Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Dow Fulcrum™ Thermoplastic Glass-Filled Polyurethane Composite Rod

Category Polymer , Thermoplastic , Polyurethane, TP , Thermoplastic Polyurethane (TPUR), Glass Fiber Reinforced
Manufacturer Dow Chemical
Trade Name Fulcrum™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Fulcrum™ Thermoplastic Glass-Filled Polyurethane Composite Rod.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
FULCRUM Thermoplastic Composite Technology is specifically designed for the fabrication of continuous fiber composites that have greater flexibility in post-processing operations as well as higher toughness and faster production rates than traditional composite materials. The technology, using ISOPLAST® Engineering Thermoplastic Polyurethane (ETPU), allows production of hollow as well as solid elongated profiles using pultrusion techniques.Information provided by Dow Chemical.
Physical Properties Metric English Comments
Density 1.86 g/cc
0.0672 lb/in³
ASTM D792
Filler Content 66 %
66 %
Glass
Mechanical Properties Metric English Comments
Elongation at Break 1.5 %
1.5 %
In Compression; ASTM D695
Flexural Strength 1050 MPa
152000 psi
ASTM D4476
Flexural Modulus 40.0 GPa
5800 ksi
ASTM D4476
Compressive Strength 440 MPa
63800 psi
ASTM D695
Compressive Modulus 35.0 GPa
5080 ksi
ASTM D695
Shear Strength 55.0 MPa
7980 psi
ASTM D3846
Izod Impact, Notched 41.0 J/cm
76.8 ft-lb/in
ASTM D256
Izod Impact, Unnotched 59.0 J/cm
111 ft-lb/in
3 strips glued together; ASTM D4812
Users viewing this material also viewed the following: