Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.04 - 1.27 g/cc | 0.0376 - 0.0459 lb/in³ | Average value: 1.08 g/cc Grade Count:66 |
Overview of materials for Polyphenylene Ether, Molded This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, Molded". Each property range of values reported is minimum and maximum values of ap.. |
|||
Density | 0.910 - 1.27 g/cc | 0.0329 - 0.0459 lb/in³ | Average value: 0.949 g/cc Grade Count:65 |
Overview of materials for Ethylene Acrylic Acid This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Acrylic Acid". Each property range of values reported is minimum and maximum values of appropri.. |
|||
Density | 1.03 - 1.27 g/cc | 0.0371 - 0.0459 lb/in³ | Average value: 1.13 g/cc Grade Count:79 |
Overview of materials for Nylon 66/6 This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6". Each property range of values reported is minimum and maximum values of appropriate MatWeb .. |
|||
Density | 1.23 - 1.27 g/cc | 0.0444 - 0.0459 lb/in³ | B Curative |
Lord Adhesives 7542 Urethane Adhesive LORD® 7542 adhesive is an equal-mix, two-component urethane adhesive system used to bond FRP, SMC and other plastics with little surface preparation. This adhesive will also bond primed metals. L.. |
|||
Density | 1.23 - 1.27 g/cc | 0.0444 - 0.0459 lb/in³ | D Curative |
Lord Adhesives 7542 Urethane Adhesive LORD® 7542 adhesive is an equal-mix, two-component urethane adhesive system used to bond FRP, SMC and other plastics with little surface preparation. This adhesive will also bond primed metals. L.. |
|||
Density | 1.23 - 1.27 g/cc | 0.0444 - 0.0459 lb/in³ | E Curative |
Lord Adhesives 7542 Urethane Adhesive LORD® 7542 adhesive is an equal-mix, two-component urethane adhesive system used to bond FRP, SMC and other plastics with little surface preparation. This adhesive will also bond primed metals. L.. |
|||
Density | 1.23 - 1.27 g/cc | 0.0444 - 0.0459 lb/in³ | ISO R 1183 |
Fainplast Compounds CKL 70 Flexible PVC, Sheathing Lead Free General purposes |
|||
Density | 1.23 - 1.27 g/cc | 0.0444 - 0.0459 lb/in³ | ISO R 1183 |
Fainplast Compounds GS 74 Flexible PVC, Injection Molding for Footwear Soles for mild climates |
|||
Density | 1.23 - 1.27 g/cc | 0.0444 - 0.0459 lb/in³ | ISO R 1183 |
Fainplast Compounds GS 74/P Flexible PVC, Injection Molding for Footwear Pearl sandals |
|||
Density | 1.23 - 1.27 g/cc | 0.0444 - 0.0459 lb/in³ | ISO R 1183 |
Fainplast Compounds GS 90 Flexible PVC, Injection Molding for Footwear Soles |
|||
Density | 1.23 - 1.27 g/cc | 0.0444 - 0.0459 lb/in³ | ISO R 1183 |
Fainplast Compounds GSK 61 Flexible PVC, Injection Molding, Lead Free Items for building industry |
|||
Density | 1.23 - 1.27 g/cc | 0.0444 - 0.0459 lb/in³ | ISO R 1183 |
Fainplast Compounds GSK 6515 Flexible PVC, Injection Molding, Lead Free Technical items |
|||
Density | 1.23 - 1.27 g/cc | 0.0444 - 0.0459 lb/in³ | ISO R 1183 |
Fainplast Compounds GSO 70/33 Flexible PVC, Injection Molding for Footwear Soles, opaque surface |
|||
Density | 1.23 - 1.27 g/cc | 0.0444 - 0.0459 lb/in³ | ISO R 1184 |
Fainplast Compounds KLT 92/1 Flexible PVC, Insulation Transparent Cables Lead Free Transparent cables (90°C) |
|||
Density | 1.23 - 1.27 g/cc | 0.0444 - 0.0459 lb/in³ | ISO R 1183 |
Fainplast Compounds PG 80 Flexible PVC, Extrusion Modified with Rubber Profiles modified with rubber |
|||
Density | 1.23 - 1.27 g/cc | 0.0444 - 0.0459 lb/in³ | ISO R 1183 |
Fainplast Compounds PHA 91 Flexible PVC, Transparent Extrusion Atoxic pipes |
|||
Density | 1.23 - 1.27 g/cc | 0.0444 - 0.0459 lb/in³ | ISO R 1183 |
Fainplast Compounds PK 71/FR Flexible PVC, Lead Free Spiral pipes |
|||
Density | 1.25 - 1.27 g/cc | 0.0452 - 0.0459 lb/in³ | ISO 1183 |
BASF Ecoflex® F BX 7011 Biodegradable Plastic A flexible plastic designed for film extrusion and extrusion coating. Ecoflex F BX 7011 comes closer than any other biodegradable plastic to the processing properties of LDPE and LLDPE. Blown film e.. |
|||
Density | 0.933 - 1.27 g/cc | 0.0337 - 0.0459 lb/in³ | Average value: 0.958 g/cc Grade Count:129 |
Overview of materials for High Density Polyethylene (HDPE), Extruded This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Extruded". Each property range of values reported is minimum and maxim.. |
|||
Density | 1.23 - 1.27 g/cc | 0.0444 - 0.0459 lb/in³ | ISO R 1184 |
Fainplast Compounds KLT 096 Flexible PVC, Sheathing Transparent Cables Lead Free Transparent cables (105°C) |
|||
Density | 1.23 - 1.27 g/cc | 0.0444 - 0.0459 lb/in³ | ISO R 1184 |
Fainplast Compounds MPH 85 Medical Flexible PVC, Extrusion Tubolar apparatus |
|||
Density | 1.23 - 1.27 g/cc | 0.0444 - 0.0459 lb/in³ | ISO R 1183 |
Fainplast Compounds PH 77/AF Flexible PVC, Transparent Extrusion Profiles UL 94 Class V0 |
|||
Density | 1.23 - 1.27 g/cc | 0.0444 - 0.0459 lb/in³ | ISO R 1183 |
Fainplast Compounds PH 90/A Flexible PVC, Transparent Extrusion Profiles, UL 94 Class V1 |
|||
Density | 1.23 - 1.27 g/cc | 0.0444 - 0.0459 lb/in³ | ISO R 1183 |
Fainplast Compounds PM 6316/AM Flexible PVC, Lead Free Anti-mould profiles |
|||
Density | 1.23 - 1.27 g/cc | 0.0444 - 0.0459 lb/in³ | ISO R 1183 |
Fainplast Compounds PM 8005 Flexible PVC, Lead Free Various profiles |
|||
Density | 1.04 - 1.27 g/cc | 0.0376 - 0.0459 lb/in³ | Average value: 1.14 g/cc Grade Count:122 |
Overview of materials for Thermoplastic Polyurethane (TPUR), Polyether Grade This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane (TPUR), Polyether Grade". Each property range of values reported is minimum a.. |
|||
Density | 1.23 - 1.27 g/cc | 0.0444 - 0.0459 lb/in³ | ISO R 1183 |
Fainplast Compounds PMP 57 Flexible PVC, Extrusion Modified with PU Profiles mixed rubber/PU |
|||
Density | 1.25 - 1.27 g/cc | 0.0452 - 0.0459 lb/in³ | ISO 1183 |
BASF Ecoflex® P BX 7020 Biodegradable Polyester Description: Ecoflex® P BX 7020 is our biodegradable, statistical, aliphatic-aromatic copolyester based on the monomers 1,4-butanediol, adipic acid and terephthalic acid or dimethyltherephthalate i.. |
|||
Density | 1.17 - 1.27 g/cc | 0.0423 - 0.0459 lb/in³ | Average value: 1.22 g/cc Grade Count:25 |
Overview of materials for Polypropylene with 40% Mica Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Mica Filler". Specific grades with primary filler content between 35% and 44% are.. |