Fainplast Compounds PMP 57 Flexible PVC, Extrusion Modified with PU

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Extruded
Manufacturer Fainplast Compounds
Trade Name
Port Ningbo port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Fainplast Compounds PMP 57 Flexible PVC, Extrusion Modified with PU.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Profiles mixed rubber/PU
Physical Properties Metric English Comments
Density 1.23 - 1.27 g/cc
0.0444 - 0.0459 lb/in³
ISO R 1183
Mechanical Properties Metric English Comments
Hardness, Shore A 72 - 76
72 - 76
ISO R 868
Tensile Strength at Break 19.0 MPa
2760 psi
ISO R 527
Elongation at Break 400 %
400 %
ISO R 527
Abrasion 40
40
[mm³]; DIN 53516