Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Kinetics MIM K3 Heat Treat

Category Metal , Ferrous Metal , Alloy Steel , Low Alloy Steel
Manufacturer Kinetics, Inc.
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Kinetics MIM K3 Heat Treat.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
K3 is a custom Mo-Fe alloy that provides improved fatigue properties over many other steel alloys while still maintaining good strength components, industrial or structural components and other applications where compressive/tensile wear and fatigue loading is experienced. Information provided by Kinetics, Inc.
Physical Properties Metric English Comments
Density 7.71 g/cc
0.279 lb/in³
Sintered
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate >= 1590 MPa
>= 230000 psi
1720 MPa
250000 psi
Typical
Tensile Strength, Yield >= 1450 MPa
>= 210000 psi
1590 MPa
230000 psi
Typical
Elongation at Break >= 2.0 %
>= 2.0 %
in 1 inch
3.0 %
3.0 %
in 1 inch Typical
Reduction of Area >= 3.0 %
>= 3.0 %
6.0 %
6.0 %
Typical
Charpy Impact, Unnotched 40.7 J
30.0 ft-lb
1/2 size bar
Component Elements Properties Metric English Comments
Carbon, C 0.30 - 0.50 %
0.30 - 0.50 %
Iron, Fe 97.5 - 98.7 %
97.5 - 98.7 %
by difference
Molybdenum, Mo 1.0 - 2.0 %
1.0 - 2.0 %
Descriptive Properties Value Comments
Hardness R15N 87
Surface Finish 40 Ra