Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.52 g/cc | 0.0549 lb/in³ | ISO 1183 |
Polykemi AB SCANMID 6 B11^ F30 FR5 Nylon 6, Glass Fiber Reinforced, Flame Retardant Information provided by Polykemi AB |
|||
Density | 1.52 g/cc | 0.0549 lb/in³ | Crystaline; ISO 1183 |
Victrex® PEEK 90GL30 BLACK EU 30% Glass Fiber Filled, PolyEtherEtherKetone High performance thermoplastic material, 30% glass fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding, very easy flow, FDA and EU food contact compliant, .. |
|||
Density | 1.52 g/cc | 0.0549 lb/in³ | Crystalline; ISO 1183 |
Victrex® PEEK 90GL30 Polyetheretherketone, 30% Glass Fiber Reinforced Product Description:High performance thermoplastic material, 30% glass fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, very easy flow, FDA food conta.. |
|||
Density | 1.52 g/cc | 0.0549 lb/in³ | ISO 1183 |
Hexion Bakelite™ PF 7592 Phenolic Formaldehyde Resin, Galvanized, Conductive
(discontinued **) Phenolic molding compound, inorganically/organically filled. Shrinkage fies compatible to values of UP 3310 and PF 2560. Electroplateable.Application areas: Chromium plated oven strips.Information.. |
|||
Density | 1.52 g/cc | 0.0549 lb/in³ | ASTM D792 |
LG Chemical Lupox® PBT-GP-2300 30% GFR PBT Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Density | 1.52 g/cc | 0.0549 lb/in³ | ISO 1183/A |
Solvay TECHNYL® A 218HP V50 PA66, 35% glass fiber, DRY Description: TECHNYL® A 218HP V50 is a polyamide 66, reinforced with 50% of glass fiber, heat stabilized, for injection molding. This product is available in black color.Benefits: The product off.. |
|||
Density | 1.52 g/cc | 0.0549 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP LUBRICOMP RFL36L PA 66 (Asia Pacific) LNP* Lubricomp* RFL36L is a compound based on Nylon 66 resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated, Low Extractible. |
|||
Density | 1.52 g/cc | 0.0549 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Valox® EH7025AG PBT+PET Valox EH7025AG is a mineral filled PBT/PET that offers good surface appearance, good flow and good heat performance. EH7025AG was developed for automotiove bezel application. |
|||
Density | 1.52 g/cc | 0.0549 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Valox® IQNH4550 PBT (Asia Pacific) Valox* iQNH4550 resin is a non-brominated/non-chlorinated flame retardant product based on an environmentally sustainable Valox iQ* PBT resin. Post-consumer recycle (PCR) usage is 31% based on EPEAT.. |
|||
Density | 1.52 g/cc | 0.0549 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP THERMOCOMP JF004ER PES (Europe-Africa-Middle East) LNP* Thermocomp* JF-1004 S-3 is a compound based on Polyethersulfone resin containing Glass Fiber. Added features of this material include: Mold Release. |
|||
Density | 1.52 g/cc | 0.0549 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP Thermocomp RW008XXZ PA 66 LNP* Thermocomp* RW008XXZ is a compound based on Nylon 6/6 resin containing Wollastonite.This data was supplied by SABIC-IP for the Americas region. |
|||
Density | 1.52 g/cc | 0.0549 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Valox® IQNH4550 PBT (Europe-Africa-Middle East) Valox* iQNH4550 resin is a non-brominated/non-chlorinated flame retardant product based on an environmentally sustainable Valox iQ* PBT resin. Post-consumer recycle (PCR) usage is 31% based on EPEAT.. |
|||
Density | 1.52 g/cc | 0.0549 lb/in³ | ASTM D 792 |
SABIC Innovative Plastics LNP Thermocomp DF008P PC (Asia Pacific) LNP* THERMOCOMP* DF008P is a compound based on Polycarbonate resin containing Glass Fiber. Added features of this material include: Exceptional Processing.This data was supplied by SABIC-IP for the.. |
|||
Density | 1.52 g/cc | 0.0549 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP EF006H PEI (Asia Pacific) LNP* Thermocomp* EF006H is a compound based on Polyetherimide resin containing Glass Fiber. |
|||
Density | 1.52 g/cc | 0.0549 lb/in³ | ISO 1183 |
Polyplastics Duranex® HN7315 Polybutylene Terephthalate (PBT), Low warpage, 15% GF filled DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
Density | 1.52 g/cc | 0.0549 lb/in³ | ISO 1183 |
Polyplastics Duranex® 7307B Polybutylene Terephthalate (PBT), Super low warpage, GB filled DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
Density | 1.52 - 1.55 g/cc | 0.0549 - 0.0560 lb/in³ | |
Chengdu Polyster RPM440 Flame Retardant Masterbatch RPM 440 is a flame retardant phosphorus based additive designed for use in reinforced polyamide resins. It is halogen-free and has good flame retardant performance. Red pellet form. Used for electri.. |
|||
Density | 1.52 g/cc | 0.0549 lb/in³ | ISO 1183 |
DSM Stanyl® TE250F3 Nylon 46-15% Glass Reinforced (European and Asian Grade) (Dry) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Density | 1.52 g/cc | 0.0549 lb/in³ | ASTM D792 |
Entec Hylox® 9030 PBT, 30% Glass Reinforced Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Ente.. |
|||
Density | 1.52 - 1.56 g/cc | 0.0549 - 0.0564 lb/in³ | ISO R 1183 |
Fainplast Compounds GA 89/2 Flexible PVC, Flame Retardant Sheathing Operating temperature 75°C |
|||
Density | 1.52 - 1.56 g/cc | 0.0549 - 0.0564 lb/in³ | IEC 60811 |
Fainplast Compounds HAX HF 4522 Halogen Free PVC High flame retardancy |
|||
Density | 1.52 g/cc | 0.0549 lb/in³ | MIL-S-8784 |
3M AC-215 Class B-2 Aerospace Sealant 3M Aerospace Sealant AC-215 Class B are two-part, polysulfide access door sealants for faying surfaces where easy separation of jointed surfaces is required. They are a highly thixotropic reddish pa.. |
|||
Density | 1.52 g/cc | 0.0549 lb/in³ | cured 14 days @ 50% RH |
3M AC-730 Class B-6 Aerospace Sealant 3M Aerospace Sealant AC-730 Class B are fast cure, two-part, manganese-cured, non-chromate containing corrosion inhabiting sealants. These Sealants provide an effective barrier against the common ca.. |
|||
Density | 1.52 g/cc | 0.0549 lb/in³ | ISO 1183 |
BASF Ultramid® T 4381 LDS 10/25% Glass/Mineral Filled PA6/6T (Conditioned) Description: Ultramid® T 4381 LDS is a semi-crystalline, partially aromatic high temperature polyamide (PA6/6T) for laser direct structuring (LPKFLDS®). As the material is reinforced with 10% fibe.. |
|||
Density | 1.52 g/cc @Temperature 23.0 °C |
0.0549 lb/in³ @Temperature 73.4 °F |
ASTM D792 |
Beijing Ranger Chem PBT-201-G15 Flame Retarding FR PBT Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin.. |
|||
Density | 1.52 g/cc | 0.0549 lb/in³ | ISO 1183 |
DSM Arnite® TV4 261 /A PBT-GF30 30% Glass Reinforced |
|||
Density | 1.52 g/cc | 0.0549 lb/in³ | ASTM D792 |
Chang Chun Plastic Longlite PM T375J Heat Resistant Phenolic Molding Compound ASTM Grade per ASTM D700 is 13.Information provided by Dowell Trading Company Ltd. |
|||
Density | 1.52 - 1.72 g/cc | 0.0549 - 0.0621 lb/in³ | Molded |
Bulk Molding Compounds BMC T60-6009 Compression Grade Wear Resistant Molding Compound BMC T60-6009 is a compression grade wear resistant molding compound. This material was specifically formulated for applications that require excellent abrasion resistance. Due to its low specific .. |