Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.13 g/cc | 0.0410 lb/in³ | Yield Density |
Honeywell Capran® 512 LL Heat Stabilized Nylon Film
(discontinued **) Description: Capran® 512 LL is a heat-stabilized blown film produced from low lactam nylon-6 resin. It is recommended as bagging film for advanced composite fabrication and other high temperature .. |
|||
Density | 1.13 g/cc | 0.0410 lb/in³ | Yield Density |
Honeywell Capran® 518 LL Heat Stabilized Nylon Film
(discontinued **) Description: Capran® 518 LL is a green tinted, heat-stabilized blown film produced from low lactam nylon-6 resin. It is recommended as bagging film for advanced composite fabrication and other hig.. |
|||
Density | 1.13 g/cc | 0.0410 lb/in³ | Yield Density |
Honeywell Capran® 980 Heat Stabilized Nylon Film
(discontinued **) Description: Capran® 980 is a clear (low haze level), heat-stabilized cast film produced from modified nylon 6 resin. Capran® 980 has excellent heat stability and resistance to pinholing. It ca.. |
|||
Density | 1.13 g/cc | 0.0410 lb/in³ | Yield Density |
Honeywell Capran® 996 Heat Stabilized Nylon Film
(discontinued **) Description: Capran® 996 is a blue tinted, heat-stabilized cast film produced from modified nylon resin. Capran® 996 has excellent heat stability and resistance to pinholing. It can be used at t.. |
|||
Density | 1.13 g/cc | 0.0410 lb/in³ | Yield Density |
Honeywell Capran® Unidraw (0.75 mil) Nylon 6 Film
(discontinued **) Description: Capran® Unidraw is a 0.75 mil (19 micron) machine direction oriented nylon 6 film specifically designed for the continuous process lamination of glass fiber reinforced panel. High str.. |
|||
Density | 1.13 g/cc | 0.0410 lb/in³ | Yield Density |
Honeywell Capran® Unidraw (1.00 mil) Nylon 6 Film
(discontinued **) Description: Capran® Unidraw is a 1.00 mil (25 micron) machine direction oriented nylon 6 film specifically designed for the continuous process lamination of glass fiber reinforced panel. High str.. |
|||
Density | 1.13 g/cc | 0.0410 lb/in³ | Yield Density |
Honeywell Capran® Nylon Film, Multipurpose Nylon 6 Film Description: Capran® is a multipurpose nylon 6 film. Its physical properties are evenly distributed for optimum performance giving excellent resistance to flex cracking. It can be processed ove.. |
|||
Density | 1.13 g/cc | 0.0410 lb/in³ | Yield Density |
Honeywell Capran® Oxyshield™ M-OPA (0.60 mil) Monoaxially Oriented, Co-Extruded In-Line Nylon6/Nylon6/Nylon6 Film Description: Capran® Oxyshield™ M-OPA (Machine Direction Oriented Polyamide) is a clear, monoaxially oriented, co-extruded in-line nylon6/nylon6/nylon6 film with high mechanical strength and.. |
|||
Density | 1.13 g/cc | 0.0410 lb/in³ | Yield Density |
Honeywell Capran® Oxyshield™ M-OPA (0.75 mil) Monoaxially Oriented, Co-Extruded In-Line Nylon6/Nylon6/Nylon6 Film Description: Capran® Oxyshield™ M-OPA (Machine Direction Oriented Polyamide) is a clear, monoaxially oriented, co-extruded in-line nylon6/nylon6/nylon6 film with high mechanical strength and.. |
|||
Density | 1.13 g/cc | 0.0410 lb/in³ | Yield Density |
Honeywell Capran® Oxyshield™ M-OPA (1.0 mil) Monoaxially Oriented, Co-Extruded In-Line Nylon6/Nylon6/Nylon6 Film Description: Capran® Oxyshield™ M-OPA (Machine Direction Oriented Polyamide) is a clear, monoaxially oriented, co-extruded in-line nylon6/nylon6/nylon6 film with high mechanical strength and.. |
|||
Density | 1.13 g/cc | 0.0410 lb/in³ | Yield Density |
Honeywell Capran® Oxyshield™ OBS Monoaxially Oriented, Co-Extruded Nylon 6/EVOH/Nylon 6 Clear Film Description: Oxyshield™ Oriented Barrer is a 0.60 mil (15 micron) monoaxially oriented, co-extruded nylon 6/EVOH/nylon 6 clear film with slip additive having excellent gas barrier through a bro.. |
|||
Density | 1.13 g/cc | 0.0410 lb/in³ | Yield Density |
Honeywell Capran® Oxyshield™ OMBS (0.60 mil) Monoaxially Oriented, Co-Extruded Nylon6/EVOH/Nylon 6 Clear Film Description: Oxyshield™ Oriented Medium Barrier is a 0.60 mil (15 micron) monoaxially oriented, coextruded nylon 6/EVOH/nylon 6 clear film with slip additive having excellent gas barrier throug.. |
|||
Density | 1.13 g/cc | 0.0410 lb/in³ | Yield Density |
Honeywell Capran® Oxyshield™ OMBS (1.00 mil) Monoaxially Oriented, Co-Extruded Nylon 6-Based Clear Film Description: Oxyshield™ Oriented Medium Barrier is a 1.00 mil (25 micron) monoaxially oriented, coextruded nylon 6/EVOH/nylon 6 clear film with slip additive having excellent gas barrier throug.. |
|||
Density | 1.13 g/cc | 0.0410 lb/in³ | Yield Density |
Honeywell Capran® Oxyshield™ OXTR (Retortable Grade, 0.6 mil) Monoaxially Oriented Co-Extruded Nylon 6/EVOH/Nylon 6 Clear Film Description: Capran® Oxyshield™ Oriented Ultra Barrier Retortable Grade is a monoaxially oriented, co-extruded nylon 6-based clear film having excellent gas barrier through a broad range of .. |
|||
Density | 1.13 g/cc | 0.0410 lb/in³ | |
Wingate Alloys Winco Poly NLT Engineered UHMW Winco Poly NLT is one of the oldest and most widely used engineered mechanical plastics. Its combination of toughness, dimensional stability, wear resistance, availability and versatility make it a .. |
|||
Density | 1.14 - 1.67 g/cc | 0.0410 - 0.0603 lb/in³ | Average value: 1.36 g/cc Grade Count:665 |
Overview of materials for Nylon 6, 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% are included. E.. |