Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.03 g/cc | 0.0372 lb/in³ | ASTM D792 |
NYCOA 2084 HS PA 6 lubricated flexible tubing and conduitInformation provided by NYCOA, Inc. |
|||
Density | 1.03 g/cc | 0.0372 lb/in³ | ISO 1183 |
Polykemi AB POLYabs R00 ABS, High Impact Information provided by Polykemi AB |
|||
Density | 1.03 g/cc | 0.0372 lb/in³ | ISO 1183 |
Polykemi AB POLYabs R00 UV4 ABS, High Impact, UV Stabilized Information provided by Polykemi AB |
|||
Density | 1.03 g/cc | 0.0372 lb/in³ | ISO 1183 A |
Mytex Polymers AS319L-01US Thermoplastic Polyolefin, 19% Talc Filled AS319L-01US is a compounded thermoplastic polyolefin (TPO) designed for exterior automotive applications requiring cold temperature impact, processability and paintability. Available in natural or .. |
|||
Density | 1.03 g/cc | 0.0372 lb/in³ | ISO 2781 |
Termopol Termoton® V6GA3075A TPV Compound Termoton®V, TPV compounds with a dynamically cured EPDM phase closely dispersed in a polyolefin phase (PP). Main Characteristics: Wide range of hardness; High strength elasticity; 100% recyclable;.. |
|||
Density | 1.03 - 1.03 g/cc @Temperature 270 - 270 °C |
0.0372 - 0.0372 lb/in³ @Temperature 518 - 518 °F |
Average value: 1.03 g/cc Grade Count:1 |
Overview of materials for Polycarbonate/PET Polyester Blend This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/PET Polyester Blend". Each property range of values reported is minimum and maximum values.. |
|||
Density | 1.03 - 1.11 g/cc | 0.0372 - 0.0401 lb/in³ | Average value: 1.06 g/cc Grade Count:8 |
Overview of materials for Nylon 11, Cable Sheathing Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11, Cable Sheathing Grade". Each property range of values reported is minimum and maximum values o.. |
|||
Density | 1.03 - 1.14 g/cc | 0.0372 - 0.0412 lb/in³ | Average value: 1.10 g/cc Grade Count:10 |
Overview of materials for Nylon 12, PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, PTFE Filled". Each property range of values reported is minimum and maximum values of appropri.. |
|||
Density | 1.03 g/cc | 0.0372 lb/in³ | |
Iran Petrochemical (PCC) SH-0150 Acrylonitrile Butadiene Styrene SH - 0150 ABS extrusion grade has been formulated to provide excellent mechanical properties,extrusion stability, vacuum formability and chemical resistance. It is a high flow extrusion grade with h.. |
|||
Density | 1.03 g/cc | 0.0372 lb/in³ | |
Solvay LUBRHOPHOS® LB 400 E Surfactant Identification: ETHOXYLATED OELYL-CETYL ALCOHOL, PHOSPHATE ESTERSolubility: Dispersible in water. Soluble in most polar and aromatic solvents.Available in: Asia Pacific, Europe, Latin America and No.. |
|||
Density | <= 1.03 g/cc | <= 0.0372 lb/in³ | Relative density |
Suqian Unitechem Antioxidant 3114 Chemical Name: Tris(3,5-di-tert-butyl-4-hydroxybenzyl) isocyanurateCAS NO.: 27676-62-6Molecular Formula: C48H69N3O6Property: It is one kind of multi-functional Antioxidant, with multiple functional .. |
|||
Density | 1.03 - 1.11 g/cc | 0.0372 - 0.0401 lb/in³ | RP-0549 |
Solvay RHODATERGE® BCC Surfactant Description: Rhodaterge® BCC is Surfactant Base for Low Foaming, Highly Alkaline Cleaners (45% solids). Delivers exceptional surface tension reduction in high caustic systems; stable in 50% Sodiu.. |
|||
Density | 1.03 g/cc | 0.0372 lb/in³ | ASTM D792 |
UBE 7115U Nylon 6/12 Copolymer Description: UBESTA Nylon 12 CopolymerInformation provided by UBE. |
|||
Density | 1.03 g/cc | 0.0372 lb/in³ | ASTM-D792 |
Polyram Polytron P20B01 Homopolymer Polypropylene, Chemically Coupled 20% Long Fiber A CHEMICALLY COUPLED 20% LONG FIBER GLASS REINFORCED BLACK POLYPROPYLENE HEAT STABILIZED FOR INJECTION MOLDING APPLICATION.Information provided by Polyram Ram On Ind. |
|||
Density | 1.03 g/cc | 0.0372 lb/in³ | ASTM D792 |
Chevron Phillips EB6755 Rubber Modified Polystyrene DescriptionChevron EB6755 is an extrusion grade, high impact polystyrene developed for use in packaging applications. It is designed for exceptional environmental stress-crack resistance and practi.. |
|||
Density | 1.03 g/cc | 0.0372 lb/in³ | |
DuPont Performance Polymers Crastin® BM6450XD BK560 Polybutylene Terephthalate (PBT)
(Unverified Data**)& Unreinforced Polybutylene Terephthalate Developed for Blow MoldingCrastin BM6450XD BK560 is an unreinforced supertough polybutylene terephthalate resin with very high viscosity for extrusion and blo.. |
|||
Density | 1.03 g/cc | 0.0372 lb/in³ | |
DuPont Performance Polymers Zytel® 79G13L NC010 Nylon 66
(Unverified Data**) 13% Glass Reinforced Toughened Polyamide 66 Zytel 79G13L NC010 is a 13% glass fiber reinforced toughened polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Density | 1.03 g/cc | 0.0372 lb/in³ | |
Arkema Group Orgalloy® RS 60E10TL Nylon 6 Alloy, Rigid Grade (Conditioned) RS 60 series, rigid polyamide 6 alloy: easy to process, chemical resistance (no known solvents) and low moisture absorption leading to stability of mechanical, electrical and dimensional propertie.. |
|||
Density | 1.03 g/cc | 0.0372 lb/in³ | ASTM D792 |
Aclo Accucomp ABS ABS846HL High Flow Medium Impact Grade |
|||
Density | 1.03 - 1.05 g/cc | 0.0372 - 0.0379 lb/in³ | Typical; ISO 1183-1 |
Axion Polymers Axpoly® PS01 Impact Modified Polystyrene 100% post-consumer recycled polymer (recovered from refrigerators)93% less CO2 impact compared with virgin*Successfully replaces virgin grade resinISO9000 quality certifiedAvailable in a range of co.. |
|||
Density | 1.03 g/cc | 0.0372 lb/in³ | Typical; ISO 1183-1 |
Axion Polymers Axpoly® PS02 1010 Medium Impact Polystyrene PS02 Series polystyrenes offers the designer and processor a high performance polymer with well-defined properties in a range of options to suit many applications.The Axpoly® PS02 range of resin co.. |
|||
Density | 1.03 g/cc | 0.0372 lb/in³ | ASTM D792 |
Aclo Accutech Polypropylene Homopolymer HP0336C20L1 Calcium Reinforced |
|||
Density | 1.03 g/cc | 0.0372 lb/in³ | |
BASF 1,4-Dioxane stab Formula: C4H8O2CAS: 123.91.1Description: 1,4-Dioxane stab. is a colorless to yellow liquid, with an ether-like odor. It is miscible with water and other organic solvents. Synonyms: p-Dioxan, Dioxan.. |
|||
Density | 1.03 g/cc | 0.0372 lb/in³ | |
BASF 1-Methyl imidazole Formula: C4H6N2CAS: 616-47-7Description: 1-Methyl imidazole is a colorless to yellow liquid, with an amine-like odor. It is miscible with water.Synonyms: 1-Methyl-1H-imidazole, N-methylimidazoleApp.. |
|||
Density | 1.03 g/cc | 0.0372 lb/in³ | ASTM D792 |
Aclo Accutech Polypropylene Copolymer CP0436C20L Calcium Reinforced |
|||
Density | 1.03 g/cc | 0.0372 lb/in³ | |
BASF Triisopropanolamine 85% Solution Formula: C9H21NO3CAS: 122-20-3Description Triisopropanolamine is a colorless to yellow liquid that is almost odorless. It is fully soluble in water.Synonyms: TRIPA, 1,1’,1”-Nitrilotri-2-propanol,.. |
|||
Density | 1.03 - 1.29 g/cc | 0.0372 - 0.0466 lb/in³ | Average value: 1.13 g/cc Grade Count:91 |
Overview of materials for Nylon 6, Extruded This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Extruded". Each property range of values reported is minimum and maximum values of appropriate .. |
|||
Density | 1.03 g/cc | 0.0372 lb/in³ | |
Solvay RHODAPEX® EAC-70 Surfactant Description: Primary surfactant used in shampoos, bubble baths, shin cleansers and related cosmetic products. For use in both hard and soft water.Chemical Name: AMMONIUM C10-16 ALKYL ETHERS SULFATEI.. |