Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Alliance Polymers Viprene™ P50A-22U-NAT Thermoplastic Vulcanizate Elastomer

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Vulcanizate Elastomer (TPV)
Manufacturer Alliance Polymers
Trade Name Viprene™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Alliance Polymers Viprene™ P50A-22U-NAT Thermoplastic Vulcanizate Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Viprene™ P50A-22U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing characteristics. Availability: North AmericaAdditive: Heat Stabilizer and UV StabilizerFeatures: Good Flow, Good UV Resistance and Heat StabilizedAppearance: Natural ColorForms: PelletsProcessing Method: Extrusion and Injection MoldingInformation provided by Alliance Polymers
Physical Properties Metric English Comments
Density 0.970 g/cc
0.0350 lb/in³
ISO 2781
Mechanical Properties Metric English Comments
Hardness, Shore A 50
50
ISO 868
Tensile Strength at Break 5.90 MPa
856 psi
ISO 37
Tensile Stress 1.80 MPa

@Strain 100 %
261 psi

@Strain 100 %
ISO 37
3.10 MPa

@Strain 300 %
450 psi

@Strain 300 %
ISO 37
Elongation at Break 550 %
550 %
ISO 37
Tear Strength 31.6 kN/m
180 pli
ISO 34-1
Compression Set 19 %

@Temperature 70.0 °C,
Time 79200 sec
19 %

@Temperature 158 °F,
Time 22.0 hour
ASTM D3995B
Thermal Properties Metric English Comments
Brittleness Temperature -60.0 °C
-76.0 °F
ASTM D746
Flammability, UL94 HB

@Thickness 1.00 mm
HB

@Thickness 0.0394 in
HB

@Thickness 1.50 mm
HB

@Thickness 0.0591 in
HB

@Thickness 3.00 mm
HB