Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Density = 0.0499 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 1.21 - 1.38 g/cc
0.0437 - 0.0499 lb/in³
Average value: 1.29 g/cc Grade Count:21
Overview of materials for Polyphthalamide (PPA), Aramid Fiber
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Aramid Fiber". Each property range of values reported is minimum and maximum values of ..
Density 1.32 - 1.38 g/cc
0.0477 - 0.0499 lb/in³
Average value: 1.35 g/cc Grade Count:8
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 40% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 40% Glass Fiber Filled". Specific grades with glass content betwe..
Density 1.06 - 1.38 g/cc
0.0383 - 0.0499 lb/in³
Average value: 1.18 g/cc Grade Count:14
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Glass Bead Filled
This property data is a summary of similar materials in the MatWeb database for the category "ABS + Glass Blend". Each property range of values reported is minimum and maximum values of appropriate ..
Density 1.15 - 1.38 g/cc
0.0415 - 0.0499 lb/in³
Average value: 1.20 g/cc Grade Count:8
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 30% Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 30% Carbon Fiber Filled". Specific grades with carbon fiber conte..
Density 1.30 - 1.38 g/cc
0.0470 - 0.0499 lb/in³
Average value: 1.34 g/cc Grade Count:3
Overview of materials for Polycarbonate, Carbon + Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Carbon + Glass Fiber Reinforced". Each property range of values reported is minimum and m..
Density 1.34 - 1.38 g/cc
0.0484 - 0.0499 lb/in³
ISO R 1184
Fainplast Compounds RKT 226 Rigid PVC, Extrusion Lead Free
Metal effect profiles
Density 1.34 - 1.38 g/cc
0.0484 - 0.0499 lb/in³
ISO R 1184
Fainplast Compounds RKT 736/K1 Rigid PVC, Extrusion Lead Free
Transparent profiles
Density 1.34 - 1.38 g/cc
0.0484 - 0.0499 lb/in³
ISO R 1184
Fainplast Compounds SAR 03 Rigid PVC, Antishock Injection Molding Lead Free
Electric antishock fittings
Density 1.36 - 1.38 g/cc
0.0491 - 0.0499 lb/in³
Fiber Density
SGL Carbon Group PANOX® FB M400 EEA Oxidized Textile Fiber, Milled Fiber, For carbon/carbon and spinning
PANOX® is the industry standard when it comes to fire-retardant textile fibers. As an oxidized, thermally stabilized polyacrylonitrile (PAN) fiber that will not burn, melt, soften or drip, PANOX ..
Density 1.36 - 1.38 g/cc
0.0491 - 0.0499 lb/in³
Fiber Density
SGL Carbon Group PANOX® FB T320 EEA Oxidized Textile Fiber, Continuous Tow with 320k filaments, For carbon/carbon and spinning
PANOX® is the industry standard when it comes to fire-retardant textile fibers. As an oxidized, thermally stabilized polyacrylonitrile (PAN) fiber that will not burn, melt, soften or drip, PANOX ..
Density 1.34 - 1.38 g/cc
0.0484 - 0.0499 lb/in³
ISO R 1183
Fainplast Compounds CKL 8318/2 Flexible PVC, Sheathing Lead Free
Sheathing coaxial TV cables
Density 1.34 - 1.38 g/cc
0.0484 - 0.0499 lb/in³
ISO R 1183
Fainplast Compounds FR 89/2 Flexible PVC, Insulation
Insulation for special application
Density 1.34 - 1.38 g/cc
0.0484 - 0.0499 lb/in³
ISO R 1183
Fainplast Compounds GS 100/2 Flexible PVC, Injection Molding, Lead Free
Semi-rigid for cable passage
Density 1.34 - 1.38 g/cc
0.0484 - 0.0499 lb/in³
ISO R 1184
Fainplast Compounds HL 101 Flexible PVC, Insulation for High Temperatures
Operating temperature 80°C
Density 1.34 - 1.38 g/cc
0.0484 - 0.0499 lb/in³
ISO R 1184
Fainplast Compounds HLA 075 Flexible PVC, Insulation for High Temperatures
Operating temperature 105°C
Density 1.34 - 1.38 g/cc
0.0484 - 0.0499 lb/in³
ISO R 1184
Fainplast Compounds ARC 20 Rigid PVC, Atoxic for General Purpose
Bottles medium/high antishock
Density 1.34 - 1.38 g/cc
0.0484 - 0.0499 lb/in³
ISO R 1184
Fainplast Compounds ARC 30 Rigid PVC, Atoxic for General Purpose
Bottles very high antishock
Density 1.34 - 1.38 g/cc
0.0484 - 0.0499 lb/in³
ISO R 1183
Fainplast Compounds CL 69 Flexible PVC, Sheathing
Sheath for low temperatures
Density 1.34 - 1.38 g/cc
0.0484 - 0.0499 lb/in³
ISO R 1183
Fainplast Compounds GA 75/R Flexible PVC, Flame Retardant Sheathing
According to UL 1581 Class 43 (90°C)
Density 1.34 - 1.38 g/cc
0.0484 - 0.0499 lb/in³
ISO R 1183
Fainplast Compounds HL 91 Flexible PVC, Insulation for High Temperatures
Operating temperature 105°C
Density 1.32 - 1.38 g/cc
0.0477 - 0.0499 lb/in³
Molding; IS 867-1963
Amity Thermosets ATI 101 Phenolic Molding Organic Filler, Injection Molded
Characteristics:Electrical low loss Good mechanical strengthHigh electrical insulationGood mechanical strengthGlossy surfaceLow water absorptionColor-blackVery soft flow Applications: Electric swit..
Density 1.32 - 1.38 g/cc
0.0477 - 0.0499 lb/in³
Molding; IS 867-1963
Amity Thermosets ATM 123 Phenolic Molding Organic Filler, Compression Molded
Characteristics:Glossy surface free of filler marks Surface good & free of flaws Good mouldabilitySurface free of filler marks even after turningGood mechanical strengthColor-black, brownMedium flow..
Density 1.35 - 1.38 g/cc
0.0488 - 0.0499 lb/in³
Molding; IS 867-1963
Amity Thermosets ATM 125 Phenolic Molding Organic Filler, Compression Molded
Characteristics:Glossy surface free of filler marks Surface good & free of flaws Good mouldabilitySurface free of filler marks even after turningGood mechanical strengthColor-black, brownSoft/medium..
Density 1.35 - 1.38 g/cc
0.0488 - 0.0499 lb/in³
Molding; IS 867-1963
Amity Thermosets ATO 142 Phenolic Molding Organic Filler, Compression Molded
Characteristics:Electrical low loss Good mechanical strengthHigh electrical insulationGood mechanical strengthGlossy surfaceLow water absorptionColor-black, brownMedium/hard flow Applications: Elec..
Density 1.32 - 1.38 g/cc
0.0477 - 0.0499 lb/in³
Molding; IS 867-1963
Amity Thermosets ATI 102 Phenolic Molding Organic Filler, Injection Molded
Characteristics:Electrical low loss Good mechanical strengthHigh electrical insulationGood mechanical strengthGlossy surfaceLow water absorptionColor-blackVery soft flow Applications: Electric swit..
Density 1.35 - 1.38 g/cc
0.0488 - 0.0499 lb/in³
Molding; IS 867-1963
Amity Thermosets ATO 145 Phenolic Molding Organic Filler, Compression Molded
Characteristics:Electrical low loss Good mechanical strengthHigh electrical insulationGood mechanical strengthGlossy surfaceLow water absorptionColor-black, brownMedium flow Applications: Electric ..
Density 1.28 - 1.38 g/cc
0.0462 - 0.0499 lb/in³
Average value: 1.32 g/cc Grade Count:7
Overview of materials for Polyetherimide (PEI), Aramid Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide, Aramid Fiber Filled". Each property range of values reported is minimum and maximum valu..
Density 1.34 - 1.38 g/cc
0.0484 - 0.0499 lb/in³
ISO R 1184
Fainplast Compounds KL 96 Flexible PVC, Insulation for High Temperatures Lead Free
Operating temperature 105°C
Density 1.34 - 1.38 g/cc
0.0484 - 0.0499 lb/in³
ISO R 1184
Fainplast Compounds RKT 736 Rigid PVC, Extrusion Lead Free
Transparent antishock profiles
Density 1.34 - 1.38 g/cc
0.0484 - 0.0499 lb/in³
ISO R 1183
Fainplast Compounds CL 76/1 Flexible PVC, Sheathing
General purposes
Copyright © lookpolymers.com All Rights Reserved