NanoScale NanoActive® Calcium Oxide

Category Ceramic , Oxide
Manufacturer NanoScale
Trade Name NanoActive®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF NanoScale NanoActive® Calcium Oxide.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
NanoActive CaO is produced using proprietary processes to obtain high specific surface area (over 20 m²/g vs. 1-2 m²/g for standard CaO) with strong affinity towards carbon dioxide and hydrogen sulfide.Applications: Applications include desiccant, elevated temperature hazardous waste treatment, flue gas treatment, insecticide and fungicide, odor reduction, precursor, pulp and paper, and water treatment.Information provided by NanoScaleComposition based on metal
Physical Properties Metric English Comments
Bulk Density 0.500 g/cc
0.0181 lb/in³
Density 3.30 g/cc
0.119 lb/in³
Particle Size 4.0 µm
4.0 µm
mean aggregate size
Specific Surface Area >= 20 m²/g
>= 20 m²/g
BET
Pore Size 0.0165 microns
0.000650 mil
Average Diameter
Component Elements Properties Metric English Comments
Calcium, Ca >= 99.8 %
>= 99.8 %
Descriptive Properties Value Comments
Appearance / Color White Powder
Minimum Total Pore Volume cc/g 0.1