Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.970 - 1.03 g/cc | 0.0350 - 0.0372 lb/in³ | ASTM D792 |
Multibase Multi-Flex® TPE A 8502 BLK The fogging test value is 90% according to ASTM SAE-J275. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase. |
|||
Density | 1.03 - 1.03 g/cc @Temperature 270 - 270 °C |
0.0372 - 0.0372 lb/in³ @Temperature 518 - 518 °F |
Average value: 1.03 g/cc Grade Count:1 |
Overview of materials for Polycarbonate/PET Polyester Blend This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/PET Polyester Blend". Each property range of values reported is minimum and maximum values.. |
|||
Density | 1.02 - 1.03 g/cc @Temperature 260 - 260 °C |
0.0368 - 0.0372 lb/in³ @Temperature 500 - 500 °F |
Average value: 1.02 g/cc Grade Count:15 |
Overview of materials for Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced". Each property range of values repor.. |
|||
Density | 1.03 - 1.03 g/cc @Temperature 290 - 290 °C |
0.0372 - 0.0372 lb/in³ @Temperature 554 - 554 °F |
Average value: 1.03 g/cc Grade Count:1 |
Overview of materials for Nylon 66, Unreinforced, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Unreinforced, Flame Retardant". Each property range of values reported is minimum and maximum .. |
|||
Density | 1.03 - 1.03 g/cc @Temperature 295 - 295 °C |
0.0372 - 0.0372 lb/in³ @Temperature 563 - 563 °F |
Average value: 1.03 g/cc Grade Count:1 |
Overview of materials for Nylon 66, 10% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 10% Glass Fiber Filled". Specific grades with glass content between 5% and 14% are included. .. |
|||
Density | 0.971 - 1.03 g/cc | 0.0351 - 0.0372 lb/in³ | |
Lord Adhesives 521 Medium Viscosity, Slow Cure Acrylic Adhesive Lord 500 SeriesLord 500 Series Acrylic Adhesives bond plastics and prepared metals; they offer excellent adhesion to both thermoplastics and thermoset plastics. They are available with varying handi.. |
|||
Density | 0.990 - 1.03 g/cc | 0.0358 - 0.0372 lb/in³ | AV15 |
Solvay Duraphos Octyl Acid Phosphate Surfactant Identification: DI(N-OCTYL) PHOSPHORIC ACID, N-OCTYL PHOSPHORIC ACID, PHOSPHORIC ACID CAS: 3115-39-7; 3991-73-9; 7664-38-2Solublility: Soluble in common organic solvents and slightly soluble in wate.. |
|||
Density | 0.990 - 1.03 g/cc | 0.0358 - 0.0372 lb/in³ | RP-17617 |
Solvay RHODOLINE® DF-988 Surfactant Description: Silicone free and mineral oil free defoamer for high gloss paints.Identification: DEFOAMERAvailable in: North AmericaApplications: RHODOLINE© DF-988 is a silicone-free, mineral oil-f.. |
|||
Density | 1.00 - 1.03 g/cc | 0.0361 - 0.0372 lb/in³ | RP-0549 |
Solvay RHODISOLV® INFINITY Solvent Description: Rhodiasolv INFINITY is a blend of dibasic ester solvent and proprietary surfactantsChemical Name: Microemulsion concentrate based on dimethyl-2-methyl glutarateSolubility in water: 100%.. |