |
Addcomp ADD-VANCE® NU 489 Nucleation masterbatch, PP based Fields of application: Extruded and injection molded articles made from PP resins.Examples: Extruded PP sheets, films, tapes and blow molded and injection molded articles, such as garden furniture, .. |
|||
Bulk Density | 0.500 - 0.650 g/cc | 0.0181 - 0.0235 lb/in³ | |
Addcomp ADD-VANCE® THC 453 PP based masterbatch containing heat stabilizers and carbon black Fields of application: Stabilization masterbatch for producing long fiber reinforced polypropylene for D-LFT processExamples: Long fiber reinforced pellets to be used for automotive parts, like unde.. |
|||
Bulk Density | 0.500 - 0.800 g/cc | 0.0181 - 0.0289 lb/in³ | |
BASF Ultramid® B3EG5 25% Glass Filled PA6 (Dry) Description: 25% glass-fiber reinforced injection-molding grade for industrial articles and electrical insulating partsInformation provided by BASF |
|||
Bulk Density | 0.500 - 0.800 g/cc | 0.0181 - 0.0289 lb/in³ | |
BASF Ultramid® B3EG7 35% Glass Filled PA6 (Dry) Description: 35% Glass fiber reinforced injection molding grade for industrial articles and electrical insulating parts.Information provided by BASF |
|||
Bulk Density | 0.500 - 0.800 g/cc | 0.0181 - 0.0289 lb/in³ | |
BASF Ultramid® B3EG7 BK 00564 35% Glass Filled PA6 (Conditioned) Description: 35% Glass fiber reinforced injection molding grade for industrial articles and electrical insulating parts.Information provided by BASF |
|||
Bulk Density | 0.500 - 0.800 g/cc | 0.0181 - 0.0289 lb/in³ | |
BASF Ultramid® B3EG7 BK 00564 35% Glass Filled PA6 (Dry) Description: 35% Glass fiber reinforced injection molding grade for industrial articles and electrical insulating parts.Information provided by BASF |
|||
Bulk Density | 0.500 - 0.800 g/cc | 0.0181 - 0.0289 lb/in³ | |
BASF Ultramid® KR 4355 G10 BK 23215 50% Glass Filled PA6/6T (Dry) Description: 50% glass-fiber reinforced product for injection molding; high toughness and rigidity; low water absorption, high melting point (285°C); mechanical properties remain constant up to 60°.. |
|||
Bulk Density | 0.500 - 0.800 g/cc | 0.0181 - 0.0289 lb/in³ | |
BASF Ultramid® KR 4357 G6 BK 00564 30% Glass Filled PA6/6T (Dry) Description: 30% glass-fiber reinforced, impact-modified product for injection-molding; high toughness, strength and stiffness, low water absorption, high melting point (295°C [563°F]). The mechan.. |
|||
Bulk Density | 0.500 - 0.800 g/cc | 0.0181 - 0.0289 lb/in³ | |
BASF Ultramid® KR 4365 G5 35% Glass Filled PA6/6T FR (Conditioned) Description: Partially aromatic polyamide; flame retardant based on red phosphorus; low water absorption, high melting point (295°C); low tendency to form deposits on electrical contacts, very resi.. |
|||
Bulk Density | 0.500 - 0.800 g/cc | 0.0181 - 0.0289 lb/in³ | |
BASF Ultramid® A3EG5 25% Glass Filled PA66 (Dry) Description: Glass fiber reinforced injection molding grade for machinery components and housings of high stiffness and dimensional stability such as coil formers and bearing cages. Also used for el.. |
|||
Bulk Density | 0.500 - 0.800 g/cc | 0.0181 - 0.0289 lb/in³ | |
BASF Ultramid® A3HG6 HR BK 23591 30% Glass Filled PA66 (Dry) Description: 30% glass-fiber reinforced injection-molding grade with enhanced hydrolysis resistance, e.g., for applications in vehicle cooling systems.Information provided by BASF |
|||
Bulk Density | 0.500 - 0.800 g/cc | 0.0181 - 0.0289 lb/in³ | |
BASF Ultramid® B35EG3 BK 00564 15% Glass Filled PA6 (Dry) Description: 15% glass-fiber reinforced injection-molding grade for gIT applications such as, for example, steering column switches, vehicle mirror housings and the wheels of mountain bikes.Informat.. |
|||
Bulk Density | 0.500 - 0.800 g/cc | 0.0181 - 0.0289 lb/in³ | |
BASF Ultramid® B3EG5 25% Glass Filled PA6 (Conditioned) Description: 25% glass-fiber reinforced injection-molding grade for industrial articles and electrical insulating partsInformation provided by BASF |
|||
Bulk Density | 0.500 - 0.800 g/cc | 0.0181 - 0.0289 lb/in³ | |
BASF Ultramid® B3UG4 Grey 22975 20% Glass Filled PA66 FR (Dry) Description: Halogen-free and phosphorus free flame retardant injection-molding grade with outstanding free-flow properties, good electrical properties and low smoke density; resistant to glow wire.. |
|||
Bulk Density | 0.500 - 0.800 g/cc | 0.0181 - 0.0289 lb/in³ | |
BASF Ultramid® B3UG4 LS BK 23215 20% Glass Filled PA66 FR (Dry) Description: Halogen-free and phosphorus free flame retardant injection-molding grade with outstanding free-flow properties, good electrical properties and low smoke density; resistant to glow wire.. |
|||
Bulk Density | 0.500 - 0.800 g/cc | 0.0181 - 0.0289 lb/in³ | |
BASF Ultramid® B3UG4 LS Grey 22985 20% Glass Filled PA66 FR (Conditioned) Description: Halogen-free and phosphorus free flame retardant injection-molding grade with outstanding free-flow properties, good electrical properties and low smoke density; resistant to glow wire.. |
|||
Bulk Density | 0.500 - 0.650 g/cc | 0.0181 - 0.0235 lb/in³ | |
Addcomp ADD-VANCE® FR 243 Halogen-free flame retardant masterbatch, PP based Fields of application: Foils, films, fibers and extruded articles made from PP with a high surface/volume ratio.Examples: Foils, films, tapes, ropes, and filaments / fibers for carpets, non-wovens, .. |
|||
Bulk Density | 0.500 g/cc | 0.0181 lb/in³ | |
BASF 2,5-Dimethyl-2,5-hexanediol Formula: C8H18O2CAS: 110-03-2Description: Dimethylhexanediol is a colorless to yellow solid, and is odorless. It is soluble in water and easily soluble in alcohols and acetone.Synonyms: 2,5-Dimethy.. |
|||
Bulk Density | 0.500 g/cc | 0.0181 lb/in³ | |
BASF Theroplast® Yellow 104 Color Additive Chemical Structure: Pyrazolone YellowApplication: Colourant for plastics: PVC-u, PS, SAN, PMMA, PC, and UPRecommendations for food applications: BgVV, FrancePhysical form: PowderInformation provided.. |
|||
Bulk Density | 0.500 - 0.800 g/cc | 0.0181 - 0.0289 lb/in³ | |
BASF Ultramid® B3WG5 25% Glass Filled PA6 (Dry) Description: 25% glass-fiber reinforced and heat aging resistant injection-molding grade, for instance, for fan impeller glass-fiber reinforced injection-molding grade for industrial articles and el.. |