Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.946 - 0.950 g/cc | 0.0342 - 0.0343 lb/in³ | Base Resin; ASTM D1505 |
NIZHNEKAMSKNEFTEKHIM PE 4148B (484H2) High Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Density | 0.946 - 0.950 g/cc | 0.0342 - 0.0343 lb/in³ | Base Resin; ASTM D1505 |
NIZHNEKAMSKNEFTEKHIM PE 6148C (486H3) High Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Density | 0.946 - 0.950 g/cc | 0.0342 - 0.0343 lb/in³ | Base Resin; ASTM D1505 |
NIZHNEKAMSKNEFTEKHIM PE 6348K (486F3) High Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Density | 0.946 - 0.950 g/cc | 0.0342 - 0.0343 lb/in³ | Base Resin; ASTM D1505 |
NIZHNEKAMSKNEFTEKHIM PE 6348M (486F8) High Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Density | 0.946 - 0.950 g/cc | 0.0342 - 0.0343 lb/in³ | Base Resin; ASTM D1505 |
NIZHNEKAMSKNEFTEKHIM PE 6748F (486H6) High Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Density | 0.946 - 0.950 g/cc | 0.0342 - 0.0343 lb/in³ | Base Resin; ASTM D1505 |
NIZHNEKAMSKNEFTEKHIM PE 6749F (486H6) High Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Density | 0.946 - 0.950 g/cc | 0.0342 - 0.0343 lb/in³ | Base Resin; ASTM D1505 |
NIZHNEKAMSKNEFTEKHIM PE 6948C (486H3) High Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Density | 0.946 - 0.950 g/cc | 0.0342 - 0.0343 lb/in³ | Base Resin; ASTM D1505 |
NIZHNEKAMSKNEFTEKHIM PE 6949C (486H3) High Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Density | 0.928 - 0.950 g/cc | 0.0335 - 0.0343 lb/in³ | Average value: 0.938 g/cc Grade Count:30 |
Overview of materials for Medium Density Polyethylene (MDPE), Molded This property data is a summary of similar materials in the MatWeb database for the category "Medium Density Polyethylene (MDPE), Molded". Each property range of values reported is minimum and maxim.. |
|||
Density | 0.942 - 0.949 g/cc | 0.0340 - 0.0343 lb/in³ | Average value: 0.946 g/cc Grade Count:4 |
Overview of materials for High Density Polyethylene (HDPE), Copolymer Film Grade This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Copolymer Film Grade". Each property range of values reported is minim.. |
|||
Density | 0.950 - 0.950 g/cc @Temperature 285 - 285 °C |
0.0343 - 0.0343 lb/in³ @Temperature 545 - 545 °F |
Average value: 0.950 g/cc Grade Count:1 |
Overview of materials for Nylon 66, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Impact Grade". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Density | 0.943 - 0.949 g/cc | 0.0341 - 0.0343 lb/in³ | |
Kazanorgsintez 293-285 High Density Polyethylene Composite, Film Grade Production Method: Compositions are achieved by ethylene copolymerization by gaseous-phase method at low pressure using complex catalysts on carrier material. Application: HDPE compositions are .. |
|||
Density | 0.943 - 0.949 g/cc | 0.0341 - 0.0343 lb/in³ | |
Kazanorgsintez 293-285D High Density Polyethylene Composite, Film Grade Production Method: Compositions are achieved by ethylene copolymerization by gaseous-phase method at low pressure using complex catalysts on carrier material. Application: HDPE compositions are .. |
|||
Density | 0.943 - 0.949 g/cc | 0.0341 - 0.0343 lb/in³ | |
Kazanorgsintez 297-285 High Density Polyethylene Composite Production Method: Compositions are achieved by ethylene copolymerization by gaseous-phase method at low pressure using complex catalysts on carrier material. Application: HDPE compositions 296-.. |
|||
Density | 0.943 - 0.949 g/cc | 0.0341 - 0.0343 lb/in³ | |
Kazanorgsintez 297-285D High Density Polyethylene Composite Production Method: Compositions are achieved by ethylene copolymerization by gaseous-phase method at low pressure using complex catalysts on carrier material. Application: HDPE compositions 296-.. |
|||
Density | 0.944 - 0.950 g/cc | 0.0341 - 0.0343 lb/in³ | ASTM D792-98 |
Ipiranga Petrochem HD 7555 LS-L HDPE IPQ produces High Density Polyethylene (HDPE) for use by different segments of the plastics molding industry in several processes, including blow molding, extrusion and injection molding.To produce .. |
|||
Density | 0.925 - 0.950 g/cc | 0.0334 - 0.0343 lb/in³ | ASTM D1505 |
Micropol Microlink XL Crosslinkable Polyethylene Characteristics: exceptional toughness, exceptional enviromental stress cracking resistance, outstanding low temperature impact resistance down to -40°C, fully stabilized for outdoor use world wi.. |
|||
Density | 0.943 - 0.949 g/cc | 0.0341 - 0.0343 lb/in³ | |
Kazanorgsintez 293-285SK High Density Polyethylene Composite, Film Grade Production Method: Compositions are achieved by ethylene copolymerization by gaseous-phase method at low pressure using complex catalysts on carrier material. Application: HDPE compositions are .. |
|||
Density | 0.945 - 0.949 g/cc | 0.0341 - 0.0343 lb/in³ | ASTM D792-98 |
Ipiranga Petrochem GM 7040 G HDPE IPQ produces High Density Polyethylene (HDPE) for use by different segments of the plastics molding industry in several processes, including blow molding, extrusion and injection molding.To produce .. |
|||
Density | 0.940 - 0.950 g/cc | 0.0340 - 0.0343 lb/in³ | |
Solvay CATAFOR® CA80 Surfactant Identification: QUATERNARY AMMONIUM ETHOSULPHATECAS: 68308 – 64 – 5Solubility: Readily soluble in ethyl alcohol, butanol chloroform, trichloroethylene, ethyl acetate and water.Solvent: n-B.. |
|||
Density | 0.910 - 0.950 g/cc | 0.0329 - 0.0343 lb/in³ | ISO 1183 |
Fainplast Compounds Hax™ CAT 100T Catalyst for Cable Compound Catalyst for cross-linking Fainplast Compounds' polyolefin based HFFR silane grafted compoundGrade description:• Low reactive catalystInformation provided by Fainplast Compounds |
|||
Density | 0.910 - 0.950 g/cc | 0.0329 - 0.0343 lb/in³ | ISO 1183 |
Fainplast Compounds Hax™ CAT 103T Catalyst for Cable Compound Catalyst for cross-linking Fainplast Compounds' polyolefin based HFFR silane grafted compoundGrade description:• High reactive cataylstInformation provided by Fainplast Compounds |
|||
Density | 0.910 - 0.950 g/cc | 0.0329 - 0.0343 lb/in³ | ISO 1183 |
Fainplast Compounds Hax™ CAT 111 Catalyst for Cable Compound Catalyst for cross-linking Fainplast Compounds' polyolefin based HFFR silane grafted compoundGrade description:• Cataylst for extreme ageing conditionsInformation provided by Fainplast Compounds |
|||
Density | 0.910 - 0.950 g/cc | 0.0329 - 0.0343 lb/in³ | ISO 1183 |
Fainplast Compounds Hax™ CAT 113 Catalyst for Cable Compound Catalyst for cross-linking Fainplast Compounds' polyolefin based HFFR silane grafted compoundGrade description:• Cataylst for extreme ageing conditionsInformation provided by Fainplast Compounds |
|||
Density | 0.910 - 0.950 g/cc | 0.0329 - 0.0343 lb/in³ | ISO 1183 |
Fainplast Compounds Hax™ CAT 115/1 Catalyst for Cable Compound Catalyst for cross-linking Fainplast Compounds' polyolefin based HFFR silane grafted compoundGrade description:• High reactive cataylstInformation provided by Fainplast Compounds |
|||
Density | 0.910 - 0.950 g/cc | 0.0329 - 0.0343 lb/in³ | ISO 1183 |
Fainplast Compounds Hax™ CAT 115LS Catalyst for Cable Compound Catalyst for cross-linking Fainplast Compounds' polyolefin based HFFR silane grafted compoundGrade description:• Low reactive catalystInformation provided by Fainplast Compounds |
|||
Density | 0.940 - 0.950 g/cc | 0.0340 - 0.0343 lb/in³ | Average value: 0.941 g/cc Grade Count:27 |
Overview of materials for Ionomer, Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Ionomer, Film Grade". Each property range of values reported is minimum and maximum values of appropriat.. |
|||
Density | 0.900 - 0.950 g/cc | 0.0325 - 0.0343 lb/in³ | DIN 52004 |
Lucobit Lucosol® Bitumen Road Binder Lucosol is a solvent based bitumen road binder made out of selected bitumen qualities and hydrocarbon solventsInformation provided by Lucobit AG |