Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Rotuba 860M Ethyl Cellulose

Category Polymer , Renewable/Recycled Polymer , Thermoplastic , Cellulosic , Ethyl Cellulose, Molded
Manufacturer Rotuba
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Rotuba 860M Ethyl Cellulose.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Data provided by the manufacturer.
Physical Properties Metric English Comments
Density 1.11 g/cc
0.0401 lb/in³
ASTM D792-60T
Mechanical Properties Metric English Comments
Hardness, Rockwell R 106
106
ASTM D785
Tensile Strength, Ultimate 34.0 MPa
4930 psi
ASTM D638-61T
Elongation at Break 27 %
27 %
ASTM D638-61T
Izod Impact, Notched 1.28 J/cm
2.40 ft-lb/in
ASTM D256-56
0.270 J/cm

@Temperature -40.0 °C
0.506 ft-lb/in

@Temperature -40.0 °F
ASTM D256
Thermal Properties Metric English Comments
Melting Point 144 °C
291 °F
Flow temperature, ASTM D569-59
Deflection Temperature at 0.46 MPa (66 psi) 82.0 °C
180 °F
ASTM D648-56
Electrical Properties Metric English Comments
Dielectric Constant 3.18

@Frequency 10000 Hz
3.18

@Frequency 10000 Hz
ASTM D150-54T
3.23

@Frequency 1000 Hz
3.23

@Frequency 1000 Hz
ASTM D150-54T
Dissipation Factor 0.0072

@Frequency 1000 Hz
0.0072

@Frequency 1000 Hz
ASTM D150-54T
0.0127

@Frequency 10000 Hz
0.0127

@Frequency 10000 Hz
ASTM D150-54T