Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.51 g/cc | 0.0546 lb/in³ | ISO 1183 |
Polykemi AB SCANMID 6 B11^ F45 Nylon 6, Glass Fiber Reinforced Information provided by Polykemi AB |
|||
Density | 1.51 - 1.55 g/cc | 0.0546 - 0.0560 lb/in³ | ISO R 1184 |
Fainplast Compounds RK 325/AM Rigid PVC, Extrusion Lead Free Profiles anti mould |
|||
Density | 1.51 g/cc | 0.0546 lb/in³ | ASTM D792 |
Manifattura Cattaneo VESPEL® SP21 Polyimide Manifattura Cattaneo products are available in semi-finished forms such as bars, profiles, sheets and plates.Information provided by Manifattura Cattaneo s.p.a. |
|||
Density | 1.51 g/cc | 0.0546 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP LUBRICOMP KFP032 Acetal Copolymer LNP LUBRICOMP* KFP032 is a compound based on Acetal Copolymer resin containing 10% Glass Fiber, 15% PTFE/Silicone. Added feature of this material is: Wear Resistant. |
|||
Density | 1.51 g/cc | 0.0546 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP LUBRICOMP KFP032 Acetal Copolymer (Asia Pacific) LNP* LUBRICOMP* KFP032 is a compound based on Acetal Copolymer resin containing PTFE, Silicone, Glass Fiber. Added features of this material include: Internally Lubricated. |
|||
Density | 1.51 g/cc | 0.0546 lb/in³ | ISO 1183 |
SABIC Innovative Plastics ULTEM 2300F PEI (Europe-Africa-Middle East) 30% Glass fiber filled, standard flow Polyetherimide (Tg 217C). Resin is RoHS compliant. US FDA and European Food Contact compliant. Effective June, 2007 this grade will no longer be supported with .. |
|||
Density | 1.51 g/cc | 0.0546 lb/in³ | ISO 1183 |
SABIC Innovative Plastics ULTEM 2310R PEI (Europe-Africa-Middle East) 30% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C) with internal mold release. Resin is RoHS compliant. UL94 V0 and 5VA listing. |
|||
Density | 1.51 g/cc | 0.0546 lb/in³ | ISO 1183 |
SABIC Innovative Plastics ULTEM HU2310 PEI 30% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP.. |
|||
Density | 1.51 g/cc | 0.0546 lb/in³ | ASTM D792 |
Techmer ES HiFill FR® PA6/6 GF25 FR BK 25% Glass Filled (Dry) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 25% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Flame Retardant, Heat Stabilized and LubricatedAppear.. |
|||
Density | 1.51 g/cc | 0.0546 lb/in³ | ASTM D792 |
Techmer ES HiFill FR® PA6/6 GF25 FR NAT003 25% Glass Filled (Conditioned) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 25% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Flame Retardant, Heat Stabilized and LubricatedUL Fil.. |
|||
Density | 1.51 g/cc | 0.0546 lb/in³ | ASTM D792 |
Techmer ES HiFill® PA6/6 CM40 40% Mineral Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Mineral Filler, 40% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Heat Stabilized and LubricatedAppearance: Natural .. |
|||
Density | 1.51 g/cc | 0.0546 lb/in³ | GB/T 1033.1-2008 |
Sichuan Deyang Haton® hCF41 Polyphenylene Sulfide Injection molding, high strengthInformation provided by Sichuan Deyang Chemical Co., LTD |
|||
Density | 1.51 g/cc | 0.0546 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP JF004 PES LNP THERMOCOMP* JF004 is a compound based on Polyethersulfone resin containing 20% Glass Fiber. |
|||
Density | 1.51 g/cc | 0.0546 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP THERMOCOMP JF004 PES (Europe-Africa-Middle East) LNP* Thermocomp* JF004 is a compound based on Polyethersulfone resin containing Glass Fiber. |
|||
Density | 1.51 g/cc | 0.0546 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP THERMOCOMP JF004EXP PES LNP* THERMOCOMP* JF004EXP is a compound based on Polyethersulfone resin containing 20% Glass Fiber. Added features of this material include: Easy Molding. |
|||
Density | 1.51 g/cc | 0.0546 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP THERMOCOMP JF004Z PES (Europe-Africa-Middle East) LNP* Thermocomp* JF004Z is a compound based on Polyethersulfone resin containing Glass Fiber. Added features of this material include: HV. |
|||
Density | 1.51 g/cc | 0.0546 lb/in³ | ASTM D792 |
Techmer ES HiFill FR® PA6/6 GF25 FR NAT003 25% Glass Filled (Dry) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 25% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Flame Retardant, Heat Stabilized and LubricatedUL Fil.. |
|||
Density | 1.51 g/cc | 0.0546 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP THERMOTUF DF008EI PC (Asia Pacific) LNP* Thermotuf* DF008EI is a compound based on Polycarbonate resin containing Glass Fiber. Added features of this material include: Easy Molding, Mold Release, High Impact. |
|||
Density | 1.51 g/cc | 0.0546 lb/in³ | DAM; ISO 1183 |
DSM Stanyl® TW241F8 Nylon 46-40% Glass Reinforced, Heat Stabilized, Lubricated (Asian Grade) (Cond) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Density | 1.51 g/cc @Temperature 23.0 °C |
0.0546 lb/in³ @Temperature 73.4 °F |
DIN 53 479 |
Ensinger TECASINT™ 2061 Polyimide, 15% Graphite, 10% PTFE Filled (PI) TECASINT™ 2000 series of polyimide stock shapes provide a superior combination of high temperature and bearing and wear, properties that make it an ideal choice for the most demanding applications... |
|||
Density | 1.51 g/cc | 0.0546 lb/in³ | ASTM D792 |
Ensinger Tecatron® XP-71 Compression Molded PPS Compound, 20% PTFE Filled Natural Ensinger Special Polymers has over twenty different grades of TECATRON PPS available. Custom formulations can be blended to suit specific applications. Compression molding is amenable to short run p.. |
|||
Density | 1.51 g/cc | 0.0546 lb/in³ | ASTM D792 |
Ensinger Tecatron® XP-86 Compression Molded PPS Compound, with 40% Carbon Fiber Ensinger Special Polymers has over twenty different grades of TECATRON PPS available. Custom formulations can be blended to suit specific applications. Compression molding is amenable to short run p.. |
|||
Density | 1.51 g/cc | 0.0546 lb/in³ | DAM; ISO 1183 |
DuPont Performance Polymers Minlon® 10B40HS1 BK061 Nylon 66
(Unverified Data**) 40% Mineral Reinforced Heat Stabilized Polyamide 66 Minlon 10B40HS1 BK061 is a 40% mineral reinforced heat stabilized black polyamide 66 resin for injection molding.Information provided by DuPont Pe.. |
|||
Density | 1.51 - 1.55 g/cc | 0.0546 - 0.0560 lb/in³ | ISO R 1184 |
Fainplast Compounds HGKA 0183 Flexible PVC, Sheathing for High Temperatures Lead Free Sheathing high LOI |
|||
Density | 1.51 g/cc | 0.0546 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP VERTON RX00078 PA 66 (Europe-Africa-Middle East) LNP* VERTON* RX00078 is a compound based on PA 66 resin containing Long Glass Fiber, Proprietary Lubricant. Added features include: Internally Lubricated. |
|||
Density | 1.51 g/cc | 0.0546 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP VERTON RX970079 PA 66 (Europe-Africa-Middle East) LNP* VERTON* RX970079 is a compound based on PA 66 resin containing Long Glass Fiber and PTFE. Added features include; Internally Lubricated. |
|||
Density | 1.51 g/cc | 0.0546 lb/in³ | DAM; ISO 1183 |
DuPont Performance Polymers Zytel® 73G45L NC010 Nylon 6
(Unverified Data**) 45% Glass Reinforced Polyamide 6Zytel 73G45L NC010 is a 45% glass fiber reinforced polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Density | 1.51 g/cc | 0.0546 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP JF004E PES LNP* THERMOCOMP* JF004E is a compound based on Polyethersulfone resin containing 20% Glass Fiber. Added features of this material include: Easy Molding. |
|||
Density | 1.51 g/cc | 0.0546 lb/in³ | Crystaline; ISO 1183 |
Victrex® PEEK 650GL30 30% Glass Fiber Filled, PolyEtherEtherKetone High performance thermoplastic material, 30% glass fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding and extrusion, low flow, color natural/beige.Typical.. |