Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 2.13 g/cc | 0.0770 lb/in³ | Yield Density |
Honeywell ACLAR® 11A (8.00 mil) CTFE Homopolymer, Barrier Film
(discontinued **) Description: ACLAR® 11A is a CTFE homopolymer, high performance barrier film for industrial and electronics applications.Information provided by Honeywell. |
|||
Density | 2.13 g/cc | 0.0770 lb/in³ | Yield Density |
Honeywell ACLAR® 11A (4.00 mil) CTFE Homopolymer, Barrier Film
(discontinued **) Description: ACLAR® 11A is a CTFE homopolymer, high performance barrier film for industrial and electronics applications.Information provided by Honeywell. |
|||
Density | 2.13 g/cc | 0.0770 lb/in³ | Yield Density |
Honeywell ACLAR® UltRx 2000 CTFE Homopolymer, Barrier Film Description: ACLAR® UltRx 2000 is a 2 mil CTFE homopolymer high performance barrier film for the pharmaceutical and medical markets. It thermoforms well on conventional blister packaging equipmen.. |
|||
Density | 2.13 - 2.18 g/cc | 0.0770 - 0.0788 lb/in³ | ASTM D792 |
Solvay Specialty Polymers Hyflon® PFA 420 Perfluoroalkoxy (PFA) Hyflon® PFA is a family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat resistance.. |
|||
Density | 2.13 - 2.18 g/cc | 0.0770 - 0.0788 lb/in³ | ASTM D792 |
Solvay Specialty Polymers Hyflon® PFA M620 Perfluoroalkoxy (PFA) Hyflon® PFA is a unique family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat res.. |
|||
Density | 2.13 - 2.18 g/cc | 0.0770 - 0.0788 lb/in³ | ASTM D792 |
Solvay Specialty Polymers Hyflon® PFA M640 Perfluoroalkoxy (PFA) Hyflon® PFA is a unique family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat res.. |
|||
Density | 2.13 - 2.18 g/cc | 0.0770 - 0.0788 lb/in³ | ASTM D792 |
Solvay Specialty Polymers Hyflon® PFA P450 Perfluoroalkoxy (PFA) Hyflon® PFA is a unique family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat res.. |
|||
Density | 2.13 - 2.18 g/cc | 0.0770 - 0.0788 lb/in³ | ASTM D792 |
Solvay Specialty Polymers Hyflon® PFA P455 Perfluoroalkoxy (PFA) Hyflon® PFA is a unique family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat res.. |
|||
Density | 2.13 g/cc | 0.0770 lb/in³ | ASTM D792 |
Saint-Gobain Fluoroloy® A16 High Performance Seal Material General purpose material for heat and wear resistance; Recommended for dry and poorly lubricated applications; Particularly suitable for water and steam service
Information provided by Saint-Goba.. |
|||
Density | 2.13 - 2.18 g/cc | 0.0770 - 0.0788 lb/in³ | ASTM D792 |
Solvay Specialty Polymers Hyflon® MFA® 1041 Perfluoropolymer Hyflon® MFA 1041 is a high extrusion speed resin specifically designed for insulation for plenum-rated LAN cables. MFA 1041 delivers superior electrical performance in addition to its excellent f.. |
|||
Density | 2.13 - 2.19 g/cc | 0.0770 - 0.0791 lb/in³ | BS2782:Pt6 |
Dalau Dalcon 001 100% Virgin PTFE Applications & Industries:General: The static and dynamic friction coefficient are numerically equal, consequently no ’Stick Slip’ occurs.Chemical: Dynamic & shaft seals; Pipes & tubing for carryi.. |
|||
Density | 2.13 - 2.19 g/cc | 0.0770 - 0.0791 lb/in³ | BS2782:Pt6 |
Dalau Dalcon 020 Virgin PTFE, Carbon (Anti-Static) Applications & Industries: General: The static and dynamic friction coefficient are numerically equal, consequently no ’Stick Slip’ occurs. Electrical: Ideal for Anti - Static Applications; Anti -.. |
|||
Density | 2.13 g/cc | 0.0770 lb/in³ | ASTM D792 |
Plenco 6553 Phenolic, Granular, Compression Molded Two-Stage Phenolic. PLENCO 06553 is a phenolic molding compound, formulated specifically for automotive brake pistons. 06553 exhibits excellent dimensional stability, and resistance to brake fluids.. |
|||
Density | 2.13 g/cc | 0.0770 lb/in³ | ISO 1183 |
Polyplastics Freqtis® P0813A (PPS/LCP), Molding Compound Both base resins (PPS and LCP) exhibit excellent heat resistance, dimensional stability and molding processability. Therefore Freqtis® is widely used for surface mounted electronic components. In .. |
|||
Density | 2.13 g/cc | 0.0770 lb/in³ | |
Corning 7070 Lithia Potash Borosilicate Crushed/Powdered Glass Available in mesh sizes 4 through 325 and can be customized. Devitrifies before reaching a softening point. Used for sealing and other applications.Information provided by Corning Incorporated. |
|||
Density | 2.13 g/cc | 0.0770 lb/in³ | |
Cytec Thornel® P-100 2K Carbon Fiber, Pitch Precursor Data provided by the manufacturer, Amoco Performance Products, Inc.Continuous filament, ultra high modulus fibers consisting of 2000 filaments in a one-ply construction.0.32 m/g yield, 0 or 32 tpm t.. |
|||
Density | 2.13 g/cc | 0.0770 lb/in³ | |
Cytec Thornel® P-100S 2K Carbon Fiber, Pitch Precursor Data provided by the manufacturer, Amoco Performance Products, Inc.Continuous filament, ultra high modulus fibers consisting of 2000 filaments in a one-ply construction. The fiber surface has been .. |
|||
Density | 2.13 g/cc | 0.0770 lb/in³ | |
Cytec Thornel® P-120 2K Carbon Fiber, Pitch Precursor Data provided by the manufacturer, Amoco Performance Products, Inc.Continuous filament, ultra high modulus fibers consisting of 2000 filaments in a one-ply construction.2000 filaments/strand, 0.33 m.. |
|||
Density | 2.13 g/cc | 0.0770 lb/in³ | |
Cytec Thornel® P-120S 2K Carbon Fiber, Pitch Precursor Data provided by the manufacturer, Amoco Performance Products, Inc.Continuous filament, ultra high modulus fibers consisting of 2000 filaments in a one-ply construction. The fiber surface has been .. |
|||
Density | 2.13 - 2.19 g/cc | 0.0770 - 0.0791 lb/in³ | BS2782:Pt6 |
Dalau Dalcon 001 100% Virgin PTFE Applications & Industries:General: The static and dynamic friction coefficient are numerically equal, consequently no ’Stick Slip’ occurs.Chemical: Dynamic & shaft seals; Pipes & tubing for carryi.. |
|||
Density | 2.13 - 2.19 g/cc | 0.0770 - 0.0791 lb/in³ | BS2782:Pt6 |
Dalau Dalcon 020 Virgin PTFE, Carbon (Anti-Static) Applications & Industries: General: The static and dynamic friction coefficient are numerically equal, consequently no ’Stick Slip’ occurs. Electrical: Ideal for Anti - Static Applications; Anti -.. |
|||
Density | 2.13 g/cc | 0.0770 lb/in³ | |
BASF Heligoen® Green L 8690 Color Additive Description: Phthalocyanine green with excellent rheologyChemical Structure: Cu-phthalocyanine, chlorinatePhysical form: PowderSuitable for: Baking systems, Waterborn systems, Acrylic-isocyanate sys.. |
|||
Density | 2.13 - 2.20 g/cc | 0.0770 - 0.0795 lb/in³ | ASTM D792 |
Guarniflon PTFE G200 Polytetrafluoroethylene A virgin PTFE with low coefficient of friction, excellent chemical inertness, non-adhesive surface, wide service temperature range, and excellent dielectric propertiesInformation provided by Guarnif.. |
|||
Density | 2.13 - 2.20 g/cc | 0.0770 - 0.0795 lb/in³ | ASTM D792 |
Guarniflon PTFE G300 Polytetrafluoroethylene A virgin PTFE with low coefficient of friction, excellent chemical inertness, non-adhesive surface, wide service temperature range, and excellent dielectric propertiesInformation provided by Guarnif.. |