Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Density = 0.0444 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most.
Physical Properties Metric English Comments
Density 1.17 - 1.23 g/cc
0.0423 - 0.0444 lb/in³
ASTM D792
Multibase Multi-Flex® TPE A 6221 M BLK
The burn rate is 1 in/min (25 mm/min) based on ASTM FM VSS 302. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase.
Density 1.19 - 1.23 g/cc
0.0430 - 0.0444 lb/in³
ASTM D792
Novatec Novaloy® 9000 PVC + ABS
Novaloy® 9000 is a specialty engineering alloy of ABS/PVC designed for injection molding, profile and sheet extrusion. Novaloy® 9000 has been formulated to provide excellent processing characte..
Density 1.19 - 1.23 g/cc
0.0430 - 0.0444 lb/in³
Average value: 1.21 g/cc Grade Count:19
Overview of materials for PCTG Copolyester
This property data is a summary of similar materials in the MatWeb database for the category "PCTG Copolyester". Each property range of values reported is minimum and maximum values of appropriate M..
Density 1.19 - 1.23 g/cc
0.0430 - 0.0444 lb/in³
ISO R 1183
Fainplast Compounds FAINGUM 6510 Flexible PVC, Injection Molding for Footwear
Soles with rubber
Density 1.19 - 1.23 g/cc
0.0430 - 0.0444 lb/in³
ISO R 1183
Fainplast Compounds GS 64/70 Flexible PVC, Injection Molding for Footwear
Soles for cold climates
Density 1.19 - 1.23 g/cc
0.0430 - 0.0444 lb/in³
ISO R 1183
Fainplast Compounds GS 66/F Flexible PVC, Injection Molding for Footwear
Fluorescent sandals
Density 1.19 - 1.23 g/cc
0.0430 - 0.0444 lb/in³
ISO R 1183
Fainplast Compounds GS 69/T Flexible PVC, Injection Molding for Footwear
Crystal sandals
Density 1.19 - 1.23 g/cc
0.0430 - 0.0444 lb/in³
ISO R 1183
Fainplast Compounds GS 70 Flexible PVC, Injection Molding for Footwear
Soles and heels
Density 1.19 - 1.23 g/cc
0.0430 - 0.0444 lb/in³
ISO R 1183
Fainplast Compounds GS 70/AT Flexible PVC, Injection Molding for Transparent Technical Items
Toys
Density 1.19 - 1.23 g/cc
0.0430 - 0.0444 lb/in³
ISO R 1183
Fainplast Compounds GS 70/BT Flexible PVC, Injection Molding for Footwear
Soles for cold climates
Density 1.19 - 1.23 g/cc
0.0430 - 0.0444 lb/in³
ISO R 1183
Fainplast Compounds PMS 60 Flexible PVC, Lead Free
Gaskets for frames
Density 1.19 - 1.23 g/cc
0.0430 - 0.0444 lb/in³
ISO R 1183
Fainplast Compounds GS 7005/BT Flexible PVC, Injection Molding for Footwear
Soles for cold climates
Density 1.19 - 1.23 g/cc
0.0430 - 0.0444 lb/in³
ISO R 1183
Fainplast Compounds GS 74/BT Flexible PVC, Injection Molding for Footwear
Soles for cold climates
Density 1.19 - 1.23 g/cc
0.0430 - 0.0444 lb/in³
ISO R 1184
Fainplast Compounds MPH 78/OP Medical Flexible PVC, Extrusion
Tubolar apparatus anti bend
Density 1.19 - 1.23 g/cc
0.0430 - 0.0444 lb/in³
ISO R 1183
Fainplast Compounds PG 7030 Flexible PVC, Extrusion Modified with Rubber
Diesel Oil resistent profiles
Density 1.19 - 1.23 g/cc
0.0430 - 0.0444 lb/in³
ISO 1183
Austin Novel Materials Texalan® 290A Polyester-based TPU
Description: Good abrasion resistance, tensile strength, oil resistance and transparency which can meet different demands in various industryInformation from Dawnentech
Density 1.19 - 1.23 g/cc
0.0430 - 0.0444 lb/in³
ISO 1183
Austin Novel Materials Texalan® 390A Polyester-based TPU
Description: Good abrasion resistance, tensile strength, oil resistance which can be used in injection, extrusion purpose.Information from Dawnentech
Density 1.19 - 1.23 g/cc
0.0430 - 0.0444 lb/in³
ISO 1183
Austin Novel Materials Texalan® 490A Polyester-based TPU
Description: Can be considered as custom-made products which use different raw materials to meet customers special requirementsInformation from Dawnentech
Density 1.19 - 1.23 g/cc
0.0430 - 0.0444 lb/in³
ISO 1183
Austin Novel Materials Texalan® 495A Polyester-based TPU
Description: Can be considered as custom-made products which use different raw materials to meet customers special requirementsInformation from Dawnentech
Density 1.19 - 1.23 g/cc
0.0430 - 0.0444 lb/in³
ISO 1183
Austin Novel Materials Texalan® 690A Polyester and Polyether based TPU
Description: A kind of custom-made products which use different raw materials to meet customers special requirementsInformation from Dawnentech
Density 1.19 - 1.23 g/cc
0.0430 - 0.0444 lb/in³
ISO 1183
Austin Novel Materials Texalan® 395A Polyester-based TPU
Description: Good abrasion resistance, tensile strength, oil resistance which can be used in injection, extrusion purpose.Information from Dawnentech
Density 1.19 - 1.23 g/cc
0.0430 - 0.0444 lb/in³
ISO R 1184
Fainplast Compounds KLT 75/G Flexible PVC, Sheathing Transparent Cables Lead Free
Transparent sheathing
Density 1.19 - 1.23 g/cc
0.0430 - 0.0444 lb/in³
ISO R 1183
Fainplast Compounds PG 60/C Flexible PVC, Extrusion Modified with Rubber
Gaskets modified with rubber
Density 1.19 - 1.23 g/cc
0.0430 - 0.0444 lb/in³
ISO R 1183
Fainplast Compounds PH 68/A Flexible PVC, Transparent Extrusion
Profiles, UL Class V1
Density 1.19 - 1.23 g/cc
0.0430 - 0.0444 lb/in³
ISO 1183
Austin Novel Materials Texalan® 695A Polyester and Polyether based TPU
Description: A kind of custom-made products which use different raw materials to meet customers special requirementsInformation from Dawnentech
Density 1.19 - 1.23 g/cc
0.0430 - 0.0444 lb/in³
ISO 1183
Austin Novel Materials Texalan® 798A PCL TPU
Description: Good abrasion resistance, tensile strength, oil resistance and heat resistance which can be used in mechanic parts and various industry parts.Information from Dawnentech
Density 1.19 - 1.23 g/cc
0.0430 - 0.0444 lb/in³
ISO R 1183
Fainplast Compounds PMP 77 Flexible PVC, Extrusion Modified with PU
Various profiles
Density 1.04 - 1.23 g/cc
0.0376 - 0.0444 lb/in³
Average value: 1.17 g/cc Grade Count:9
Overview of materials for Polypropylene with Glass Fiber + Bead Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with Glass Fiber + Bead Filler". Each property range of values reported is minimum and max..
Density 1.19 - 1.23 g/cc
0.0430 - 0.0444 lb/in³
ISO R 1183
Fainplast Compounds PMP 338 Flexible PVC, Extrusion Modified with PU
Sheath PVC/PU for low temperatures
Density 0.872 - 1.23 g/cc
0.0315 - 0.0444 lb/in³
Average value: 1.02 g/cc Grade Count:19
Overview of materials for Polypropylene, Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Carbon Fiber 10%". Each property range of values reported is minimum and maximum values o..
Copyright © lookpolymers.com All Rights Reserved