Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.96 g/cc | 0.0708 lb/in³ | ISO 1183 |
Solvay Specialty Polymers Primef® 7002 Polyphenylene Sulfide (PPS), 65% GlassMineral
(discontinued **) Primef 7002 is a 65% mineral/glass fiber reinforced polyphenylene sulfide (PPS). This grade offers higher fluidity than Primef 7010 (also 65% mineral/glass fiber), but with somewhat lower mechanical.. |
|||
Density | 1.96 g/cc | 0.0708 lb/in³ | ISO 1183 |
Solvay Specialty Polymers Primef® 7010 Polyphenylene Sulfide (PPS), 65% GlassMineral
(discontinued **) Primef 7010 is a 65% mineral/glass fiber reinforced polyphenylene sulfide (PPS). This grade offers improved mechanical properties versus Primef 7002 (also 65% mineral/glass fiber), but with less flu.. |
|||
Density | 1.96 g/cc | 0.0708 lb/in³ | |
IDI Composites 44-10 Thermoset Polyester, Molding Multi-purpose medium strength material with excellent surface appearance, corrosion resistance, and V-O flame resistance.Data provided by the manufacturer. |
|||
Density | 1.96 g/cc | 0.0708 lb/in³ | ISO R 1183 |
Multibase Multibatch® ME 50043 Anti-blocking Masterbatch LLDPE. 50% CaCO3, 30%TiO2FilledWhiteInformation provided by Multibase |
|||
Density | 1.96 g/cc | 0.0708 lb/in³ | |
LATI Latigray 53/22-01 CX/70 PP Homopolymer, Impact Modified Radiopaque compound based on Polypropylene homopolymer (PPh), impact modified. Special mineral filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformati.. |
|||
Density | 1.96 g/cc | 0.0708 lb/in³ | |
Saint-Gobain Rulon® DC1042 Bearing/Seal PTFE Can be used in a wide range of sealing and bearing applications. Rulon DC1042 is ideal for applications in which the bearing, seal is in contact with harsh chemicals or in applications where electri.. |
|||
Density | 1.96 g/cc | 0.0708 lb/in³ | |
Saint-Gobain Rulon® DC7035 Bearing/Seal PTFE Offers electrical conductivity in a low wear, self lubricating bearing material. This material is ideal in applications where static dissipation is needed. DC7035 is often used as a static bleed mec.. |
|||
Density | 1.96 g/cc | 0.0708 lb/in³ | ASTM D 792 |
SABIC Innovative Plastics LNP Thermocomp OFJ66 PPS - Linear LNP* Thermocomp* OFJ66 is a compound based on PPS - Linear resin containing Glass Fiber, Mineral. Added features of this material include: Low Warpage.This data was supplied by SABIC-IP for the Ame.. |
|||
Density | 1.96 g/cc | 0.0708 lb/in³ | GB/T 1033.1-2008 |
Sichuan Deyang Haton® hMR61 Polyphenylene Sulfide, Glass & Mineral Reinforced Injection moldingInformation provided by Sichuan Deyang Chemical Co., LTD |
|||
Density | 1.96 g/cc | 0.0708 lb/in³ | ASTM D 792 |
SABIC Innovative Plastics LNP Thermocomp OFJ66 PPS - Linear (Asia Pacific) LNP* Thermocomp* OFJ66 is a compound based on PPS - Linear resin containing Glass Fiber, Mineral. Added features of this material include: Low Warpage.This data was supplied by SABIC-IP for the Asi.. |
|||
Density | 1.96 g/cc | 0.0708 lb/in³ | ASTM D792 |
Toyobo TS201 HS PPS, Glass Fiber/Mineral Reinforced Key Feature: High stiffness, high toughnessHigh performance injection-molding resin created from crystalline polyphenylene sulfide, using a special formulation technology developed by Toyobo. Excel.. |
|||
Density | 1.96 g/cc | 0.0708 lb/in³ | ASTM D792 |
Toyobo TS201 PPS, Glass Fiber/Mineral Reinforced Key Feature: Standard high stiffness - used for metal replacementHigh performance injection-molding resin created from crystalline polyphenylene sulfide, using a special formulation technology devel.. |
|||
Density | 1.96 - 2.00 g/cc | 0.0708 - 0.0723 lb/in³ | ISO R 1183 |
Fainplast Compounds CRA 84 Flexible PVC, Flame Retardant Electrical Bedding Flame retardant bedding |
|||
Density | 1.96 - 2.16 g/cc | 0.0708 - 0.0780 lb/in³ | Molded |
Bulk Molding Compounds BMC T9 General Purpose Molding Compound BMC T9 is a low cost, general purpose bulk molding compound designed for the electrical industry. It is UL listed and is used extensively in the manufacture of residential circuit breakers. BMC T9.. |
|||
Density | 1.96 g/cc | 0.0708 lb/in³ | ASTM D1475 |
Aptek DAT-A-THERM 1000 Electrically insulating urethane film DAT-A-THERM 1000 is a tough, flexible, void free, electrically insulating urethane film designed to fill air gaps and dissipate heat between devices and substrates. DAT-A-THERM 1000 film is a 100% s.. |
|||
Density | 1.96 g/cc @Temperature -100 °C |
0.0708 lb/in³ @Temperature -148 °F |
|
3M Novec™ 649 Engineered Fluid 3M™ Novec™ 649 Engineered Fluid is a clear, colorless and low odor fluid, one in a line of 3M products designed as replacements for ozone depleting substances (ODSs) and compounds with high global.. |
|||
Density | 1.96 g/cc | 0.0708 lb/in³ | 50% Resin Content; Internal Method |
Park Electrochemical Nelco® N4000-11 BC® Buried Capacitance™ Epoxy Laminate and Prepreg The Nelco® N4000-11 is a CAF resistant, high Tg (175º C by DSC) multifunctional epoxy dielectric substrate. This material is formulated to provide the PWB manufacturer and OEM with vastly improved.. |
|||
Density | 1.96 g/cc | 0.0708 lb/in³ | 50% Resin Content; Internal Method |
Park Electrochemical Nelco® N4000-11 Multifunctional Epoxy Laminate and Prepreg The Nelco® N4000-11 is a CAF resistant, high Tg (175º C by DSC) multifunctional epoxy dielectric substrate. This material is formulated to provide the PWB manufacturer and OEM with vastly improved.. |