Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.11 g/cc | 0.0401 lb/in³ | |
Nylene® PA6/6 Impact Modified 411 HS Nylon 6/6 Medium Impact Grade; Property data for dry as molded samples.ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources Corporation. |
|||
Density | 1.11 g/cc | 0.0401 lb/in³ | ASTM D792-60T |
Rotuba 860M Ethyl Cellulose Data provided by the manufacturer. |
|||
Density | 1.11 g/cc | 0.0401 lb/in³ | ASTM D792-60T |
Rotuba 860MH 686.4 Ethyl Cellulose Data provided by the manufacturer. |
|||
Density | 1.11 - 1.65 g/cc | 0.0401 - 0.0596 lb/in³ | Average value: 1.21 g/cc Grade Count:22 |
Overview of materials for Nylon 12, 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, 20% Glass Fiber Filled". Specific grades with glass content between 15% and 24% are included. .. |
|||
Density | 1.11 g/cc | 0.0401 lb/in³ | |
LATI Latene® 22H2 MX/25 PP Homopolymer, Heat Stabilized Polypropylene homopolymer (PPh) based compound. Heat stabilized. Special mineral filler. Very good surface appearance.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North A.. |
|||
Density | 1.11 g/cc | 0.0401 lb/in³ | ISO 1183 |
LyondellBasell Hifaxâ„¢ CB272 Thermoplastic Polyolefin Elastomer Description: Hifaxâ„¢ CB272 high melt flow, 900 MPa flexural modulus, low CLTE, paintable, mineral-filled thermoplastic elastomeric olefin (TEO) resin has a very good balance of rigidity and dime.. |
|||
Density | 1.11 g/cc | 0.0401 lb/in³ | ISO 1183 |
SABIC Innovative Plastics NORYL V0150B PPE+HIPS (Asia Pacific) Noryl* V0150B is an unfilled, injection moldable modified polyphenylene ether resin.. Designed for high heat resistance and thin wall FR performance, this resin delivers a UL94 V0 rating at 1.5 mm a.. |
|||
Density | 1.11 g/cc | 0.0401 lb/in³ | ASTM D 792 |
Shakespeare Isocorâ„¢ CU145SI Nylon 6/66 Isocorâ„¢ CU145SI is a high viscosity, plasticized, PA-6/66 copolymer resin. This resin is specifically suited for applications requiring excellent abrasion resistance while maintaining a balan.. |
|||
Density | 1.11 g/cc | 0.0401 lb/in³ | ASTM D792 |
Techmer ES Electrablend® HIPS Availability: North AmericaForms: PelletsFeatures: ConductiveInformation provided by TP Composites, Inc. |
|||
Density | 1.11 g/cc | 0.0401 lb/in³ | ISO 1183 |
SABIC Innovative Plastics NORYL LS6010 PPE+HIPS (Asia Pacific) Noryl* LS6010 resin is a high performance modified PPE-PS blend that exhibits an excellent balance of nonhalogenated flame retardance, lower smoke production upon burning and low specifc gravity for.. |
|||
Density | 1.11 g/cc | 0.0401 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP STAT-KON 9X04323 PPE+PA66 (Asia Pacific) LNP* Stat-kon* 9X04323 is a compound based on Noryl GTX resin,Added features of this material include: Electrically Conductive. |
|||
Density | 1.11 g/cc | 0.0401 lb/in³ | ASTM D792 |
Techmer ES Luriblend® HIPS TL10 BK Availability: North AmericaForms: PelletsAdditive: PTFE Lubricant (10%)Features: Good Wear Resistance, Low Friction and LubricatedAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Density | 1.11 g/cc | 0.0401 lb/in³ | ISO 1183 |
DSM Arnitel® EM400 40 Shore D, Injection or Extrusion Grade Copolyester Elastomer (North America) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Density | 1.11 g/cc | 0.0401 lb/in³ | ISO 1183 |
CP-Polymer-Technik Wellamid® 6000/50 CP Nylon 6, Impact Modified Until 0°C, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Density | 1.11 g/cc | 0.0401 lb/in³ | ISO 1183 |
CP-Polymer-Technik Wellamid® 6600/42 HWCP Nylon 66, Polymer Modified, Heat Stabilized, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Density | 1.11 g/cc | 0.0401 lb/in³ | |
DuPont Performance Polymers Crastin® S620F20 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**)&l Unreinforced Medium Viscosity Polybutylene Terephthalate Crastin S620F20 NC010 is an unreinforced nucleated lubricated medium viscosity polybutylene terephthalate resin for fast injection molding.In.. |
|||
Density | 1.11 g/cc | 0.0401 lb/in³ | ISO 1183 |
Eurotec® Tecolen® HP30 KG30 NL HS 0B PPCP, 30% glass fiber/glass bead reinforced, heat stabilized, natural Information provided by Eurotec® |
|||
Density | 1.11 g/cc @Temperature 270 °C |
0.0401 lb/in³ @Temperature 518 °F |
Melt |
Covestro Makroblend® DP 2-7655 Polycarbonate + PET, Mineral Filled Impact Grade Developmental productISO 7792-1-PC/PET,MHPR,-030,MD10(PC+PET)-blendsimpact modifiedInjection molding grade 10% mineral filledPreprocessingMax. Water content |
|||
Density | 1.11 g/cc | 0.0401 lb/in³ | ISO 1183 |
Ascend Performance Materials Vydyne® 49 Nylon 66, Impact Modified, DAM Vydyne® 49 is general-purpose, impact-modified PA66 resin. Available in natural, is recognized for all the processing and property advantages inherent to PA66 with the addition of improved impact s.. |
|||
Density | 1.11 g/cc | 0.0401 lb/in³ | ASTM D792 |
Techmer ES Statiblend® PP TM10 BK Availability: North AmericaForms: PelletsFiller/Reinforcement: Talc Filler, 10% Filler by WeightFeatures: ConductiveUL File Number: E157318Appearance: BlackInformation provided by TP Composites, Inc.. |
|||
Density | 1.11 g/cc | 0.0401 lb/in³ | ISO 1183 |
SABIC Innovative Plastics NORYL RN0712 PPE+HIPS Noryl RN0712 is an unfilled Post Consumer recycle (PCR) based injection moldable modified polyphenylene ether resin comprising at least 37% PCR styrenic series resin content. Designed for good dimen.. |
|||
Density | 1.11 g/cc | 0.0401 lb/in³ | ISO 1183 |
Total Lacqrene® 851 High Impact Polystyrene
(discontinued **) LACQRENE® 851 is a flame retardant, high impact polystyrene, halogen free rated UL 94 V0 @ 2.5 mm and UL 94 5VA @ 2mm. LACQRENE® 851 offers rheological and mechanics properties which permits larg.. |
|||
Density | 1.11 g/cc | 0.0401 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP STAT-KON QD000I PA 6/10 (Asia Pacific) LNP STAT-KON* QD000I is a compound based on Nylon 6/10 resin containing Carbon Powder. Added features of this material include: Electrically Conductive. |