Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

KYDEX® 6565 Acrylic/PVC Thermoplastic Sheet

Category Polymer , Thermoplastic , Acrylic (PMMA) , Vinyl (PVC) , PVC/Acrylic Alloy
Manufacturer KYDEX LLC
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF KYDEX® 6565 Acrylic/PVC Thermoplastic Sheet.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Low heat release aviation gradeApplications: Airducts, seat parts, bulkhead laminates, escape slide packboards, gallery parts, instrument panels, laboratory floorplans, sidewall panels, life vest shrouds, window revealFeatures: Meets all fire retardancy requirements set forth by the FAR. An ideal material to form two and three dimensional aircraft components. It is very resistant to a wide range of concentrate chemicals, and is therefore easy to clean with aggressive cleaners. Passes Motor Vehicle Safety Standards (MVSS 302). Radiant Panel: Pass as per ASTM E162Fabrication: Kydex 6565 forms to deep draws with low forces when heated to the upper end of the proper forming temperature range. Crisp detail is achieved and rejects are minimized. Kydex 6565 sheet can be formed on all standard presses, and cut on all standard die-cutting machines.Data provided by the Kleerdex Company.
Physical Properties Metric English Comments
Density 1.46 - 1.49 g/cc
0.0527 - 0.0538 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Rockwell R 98
98
ASTM D785
Tensile Strength, Ultimate 45.0 MPa
6530 psi
ASTM D638
Elongation at Break 55 %
55 %
Modulus of Elasticity 2.896 GPa
420.0 ksi
Flexural Yield Strength 70.0 MPa
10200 psi
ASTM D790
Impact Test 7.24 J
5.34 ft-lb
Dynatup Max Energy
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 78.0 °C
172 °F
annealed; ASTM D648
Processing Properties Metric English Comments
Processing Temperature 163 - 200 °C
325 - 392 °F
Forming Temperature