Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Latrobe LSSâ„¢ D5 Tool Steel (ASTM D5)

Category Metal , Ferrous Metal , Alloy Steel , Carbon Steel , High Carbon Steel , Tool Steel , Air-Hardening Steel
Manufacturer Latrobe Steel
Trade Name LSS™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Latrobe LSSâ„¢ D5 Tool Steel (ASTM D5).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
TLS D5 tool steel is an air hardening, high-carbon, high-chromium, tool steel that is characterized by a cobalt addition which provides unique resistance to galling and pick-up. The cobalt also imparts some resistance to tempering, which makes TLS D5 suitable for some semi-hot work tooling applications.Information Provided by Timken Latrobe Steel.Timken sold Latrobe in December 2006. They are now Latrobe Specialty Steels Co.
Physical Properties Metric English Comments
Specific Gravity 7.73 g/cc
7.73 g/cc
Density 7.72 g/cc
0.279 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell C 62
62
Air Cooled from 1038°C, 30 minutes
62.5
62.5
Air Cooled from 982°C, 45 minutes
63
63
Air Cooled from 996°C, 30 minutes
Modulus of Elasticity 207 GPa
30000 ksi
Machinability 45 - 50 %
45 - 50 %
1% Carbon Steel
Izod Impact Unnotched 54.2 J
40.0 ft-lb
Air Cooled from 1010°C; 483°C Temper Temperature
70.5 J
52.0 ft-lb
Air Cooled from 1010°C; 145°C Temper Temperature
119 J
88.0 ft-lb
Air Cooled from 1010°C; 593°C Temper Temperature
Thermal Properties Metric English Comments
CTE, linear 9.88 µm/m-°C

@Temperature 38.0 - 260 °C
5.49 µin/in-°F

@Temperature 100 - 500 °F
12.02 µm/m-°C

@Temperature 38.0 - 538 °C
6.678 µin/in-°F

@Temperature 100 - 1000 °F
Component Elements Properties Metric English Comments
Carbon, C 1.5 %
1.5 %
Chromium, Cr 11.65 %
11.65 %
Cobalt, Co 2.8 %
2.8 %
Iron, Fe 82.4 %
82.4 %
Manganese, Mn 0.35 %
0.35 %
Molybdenum, Mo 0.80 %
0.80 %
Silicon, Si 0.50 %
0.50 %
Chemical Properties Metric English Comments
Critical Temperature 754 °C
1390 °F
Ar1
832 °C
1530 °F
Ac1
Users viewing this material also viewed the following: