Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.19 g/cc | 0.0430 lb/in³ | ASTM D-792 |
Plaskolite Optix® CA - 51 HF General Purpose Acrylic Resin OPTIX® general purpose acrylics are available in a variety of performance grades that offer varying melt flow rates, heat resistance, color/opacity and gloss levels.Information provided by Plaskoli.. |
|||
Density | 1.19 g/cc | 0.0430 lb/in³ | ASTM D792 |
Plaskolite Optix® CA-82 General Purpose Acrylic Resin Injection Molding Grade Pellets. Highest Molecular Weight, good heat resistance. Superior mold release. |
|||
Density | 1.19 g/cc | 0.0430 lb/in³ | ASTM D792 |
Plaskolite West Optix® CA-80 General Purpose Acrylic Resin Extrusion Grade Pellets. Unlubricated version of CA-81. Highest Molecular weight. |
|||
Density | 1.19 g/cc | 0.0430 lb/in³ | STN 64 0111 |
Plastcom SLOVAMID 6 FRB 4 LS Polyamide 6, Halogen Free Flame Retardant, Light Stabilization FeaturesPA 6 for injection moulding with increased flammability resistance with non-halogen flame retardant. Determined for electrical purposes. Excellent flow of the material predetermines it for.. |
|||
Density | 1.19 g/cc | 0.0430 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Cycolac® FR15U ABS Flame retardant ABS with excellent indoor UV properties and excellent processing. UL94 V-0/5VA rated. Elevated UL RTI rating (90-85-90) for all colors except for blue and green colors (60-60-60). |
|||
Density | 1.19 g/cc | 0.0430 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Cycolac® FR15U ABS (Asia Pacific) Flame retardant ABS. Excellent indoor UV properties. Excellent moldability. UL94 V-0/5VA rated.ing. |
|||
Density | 1.19 g/cc | 0.0430 lb/in³ | ASTM D792 |
SABIC Innovative Plastics Lexan® 221R PC 17.5 MFR, for small, intricate parts. Improved flame retardance. Internal mold release. |
|||
Density | 1.19 g/cc | 0.0430 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Lexan® 943X PC Copolymer (Asia Pacific) Lexan* 943X is a UV stabilized medium flow impact modified injection molding (IM) grade. This resin offers UL94 V0 @ 1.5mm flame retardancy based on non-bromine, non-chlorine FR systems, low tempera.. |
|||
Density | 1.19 g/cc | 0.0430 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Lexan® EXL1413T PC Copolymer (Asia Pacific) Lexan* EXL1413T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers excellent low temperature (-30 °C) ductility in combination with medium f.. |
|||
Density | 1.19 g/cc | 0.0430 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Lexan® HPX4REU PC Copolymer (Europe-Africa-Middle East) Medium flow specialty polycarbonate - improved processability & autoclavability. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP.. |
|||
Density | 1.19 g/cc | 0.0430 lb/in³ | ASTM D 792 |
SABIC Innovative Plastics Lexan® ML7678 PC 17.5 MFR, for small, intricate parts. FDA food contact compliant in limited colors. Enhanced mold release package.This data was supplied by SABIC-IP for the Americas region. |
|||
Density | 1.19 g/cc | 0.0430 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Lexan® ML7689 PC Copolymer (Europe-Africa-Middle East) Lexan* ML7689 polycarbonate (PC) siloxane copolymer resin IS a high viscosity injection molding (IM) grade WITH good processability, offering opportunities FOR shorter IM CYCLE times compared TO sta.. |
|||
Density | 1.19 g/cc | 0.0430 lb/in³ | ASTM D-792 |
Plaskolite West Optix® CP - 51 General Purpose Acrylic Resin Generally unaffected by alkalis, hydrocarbons, non-oxidizing acids, and salt water. Transparent, translucent, opaque, and custom colors in various grades of melt flow rate and heat resistance are av.. |
|||
Density | 1.19 g/cc | 0.0430 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Lexan® EXL9132 PC Copolymer (Asia Pacific) Opaque PC-Siloxane copolymer with excellent processability. Improved flow, low temperature ductility, UV stabilized. Non-chlorinated, non-brominated flame retardant product. UL rated V0/5VA. |
|||
Density | 1.19 g/cc | 0.0430 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Lexan® FXD1413T PC Copolymer Clear PC-siloxane copolymer with excellent processability, in special light diffusion colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may af.. |
|||
Density | 1.19 g/cc | 0.0430 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Lexan® FXE1414T PC Copolymer (Europe-Africa-Middle East) Clear PC-siloxane copolymer with excellent processability, for Visual fX capability in "Energy" colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color packa.. |
|||
Density | 1.19 g/cc | 0.0430 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Lexan® HP2NR PC (Asia Pacific) Med/high flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains no.. |
|||
Density | 1.19 g/cc | 0.0430 lb/in³ | ASTM D792 |
Eastman Tenite Butyrate 465E2R30012 Natural, Trsp Cellulose Acetate Butyrate
(discontinued **) Plasticizer 12%. Weight loss on heating = 1.3% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
Density | 1.19 g/cc | 0.0430 lb/in³ | ISO 1183 |
Lucite International Perspexâ„¢ XT Acrylic Extruded Sheet 0X00 PERSPEX extruded sheet has a lower molecular weight making it easy to vacuum form and the extrusion process gives excellent thickness tolerance and is economical for long production runs.Information.. |
|||
Density | 1.19 g/cc | 0.0430 lb/in³ | |
Taiwan Sheen Soon Sheenthane® A9315E Thermoplastic Polyurethane Elastomer Thermoplastic polyurethane elastomer for extrusionInformation provided by Taiwan Sheen Soon Co., LTD. |
|||
Density | 1.19 g/cc | 0.0430 lb/in³ | |
Loctite® 5205 Flexible Cure Flange Sealant Anaerobic GasketingLoctite® 5205 Flexible Cure Flange SealantFast curing and flexible, good sealing properties against oil and water/glycol particularly at high temperatures. High viscosity. Recom.. |
|||
Density | 1.19 g/cc | 0.0430 lb/in³ | ASTM D792 |
Eastman Tenite Butyrate 580A3720016 Clear, Trsp Cellulose Acetate Butyrate Plasticizer 10%. Weight loss on heating = 0.5% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
Density | 1.19 g/cc | 0.0430 lb/in³ | |
CRP Technology Windform® GT Polyamide Glass Composite Processed by selective laser sintering (SLS). Windform® GT is a deep and dark black composite material based on polyamide fiber glass. After hand finishing, the color becomes shining and brighter... |
|||
Density | 1.19 g/cc | 0.0430 lb/in³ | |
Abatron AboCast/AboCure 8109-11 All-purpose, structural dielectric resin. Better thermal and chemical properties than 8109-8, but requires heat cure. Melts at 70-80°C and remains liquid (supercooled) for many hours at RT.Process.. |
|||
Density | 1.19 g/cc | 0.0430 lb/in³ | ASTM D792 |
Ashley Polymers Ashlene® 527-13G Nylon 66, 13% Glass Reinforced A 13% glass reinforced, impact modified Nylon 66.Data provided by the manufacturer |
|||
Density | 1.19 - 1.23 g/cc | 0.0430 - 0.0444 lb/in³ | ISO 1183 |
Austin Novel Materials Texalan® 290A Polyester-based TPU Description: Good abrasion resistance, tensile strength, oil resistance and transparency which can meet different demands in various industryInformation from Dawnentech |
|||
Density | 1.19 g/cc | 0.0430 lb/in³ | ASTM D792 |
Ashley Polymers Ashlene® 742L-13G Nylon 6/66, 13% Glass Reinforced 6/66 Copolymer with high surface gloss in addition to high stiffness and strength, 13% Glass Reinforced.Data provided by the manufacturer |
|||
Density | 1.19 g/cc | 0.0430 lb/in³ | ASTM D-792 |
Plaskolite West Optix® CP - 82 General Purpose Acrylic Resin Generally unaffected by alkalis, hydrocarbons, non-oxidizing acids, and salt water. Transparent, translucent, opaque, and custom colors in various grades of melt flow rate and heat resistance are av.. |
|||
Density | 1.19 - 1.23 g/cc | 0.0430 - 0.0444 lb/in³ | ISO 1183 |
Austin Novel Materials Texalan® 798A PCL TPU Description: Good abrasion resistance, tensile strength, oil resistance and heat resistance which can be used in mechanic parts and various industry parts.Information from Dawnentech |
|||
Density | 1.19 g/cc | 0.0430 lb/in³ | ISO 2781 |
Lubrizol Advanced Materials Pearlstick® 45-40/19 Polycaprolactone based TPU Pearlstick 45-40/19 is an elastic, linear, aromatic polyurethane, supplied in form of white spherical granules with a very high crystallization rate and a medium thermoplasticity level.Solubility: P.. |