Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 7.71 g/cc | 0.279 lb/in³ | Sintered |
Kinetics MIM K3 Heat Treat K3 is a custom Mo-Fe alloy that provides improved fatigue properties over many other steel alloys while still maintaining good strength components, industrial or structural components and other appl.. |
|||
Density | 7.71 g/cc | 0.279 lb/in³ | Sintered |
Kinetics MIM K3 Heat Treat as Sintered K3 is a custom Mo-Fe alloy that provides improved fatigue properties over many other steel alloys while still maintaining good strength components, industrial or structural components and other appl.. |
|||
Density | 7.72 g/cc | 0.279 lb/in³ | |
Latrobe LSSâ„¢ D5 Tool Steel (ASTM D5) TLS D5 tool steel is an air hardening, high-carbon, high-chromium, tool steel that is characterized by a cobalt addition which provides unique resistance to galling and pick-up. The cobalt also impa.. |
|||
Density | 7.72 g/cc | 0.279 lb/in³ | Weld Deposit Property |
The NanoSteel® Company SHS 9290 PTAW Steel Alloy, Atomized Powder Coating Description: SHS 9290 PTAW is an iron based steel alloy with a near nanoscale (submicron) microstructure that features extreme wear and abrasion resistance with high toughness. SHS 9290 PTA.. |
|||
Density | 7.73 g/cc | 0.279 lb/in³ | |
Williams Advanced Alloys WS217 Solder All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys |
|||
Density | 7.72 g/cc | 0.279 lb/in³ | hardened to 62 HRC |
Bohler-Uddeholm AISI A2 Cold Work Tool Steel Description: AISI A2 is an air- or oil hardening chromiummolybdenum-vanadium alloyed tool steel characterized byAISI A2 is characterized by: Good machinability High stability after hardening High c.. |
|||
Density | 7.72 g/cc @Temperature 199 °C |
0.279 lb/in³ @Temperature 390 °F |
hardness of 40 HRC |
Bohler-Uddeholm UDDEHOLM ALVAR 14 Hot Work Tool Steel Alvar 14 is a chromium-nickel-molybdenumvanadium alloyed steel ALVAR 14 is characterized by: Good toughnessGood resistance to high thermal stresses Good stability in hardeningGood through-hardening.. |
|||
Density | 7.72 g/cc | 0.279 lb/in³ | |
Carpenter Extendo-Die® Hot Work Die Steel, Tempered 538°C (1000°F) Data provided by Carpenter Technology Corporation.This steel combines extreme toughness with good red hardness in large section sizes. This alloy may also be considered for many cold work applicati.. |
|||
Density | 7.72 g/cc | 0.279 lb/in³ | |
Carpenter Extendo-Die® Hot Work Die Steel, Tempered 560°C Data provided by Carpenter Technology Corporation.This steel combines extreme toughness with good red hardness in large section sizes. This alloy may also be considered for many cold work applicati.. |
|||
Density | 7.72 g/cc | 0.279 lb/in³ | |
Assab Steels ASSAB 88 Cold Work Steel ASSAB 88 (SLEIPNER) is a chromium-molybdenum-vanadium alloyed tool steel which is characterized by:Good wear resistanceGood chipping resistanceHigh compressive strengthHigh hardness (>60HRC) after h.. |
|||
Density | 7.72 g/cc | 0.279 lb/in³ | |
ATI Allegheny Ludlum Martensitic Stainless Steel Type 425 Mod, Hardened + 538°C Temper Allegheny Ludlum Type 425 Mod is a hardenable straight-chromium stainless steel which combines superior wear resistance of high carbon alloys with the excellent corrosion resistance of chromium stai.. |
|||
Density | 7.72 g/cc | 0.279 lb/in³ | |
ATI Allegheny Ludlum Martensitic Stainless Steel Type 425 Mod, Hardened + 316°C Temper Allegheny Ludlum Type 425 Mod is a hardenable straight-chromium stainless steel which combines superior wear resistance of high carbon alloys with the excellent corrosion resistance of chromium stai.. |
|||
Density | 7.73 g/cc | 0.279 lb/in³ | |
ATI Allegheny Ludlum Stainless Steel AL 410S™ (UNS S41008) Allegheny Ludlum Al 410S™ stainless steel is a low-carbon modification of Type 410 stainless steel. Low carbon and optionally a small addition of titanium and /or columbium minimize austenite form.. |
|||
Density | 7.72 g/cc | 0.279 lb/in³ | |
ATI Allvac® Vasco® 13-8Mo Precipitation Hardening Steel, Heat Treatment: 927°C (1700°F) + Age Data provided by Allvac.Applications: Airframe structurals, missile components, valve parts, fasteners, chemical process equipment. |
|||
Density | 7.72 g/cc | 0.279 lb/in³ | |
Carpenter Extendo-Die® Hot Work Die Steel, Tempered 593°C Data provided by Carpenter Technology Corporation.This steel combines extreme toughness with good red hardness in large section sizes. This alloy may also be considered for many cold work applicati.. |
|||
Density | 7.72 g/cc | 0.279 lb/in³ | |
Carpenter Extendo-Die® Hot Work Die Steel, Tempered 621°C Data provided by Carpenter Technology Corporation.This steel combines extreme toughness with good red hardness in large section sizes. This alloy may also be considered for many cold work applicati.. |
|||
Density | 7.72 g/cc | 0.279 lb/in³ | |
ATI Allegheny Ludlum Martensitic Stainless Steel Type 425 Mod, Hardened + 204°C Temper Allegheny Ludlum Type 425 Mod is a hardenable straight-chromium stainless steel which combines superior wear resistance of high carbon alloys with the excellent corrosion resistance of chromium stai.. |
|||
Density | 7.73 g/cc | 0.279 lb/in³ | |
AK Steel 410 Cb Martensitic Stainless steel AK Steel 410 Cb is an improved version of standard Type 410. The addition of columbium offers 3 major advantages: 1) Greater ease in heat treating, 2) Higher strength and toughness, 3) Improved gra.. |
|||
Density | 7.73 g/cc | 0.279 lb/in³ | |
ATI Allegheny Ludlum Martensitic Stainless Steel Type 420, Hardened + 288°C Temper Allegheny Ludlum Type 420 is a hardenable straight-chromium stainless steel which combines superior wear resistance of high carbon alloys with the excellent corrosion resistance of chromium stainles.. |
|||
Density | 7.73 g/cc | 0.279 lb/in³ | |
ATI Allegheny Ludlum Martensitic Stainless Steel Type 420, Hardened + 538°C Temper Allegheny Ludlum Type 420 is a hardenable straight-chromium stainless steel which combines superior wear resistance of high carbon alloys with the excellent corrosion resistance of chromium stainles.. |
|||
Density | 7.73 g/cc | 0.279 lb/in³ | |
ATI Allegheny Ludlum Martensitic Stainless Steel Type 420, Hardened + 649°C (1200°F) Temper Allegheny Ludlum Type 420 is a hardenable straight-chromium stainless steel which combines superior wear resistance of high carbon alloys with the excellent corrosion resistance of chromium stainles.. |
|||
Density | 7.72 g/cc | 0.279 lb/in³ | |
ATI Allegheny Ludlum Martensitic Stainless Steel Type 425 Mod, Annealed Allegheny Ludlum Type 425 Mod is a hardenable straight-chromium stainless steel which combines superior wear resistance of high carbon alloys with the excellent corrosion resistance of chromium stai.. |
|||
Density | 7.72 g/cc | 0.279 lb/in³ | |
ATI Allegheny Ludlum Martensitic Stainless Steel Type 425 Mod, Hardened + 288°C Temper Allegheny Ludlum Type 425 Mod is a hardenable straight-chromium stainless steel which combines superior wear resistance of high carbon alloys with the excellent corrosion resistance of chromium stai.. |
|||
Density | 7.72 g/cc | 0.279 lb/in³ | |
ATI Allegheny Ludlum Martensitic Stainless Steel Type 425 Mod, Hardened + 482°C Temper Allegheny Ludlum Type 425 Mod is a hardenable straight-chromium stainless steel which combines superior wear resistance of high carbon alloys with the excellent corrosion resistance of chromium stai.. |
|||
Density | 7.72 g/cc | 0.279 lb/in³ | |
ATI Allegheny Ludlum Martensitic Stainless Steel Type 425 Mod, Hardened + 649°C (1200°F) Temper Allegheny Ludlum Type 425 Mod is a hardenable straight-chromium stainless steel which combines superior wear resistance of high carbon alloys with the excellent corrosion resistance of chromium stai.. |
|||
Density | 7.72 g/cc | 0.279 lb/in³ | |
Schmolz + Bickenbach Cryodur® 2363 (A-2) Cold Work Die Steel Description: Cryodur® 2363 is a cold-work steel developed for an excellent combination of wear resistance and toughness and Supplied in the annealed conditionCharacteristics: Good wear resistance; .. |
|||
Density | 7.72 g/cc | 0.279 lb/in³ | |
Schmolz + Bickenbach IMRE™ Stainless Steel Bar Description: Ugine IMRE™ is a chromium stainless steel with improved magnetic properties used in solenoid valves. IMRE™ is at 18% chromium ferritic stainless steel with 2% Mo designed to withstand.. |
|||
Density | 7.73 g/cc | 0.279 lb/in³ | |
ATI Allegheny Ludlum Martensitic Stainless Steel Type 420, Hardened + 204°C Temper Allegheny Ludlum Type 420 is a hardenable straight-chromium stainless steel which combines superior wear resistance of high carbon alloys with the excellent corrosion resistance of chromium stainles.. |
|||
Density | 7.73 g/cc | 0.279 lb/in³ | |
ATI Allegheny Ludlum Martensitic Stainless Steel Type 420, Hardened + 427°C Temper Allegheny Ludlum Type 420 is a hardenable straight-chromium stainless steel which combines superior wear resistance of high carbon alloys with the excellent corrosion resistance of chromium stainles.. |
|||
Density | 7.73 g/cc | 0.279 lb/in³ | |
ATI Allegheny Ludlum Martensitic Stainless Steel Type 420, Hardened + 482°C Temper Allegheny Ludlum Type 420 is a hardenable straight-chromium stainless steel which combines superior wear resistance of high carbon alloys with the excellent corrosion resistance of chromium stainles.. |