Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Fainplast Compounds FR 89/2 Flexible PVC, Insulation

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Wire and Cable Grade
Manufacturer Fainplast Compounds
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Fainplast Compounds FR 89/2 Flexible PVC, Insulation.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Insulation for special application
Physical Properties Metric English Comments
Density 1.34 - 1.38 g/cc
0.0484 - 0.0499 lb/in³
ISO R 1183
Mechanical Properties Metric English Comments
Hardness, Shore A 87 - 91
87 - 91
ISO R 868
Tensile Strength at Break >= 16.0 MPa
>= 2320 psi
ISO R 527
Elongation at Break >= 250 %
>= 250 %
ISO R 527
Electrical Properties Metric English Comments
Volume Resistivity 2.00e+14 ohm-cm

@Temperature 23.0 °C
2.00e+14 ohm-cm

@Temperature 73.4 °F
ASTM D257
Descriptive Properties Value Comments
Thermal Stability (minutes) 90
CEI 20-34/3-2