Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.935 - 1.02 g/cc @Temperature 240 - 260 °C |
0.0338 - 0.0368 lb/in³ @Temperature 464 - 500 °F |
Average value: 0.981 g/cc Grade Count:16 |
Overview of materials for Polycarbonate/ABS Alloy, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, Unreinforced". Each property range of values reported is minimum and maximum va.. |
|||
Density | 1.02 - 1.02 g/cc @Temperature 290 - 310 °C |
0.0368 - 0.0368 lb/in³ @Temperature 554 - 590 °F |
Average value: 1.02 g/cc Grade Count:10 |
Overview of materials for Polycarbonate, Extruded This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Extruded". Each property range of values reported is minimum and maximum values of approp.. |
|||
Density | 1.02 - 1.02 g/cc @Temperature 280 - 300 °C |
0.0368 - 0.0368 lb/in³ @Temperature 536 - 572 °F |
Average value: 1.02 g/cc Grade Count:6 |
Overview of materials for Polycarbonate, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Impact Modified". Each property range of values reported is minimum and maximum values of.. |
|||
Density | 1.01 - 1.02 g/cc | 0.0364 - 0.0368 lb/in³ | |
Mallard Creek Polymers TYLAC® 814 SBR Emulsion Tylac® 814 is a surfactant stabilized styrene-butadiene copolymer latex. Features: when used in properly designed hydraulic cement mixtures, the addition of Tylac® 814 produces grouts, mortar.. |
|||
Density | 1.01 - 1.02 g/cc | 0.0364 - 0.0368 lb/in³ | |
Mallard Creek Polymers TYLAC® 873 Nitrile Emulsion Tylac® 873 is a carboxylated acrylonitrile-butadiene copolymer latex. Features: good resistance to oil, grease and solvent, compatible with anionic asphalt emulsions, broadens the temperature ran.. |
|||
Density | 0.899 - 1.02 g/cc | 0.0325 - 0.0368 lb/in³ | |
Lord Adhesives 26 No-Mix Accelerator for 200/500 Series Lord Adhesives 26 No-Mix Accelerator for 200/500 Series |
|||
Density | 0.995 - 1.02 g/cc | 0.0359 - 0.0368 lb/in³ | |
Lord Adhesives 513 Fast Cure, Non-Sagging Acrylic Adhesive Lord 500 SeriesLord 500 Series Acrylic Adhesives bond plastics and prepared metals; they offer excellent adhesion to both thermoplastics and thermoset plastics. They are available with varying handi.. |
|||
Density | 0.971 - 1.02 g/cc | 0.0351 - 0.0368 lb/in³ | |
Lord Adhesives 660 White, Non Sag, Fast Set for FRP Acrylic Adhesive Lord Adhesives 660 White, Non Sag, Fast Set for FRP Acrylic AdhesiveLord 660 Acrylic Adhesive bonds FRP (fiber-reinforced plastics) with minimal surface preparation. Lord 660 can cross-bond FRP to m.. |
|||
Density | 0.980 - 1.02 g/cc | 0.0354 - 0.0368 lb/in³ | ISO 1183 |
Austin Novel Materials Texalan® 765A PCL TPU Description: Good abrasion resistance, tensile strength, oil resistance and heat resistance which can be used in mechanic parts and various industry parts.Information from Dawnentech |
|||
Density | 0.960 - 1.02 g/cc @Temperature 280 - 330 °C |
0.0347 - 0.0368 lb/in³ @Temperature 536 - 626 °F |
Average value: 1.01 g/cc Grade Count:43 |
Overview of materials for Polycarbonate, Molded This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Molded". Each property range of values reported is minimum and maximum values of appropri.. |
|||
Density | 1.01 - 1.02 g/cc | 0.0365 - 0.0368 lb/in³ | L140 |
Solvay STANNINE® LF Surfactant Identification: BLEND OF SUBSTITUTED THIOUREA AND SURFACTANTSSolubility: Soluble in acid solutions. Insoluble in water or neutral solutions.Available in: Asia Pacific, Europe, Latin America and Nort.. |