Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.86 g/cc | 0.0672 lb/in³ | ASTM D792 |
Multibase Multi-Flex® TPE A 8832 E BLK Multi-Flex TPE contains Kraton™ G.Data provided by Multibase. |
|||
Density | 1.86 g/cc | 0.0672 lb/in³ | ASTM D792 |
Rogers Corporation RO4350B Glass-Reinforced Hydrocarbon and Ceramic Laminate with Thin Film Resistor Foil RO4000® Series High Frequency Circuit Materials are glass-reinforced hydrocarbon and ceramic (not PTFE) laminates with TICER™ TCR® Thin Film Resistor Foils. These laminates are designed for perf.. |
|||
Density | 1.86 g/cc | 0.0672 lb/in³ | 4.0 mil thickness; ASTM D792 |
Rogers Corporation RO4450B Prepreg Prepreg is commonly used to inexpensively form less critical signal layers in antenna designs. A high post-cure Tg makes RO4400 series prepreg an excellent choice for multi-layers requiring sequent.. |
|||
Density | 1.86 - 1.89 g/cc | 0.0672 - 0.0683 lb/in³ | |
Pyrotek Pyrocast AR Castable Refractory Pyrocast AR is a fused silica castable refractory inert to liquid aluminum and its alloys. It is a high strength material offering resistance to erosion and mechanical damage. Parts cast from Pyro.. |
|||
Density | 1.86 - 1.89 g/cc | 0.0672 - 0.0683 lb/in³ | |
Pyrotek Pyrocast AR FINE Castable Refractory Pyrocast AR Fine is a fine-grain fused silica castable, offering similar insulation properties, yet lighter weight that the Pyrocast AR formulation. Pyrocast AR Fine is suited for thin wall casting.. |
|||
Density | 1.86 - 1.89 g/cc | 0.0672 - 0.0683 lb/in³ | |
Pyrotek Pyrocast PCR Abrasion-Resistant Refractory Castable Pyrocast PCR is an abrasion resistant, thermal shock resistant castable. It is suitable to give exceptional resistance for conditions such as rapid heating or rapid cooling.ApplicationsCarbon anode.. |
|||
Density | 1.86 g/cc | 0.0672 lb/in³ | |
3M Dyneon™ Fluorel™ FE-5730Q Fluoroelastomer VF2 + HFP + TFE Terpolymer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 69.2%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. 69.2% F grade terpolymer with good pe.. |
|||
Density | 1.86 g/cc | 0.0672 lb/in³ | |
3M Dyneon™ Fluorel™ FT-2320 Fluoroelastomer VF2 + HFP + TFE Terpolymer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 69%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. 69% F grade terpolymer for difficult ex.. |
|||
Density | 1.86 g/cc | 0.0672 lb/in³ | |
3M Dyneon™ Fluorel™ FT-2350 Fluoroelastomer VF2 + HFP + TFE Terpolymer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 68.6%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. Improved retention of elongation afte.. |
|||
Density | 1.86 g/cc | 0.0672 lb/in³ | |
3M Dyneon™ Fluorel™ FT-2430 Fluoroelastomer VF2 + HFP + TFE Terpolymer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Non-incorporated cure polymer, 69%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, 4% Ca(OH)2, 1.4% Dihydroxy Crosslinker, 0.4% Phospho.. |
|||
Density | 1.86 g/cc | 0.0672 lb/in³ | |
3M Dyneon™ Fluorel™ FT-2481 Fluoroelastomer VF2 + HFP Dipolymer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Non-incorporated cure polymer, 68.6%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, 4% Ca(OH)2, 1.4% Dihydroxy Crosslinker, 0.4% Phosp.. |
|||
Density | 1.86 g/cc | 0.0672 lb/in³ | ISO 1183 |
Polykemi AB POLYfill PPH B8065 Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Density | 1.86 g/cc | 0.0672 lb/in³ | ISO 1183 |
Polykemi AB POLYfill PPH B8065 VT1 Polypropylene Homopolymer, Mineral Reinforced, Heat Resistant Information provided by Polykemi AB |
|||
Density | 1.86 g/cc | 0.0672 lb/in³ | |
Cookson Group Plaskon® 1002 Conventional Encapsulant
(discontinued **) Test specimens were transfer molded and post cured 4 hours at 175°C.A low cost, low stress, conventional molding compound recommended for high volume commodity-type packages that house simple linea.. |
|||
Density | 1.86 g/cc | 0.0672 lb/in³ | |
Cookson Group Plaskon® 3300SH Mineral Filled Epoxy Molding Compound
(discontinued **) Test specimens were transfer molded and post cured 4 hours at 175°C.Exhibits exceptional reliability, excellent moldability, good release characteristics and low flash. This compound is especially.. |
|||
Density | 1.86 g/cc | 0.0672 lb/in³ | ASTM D792 |
Solvay Specialty Polymers Xydar® MG-850 Liquid Crystal Polymer (LCP), 50% GlassMineral Xydar® MG-850 liquid crystal polymer (LCP) is a 50% glass/mineral reinforced injection molding grade developed for electrical/electronic applications utilizing surface mount technology. The mater.. |
|||
Density | 1.86 g/cc | 0.0672 lb/in³ | ASTM D891 |
Solvay Specialty Polymers FOMBLIN® M60 PFPE Lubricant Information provided by Solvay Solexis, Inc. |
|||
Density | 1.86 g/cc | 0.0672 lb/in³ | ASTM D891 |
Solvay Specialty Polymers FOMBLIN® W150 PFPE Lubricant Fomblin® PFPE fluorinated lubricants are used when harsh chemical environments, high temperatures or wide working-temperature ranges are encountered.Information provided by Solvay Solexis, Inc. |
|||
Density | 1.86 g/cc | 0.0672 lb/in³ | ASTM D792 |
Sumitomo Bakelite North America E 3812M-1 Mineral and Glass Filled Electrical Encapsulation Grade Epoxy E 3812M-1 is a mineral and short fiberglass filled epoxy molding compound for low pressure encapsulation molding, featuring excellent dimensional stability, good thermal shock resistance, and good e.. |
|||
Density | 1.86 g/cc | 0.0672 lb/in³ | ASTM D792 |
Plenco 1500 Polyester, Granular, Compression Molded PLENCO 01500 is a general purpose, mineral filled granular polyester molding compound, offering excellent arc and track resistance, and low post shrinkage characteristics. UL recognized under compon.. |
|||
Density | 1.86 g/cc | 0.0672 lb/in³ | ISO 1183 |
Wolf Kunststoff ZEDEX® ZX-550PV A7A Polymer Alloy Main Characteristics: Modified friction wear; Tough; Soft; Reduced wear at temperatures at 100 ° CApplications: Chemical Engineering; Laboratory Technology; Automitve Technology; Machine ToolsInfor.. |
|||
Density | 1.86 g/cc | 0.0672 lb/in³ | ASTM D792 |
Plenco 6310 Phenolic, Granular, Compression Molded PLENCO 06310 is a glass and mineral filled phenolic molding compound offering excellent heat resistance and dimensional stability. 06310 is available in black.Information supplied by Plenco. |
|||
Density | 1.86 g/cc | 0.0672 lb/in³ | ASTM D792 |
Dow Fulcrum™ Thermoplastic Glass-Filled Polyurethane Composite Rod FULCRUM Thermoplastic Composite Technology is specifically designed for the fabrication of continuous fiber composites that have greater flexibility in post-processing operations as well as higher t.. |
|||
Density | 1.86 g/cc | 0.0672 lb/in³ | Liquid |
3M Fluorinert™ FC-40 Electronic Liquid 3M™ Fluorinert™ Liquid FC-40 is a non-conductive, thermally and chemically stable fluid ideal for single phase heat transfer fluid applications, especially in the electronics and semiconductor ind.. |
|||
Density | 1.86 g/cc | 0.0672 lb/in³ | Liquid |
3M Fluorinert™ FC-43 Electronic Liquid 3M™ Fluorinert™ Liquid FC-43 is a non-conductive, thermally and chemically stable liquid ideal for many single phase heat transfer fluid applications, especially in the electronics and semiconduct.. |
|||
Density | 1.86 g/cc | 0.0672 lb/in³ | ISO 1183 |
Vyncolit Neopreg Kinel® SK60 L8F Glass Fiber Reinforced Molding Compound Medium flow, epoxy based molding compound long glass fiber reinforced with excellent long term property retention over a wide temperature range and climate conditions. It is particularly suited f.. |
|||
Density | 1.86 g/cc | 0.0672 lb/in³ | ASTM D792 |
Sumitomo Bakelite North America FS-6 CAF Mineral Filled Diallyl Phthalate Isophthalate DAP Resin Isomer. Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Meets the requirements of ASTM D5948 Type MI.. |
|||
Density | 1.86 g/cc | 0.0672 lb/in³ | Relative Density; ISO 1183 |
Sumitomo Bakelite North America RX® 852 Novolac Phenolic Fiberglass reinforced phenolic novolac compound with good dimensional stability and good strength at elevated temperatures.Information provided by Vyncolit, a Sumitomo Bak Group |
|||
Density | 1.86 g/cc | 0.0672 lb/in³ | |
Cookson Group Plaskon® 3300S Mineral Filled Novolac Epoxy Molding Compound
(discontinued **) Test specimens were transfer molded and post cured 4 hours at 175°C.A low stress, flame retardant, novolac hardened epoxy molding compound designed to provide hermeticity protection exceeding that .. |