Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.46 g/cc | 0.0527 lb/in³ | ASTM D 792 |
SABIC Innovative Plastics LNP Faradex ES003DE PEI LNP* Faradex* ES003DE is a Polyetherimide resin containing stainless steel fibers. Characteristics of this grade are EMI/RFI Shielding.This data was supplied by SABIC-IP for the Americas region. |
|||
Density | 1.46 g/cc | 0.0527 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP FARADEX ES003E PEI LNP* FARADEX* ES003E is a Polyetherimide resin containing 15% Stainless Steel Fibers. Added feature of this grade is: EMI/RFI Shielding. |
|||
Density | 1.46 g/cc | 0.0527 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP FARADEX NX07344 PC+ABS (Asia Pacific) Faradex NX07344 is a compound based on PC+ABS blend resin containing non-brominated and non-chlorinated flame retardant system, Stainless Steel and glass fiber. Added features of this material incl.. |
|||
Density | 1.46 g/cc | 0.0527 lb/in³ | DAM; ISO 1183 |
DuPont Performance Polymers Zytel® HTN 52G35HSL BK083 Polyphthalamide (PPA)
(Unverified Data**) Zytel® HTN52G35HSL BK083 is a 35% glass reinforced, heat stabilized, lubricated high performance polyamide resin that can be molded in water heated molds. It is also a PPA resin.Information provid.. |
|||
Density | 1.46 g/cc | 0.0527 lb/in³ | ISO 1183 |
Polykemi AB SCANMID 6 B12^ QF2515 Nylon 6, Glass Fiber and Mineral Reinforced Information provided by Polykemi AB |
|||
Density | 1.46 - 1.49 g/cc | 0.0527 - 0.0538 lb/in³ | ASTM D792 |
KYDEX® 6565 Acrylic/PVC Thermoplastic Sheet Low heat release aviation gradeApplications: Airducts, seat parts, bulkhead laminates, escape slide packboards, gallery parts, instrument panels, laboratory floorplans, sidewall panels, life vest sh.. |
|||
Density | 1.46 g/cc | 0.0527 lb/in³ | |
LATI Latilub 73/13-10T Y/15 POM, 15% Aramid Fiber Reinforced, PTFE Filled Self-lubricating product based on Polyoxymethylene (POM). PTFE. Aramid fibersAvailability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Indust.. |
|||
Density | 1.46 g/cc | 0.0527 lb/in³ | ISO 1183/A |
Solvay TECHNYL® A 218 V40 Black 21 NHFE PA66, 40% glass fiber, Conditioned Description: Polyamide 66, offering high flowability and productivity gains, reinforced with 40% of glass fiber, heat stabilized, for injection molding.Available in: EuropeProduct Applications: TECH.. |
|||
Density | 1.46 g/cc | 0.0527 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP LUBRICOMP KG002 Acetal Copolymer (Europe-Africa-Middle East) LNP* LUBRICOMP* KG002 is a compound based on Acetal Copolymer containing Graphite. Added features include : Internally Lubricated. |
|||
Density | 1.46 g/cc | 0.0527 lb/in³ | ISO 1183 |
Solvay Specialty Polymers Amodel® HFZ A-4133L Polyphthalamide (PPA), 33% Glass Fiber Amodel® HFZ A-4133 L polyphthalamide (PPA) is a 33% glass-reinforced, hot water moldable resin. Key properties include heat resistance, reduced outgassing and high strength and stiffness over a b.. |
|||
Density | 1.46 g/cc | 0.0527 lb/in³ | ASTM D792 |
Solvay Specialty Polymers AvaSpire® AV-722 SL30 Polyaryletherketone (PAEK) AV-722 SL30 is a wear resistant grade of AvaSpire® polyaryletherketone (PAEK) designed to provide low wear rates in both non-lubricated and lubricated environments. In addition to the outstanding.. |
|||
Density | 1.46 g/cc @Temperature 25.0 °C |
0.0527 lb/in³ @Temperature 77.0 °F |
Liquid |
Solvay Specialty Polymers Meforex® 123 Ozone-Friendly CFC Replacement Formula: CHCl2CF3; Name: 1,1 Dichloro 2,2,2 Trifluoroethane. Replaces CFC 11. Industrial air-conditioning, heat pumps, and heat transfer fluid.Information provided by Solvay Solexis, Inc. |
|||
Density | 1.46 g/cc | 0.0527 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP STAT-KON KEP33 Acetal LNP STAT-KON* KEP33 is a compound based on Acetal resin containing 15% Carbon Fiber, 15% PTFE/Silicone. Added features of this material include: Electrically Conductive, Wear Resistant. |
|||
Density | 1.46 g/cc | 0.0527 lb/in³ | ASTM D792 |
Techmer ES HiFill® PES GF30 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Density | 1.46 g/cc | 0.0527 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Valox® SHF4910 PBT (Europe-Africa-Middle East) 6.5% glass reinforced, Super High Flow, flame retardant PBT. |
|||
Density | 1.46 g/cc | 0.0527 lb/in³ | ISO 1183 |
Wellman Wellamid® MRGF25/15 22H-N 25% Mineral/15% Glass Fiber Reinforced Nylon 66, Heat Stabilized Typical Applications: Lawn and garden equipment, automotive trim, bezels, wheel covers, window frames, gas tank filler housings, brackets, metalized lighting reflectors for automotive, automotive co.. |
|||
Density | 1.46 g/cc | 0.0527 lb/in³ | ASTM D792 |
Westlake Plastics Pomalux® CN-F Acetal Copolymer (conductive) Non-sloughing carbon-fiber-filled material which is extremely strong and stiff with excellent dimensional stability. Abrasion-resistant, highly chemical-resistant, with temperature resistance to 32.. |
|||
Density | 1.46 g/cc | 0.0527 lb/in³ | ISO 1183 |
EMS-Grivory Grivory® BG-40 S PA6-GF40 Product description: Grilon BG-40 S is a normal viscosity PA 6 injection molding type with 40% glass fibers. Grilon BG-40 S has the following important properties: High stiffnessExcellent surface fi.. |
|||
Density | 1.46 g/cc | 0.0527 lb/in³ | |
DuPont™ Kapton® 50EN Polyimide Film, 13 Micron Thickness Film thickness 13 micron (0.5 mil)Kapton® Type E and EN films have superior dimensional stability, low CHE, a CTE close to copper, and a high modulus. This type is exceptional for applications req.. |
|||
Density | 1.46 g/cc | 0.0527 lb/in³ | ISO 1183 |
EMS-Grivory Grivory® TSM-40/4 PA666-MD40 Product description: Grilon TSM-40/4 is a special heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 40% mineral filler. Grilon TSM-40/4 has the following important properties.. |
|||
Density | 1.46 g/cc | 0.0527 lb/in³ | |
DuPont Performance Polymers Crastin® SK695FR NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**)&l 30% Glass Reinforced Flame Retardant Polybutylene Terephthalate Crastin® SK695FR is a 30% glass reinforced flame retardant polybutylene terephthalate for injection moulding.Information provided b.. |
|||
Density | 1.46 g/cc | 0.0527 lb/in³ | JIS-Z-8807 |
Denka VINYKON M1071 PVC, M grade for hard injection molding A PVC resin compound offering excellent physical properties and workability. A broad product lineup is available, including hard and soft grades, as well as those for extrusion and injection molding.. |
|||
Density | 1.46 g/cc | 0.0527 lb/in³ | DAM; ISO 1183 |
DuPont Performance Polymers Zytel® HTN 51G35HSLR BK420J Polyphthalamide (PPA)
(Unverified Data**) 35% Glass Reinforced PPA High Performance Polyamide with Improved Surface Appearance Zytel HTN51G35HSLR BK420J is a 35% glass reinforced heat stabilized lubricated high performance polyamide resin w.. |
|||
Density | 1.46 g/cc | 0.0527 lb/in³ | ASTM D792 |
Techmer ES Luriblend® POM CO GF5 TL5 5% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 5% Filler by WeightAdditive: PTFE Lubricant(5%)Features: Lubricated and CopolymerInformation provided by TP Composites, In.. |
|||
Density | 1.46 g/cc | 0.0527 lb/in³ | DIN 53479 |
Polyram PM3013G2 Acetal, 10% Glass Fiber
(discontinued **) 10% Glass fiber reinforced polyacetal for injection molding applications.Information provided by Polyram Ram On Ind. |
|||
Density | 1.46 - 1.76 g/cc | 0.0527 - 0.0636 lb/in³ | Average value: 1.62 g/cc Grade Count:23 |
Overview of materials for Polybutylene Terephthalate (PBT), Glass Fiber + PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Fiber + PTFE Filled". Each property range of values reported is .. |
|||
Density | 1.46 g/cc | 0.0527 lb/in³ | DAM; ISO 1183 |
DuPont Performance Polymers Zytel® HTN 52G35HSL BK083 Polyphthalamide (PPA)
(Unverified Data**) 35% Glass Reinforced PPA High Performance Polyamide Zytel HTN52G35HSL BK083 is a 35% glass reinforced heat stabilized lubricated high performance polyamide resin that can be molded in water heated m.. |
|||
Density | 1.46 g/cc | 0.0527 lb/in³ | DAM; ISO 1183 |
Solvay Specialty Polymers Ixef® 1313/0004 Polyarylamide, 40% Glass Fiber + Elastomer, at Equilibrium (65% RH)
  Impact modified. The IXEF compounds are a family of semi-crystalline polyarylamide thermoplastics reinforced with glass fibers and/or mineral fillers for injection molding.Data provided by the manu.. |