Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.935 g/cc | 0.0338 lb/in³ | ASTM D792 |
Polimeros Mexicanos Rotolene® 93050 Medium Density Polyethylene Hexene Copolymer Linear Medium Density Polyethylene for rotational molding. This resin is fully UV8 stabilized.Recommended for general purpose applications. Frequently used for water tanks (less tha.. |
|||
Density | 0.935 g/cc | 0.0338 lb/in³ | ASTM D792 |
NOVA Chemicals Novapol® TR-0735-U Hexene MDPE Rotational Molding Resin Good impact resistance, Excellent processabilityApplications: Toys, Complex custom parts, Home and garden items, MailboxesAdditives: Processing antioxidants, UV stabilizersInformation provided by NO.. |
|||
Density | 0.936 g/cc | 0.0338 lb/in³ | ASTM D 792 |
NOVA Chemicals Surpass® FPs236-A Octene sMDPE Film Resin FPs236-A complies with the U.S. FDA regulations for olefin polymers and may thus be used in the United States as an article or component of an article intended for use in contact with food. FPs236-.. |
|||
Density | 0.936 g/cc | 0.0338 lb/in³ | ASTM D1505 |
Formosa Plastics Formolene® L63565 Rotational Molding LLDPE
(discontinued **) Hexene CopolymerApplications: Toys, medium tanks, material handling equipment and flat surface rotational molding applications.Meets all requirements of the U.S. Food and Drug Administration as spec.. |
|||
Density | 0.935 g/cc | 0.0338 lb/in³ | ASTM D1505 |
Formosa Plastics Formolene® L63568U Rotational Molding LLDPE
(discontinued **) Linear Low Density Polyethylene Hexene Copolymer for Rotational Molding Formolene® L63568U is a general-purpose rotational molding linear low density resin made using the BP Gas Phase Process™. Th.. |
|||
Density | 0.936 g/cc | 0.0338 lb/in³ | ASTM D792 |
DuPont Bynel® E403 Acid-Modified Ethylene Terpolymer Adhesive Resin
(discontinued **) Bynel® Series 2000 resins are acid-modified ethylene terpolymers with medium to high acid comonomer contents. They contain a temperature stable ester that makes them functional in high-temperature .. |
|||
Density | 0.936 g/cc | 0.0338 lb/in³ | ASTM D792 |
NOVA Chemicals Sclair® 14A Butene MDPE Film Resin
(discontinued **) Film Properties. Features: Low gel, strength and toughness, broad MW distribution.Applications: Co-extrusion, blending.Data provided by the manufacturer. |
|||
Density | 0.936 g/cc | 0.0338 lb/in³ | ASTM D792 |
NOVA Chemicals Sclair® 14K3 Octene LMDPE Film Resin
(discontinued **) Film Properties. Features: Low gel, excellent optics, good moisture barrier.Applications: Cast overwrap film.Data provided by the manufacturer. |
|||
Density | 0.935 g/cc | 0.0338 lb/in³ | ASTM D1505 |
ICO Polymers ICORENEâ„¢ 115-1323 LMDPE Rotational Molding Resin Description: ICORENE 115-1323 is a linear medium density polyethylene developed for use in rotational molding. It is an easy processing material with good surface gloss, scratch resistance and gene.. |
|||
Density | 0.935 g/cc | 0.0338 lb/in³ | ASTM D1505 |
ICO Polymers ICORENEâ„¢ 115-1329 LMDPE Rotational Molding Resin Description: ICORENE 115-1329 is a linear medium density polyethylene developed for use in rotational molding. It is an easy processing material with good surface gloss, scratch resistance and gene.. |
|||
Density | 0.936 g/cc | 0.0338 lb/in³ | ASTM D1505 |
ICO Polymers ICORENEâ„¢ 190-1325 LMDPE Rotational Molding Resin Description: ICORENE 190-1325 is a linear medium density polyethylene copolymer developed for rotational molding. It has a good balance of properties such as toughness, easy flow and stiffness. Key.. |
|||
Density | 0.935 g/cc | 0.0338 lb/in³ | ASTM D1505 |
ICO Polymers ICORENEâ„¢ 190-1328 LMDPE Rotational Molding Resin Description: ICORENE 190-1328 is a linear medium density polyethylene copolymer developed for rotational molding. It has a good balance of properties such as toughness, easy flow and stiffness. Key.. |
|||
Density | 0.936 g/cc | 0.0338 lb/in³ | Base Resin; ISO 1183 |
Borealis BorPEX™ ME2592 Medium Density Polyethylene Compound for Crosslinked Pipes (Pex-C (Irradiation)) BorPEXME2592 is a natural, high molecular weight, medium density polyethylene for crosslinkable pipes with excellent flexibility. The compound is especially designed for electron beam irradiation c.. |
|||
Density | 0.935 g/cc | 0.0338 lb/in³ | ISO 1183 |
Borealis BorPEX™ ME2510 Medium Density Polyethylene Compound for Crosslinked Pipes (Pex-B (Silane)) BorPEX ME2510 is a silane crosslinkable compound which is used together with a catalyst masterbatch (Cat-MB) to accelerate the moisture-induced crosslinking reaction. It is designed for crosslinkab.. |
|||
Density | 0.935 g/cc | 0.0338 lb/in³ | ASTM D792 |
DuPont Elvax® 550 Ethylene-Vinyl Acetate Copolymer Resin Elvax resins offer a unique combination of processing and performance characteristics. They provide outstanding toughness and resilience and maintain flexibility over a broad temperature range with.. |
|||
Density | 0.935 g/cc | 0.0338 lb/in³ | ExxonMobil method |
ExxonMobil LLDPE LL 6301RQ Wire & Cable Linear Low Density Polyethylene Resin (European Grade) Product Description: LL 6301 is a C4 Ziegler Natta LLDPE recommended for various compounding applications. Availability: Africa & Middle East, Asia Pacific and Europe Additive: Antiblock: No Slip: N.. |
|||
Density | 0.936 g/cc | 0.0338 lb/in³ | ExxonMobil method |
ExxonMobil LLDPE LL 6407.67 Linear Low Density Polyethylene Resin Product Description: LL 6407 is a narrow molecular weight hexene copolymer designed for applications that require outstanding environmental stress crack resistance. This resin offers good processabi.. |
|||
Density | 0.936 g/cc | 0.0338 lb/in³ | ExxonMobil method |
ExxonMobil LLDPE LL 8555.25 Linear Low Density Polyethylene Resin Product Description: LL 8555 is a linear low density hexene copolymer designed to offer superior processability, excellent dimensional control, whiteness and low warpage. This resin is ideally suite.. |
|||
Density | 0.936 g/cc | 0.0338 lb/in³ | ExxonMobil method |
ExxonMobil LLDPE LLP 8555.25 Linear Low Density Polyethylene Resin Product Description: LL 8555 is a linear low density hexene copolymer designed to offer superior processability, excellent dimensional control, whiteness and low warpage. This resin is ideally suite.. |
|||
Density | 0.935 g/cc | 0.0338 lb/in³ | ASTM D1505 |
Arkema Group Orevac® 9309 Film EVA-MAH Terpolymer EVA Terpolymers based Main Application: Cast film coextrusionInformation provided by Arkema Group |
|||
Density | 0.936 g/cc | 0.0338 lb/in³ | ASTM D-1505 |
Bapolene® 345F Medium Density Polyethylene Film Resin Description: Bapolene 345F is a medium molecular weight film resin with excellent tensile, impact, and tear properties. Applications: Merchandise bags, produce and trash bags.Bapolene® and Bapolan®.. |
|||
Density | 0.935 g/cc | 0.0338 lb/in³ | AboCure 50-3 |
Abatron AboCast 7802-1/AboCure 50-3 (40 pbw) Epoxy AboCast 7802-1 is a clear resin with low viscosity (600-800 cps.) and a weight of 9.1 lbs/gallon. AboCure 50-3 is a clear, slow converter for lower rigidity. It has an HDT of 60°C, variable ratio, .. |
|||
Density | 0.935 g/cc | 0.0338 lb/in³ | AboCure 50-3 |
Abatron AboCast 7802-1/AboCure 50-3 (80 pbw) Epoxy AboCast 7802-1 is a clear resin with low viscosity (600-800 cps.) and a weight of 9.1 lbs/gallon. AboCure 50-3 is a clear, slow converter for lower rigidity. It has an HDT of 60°C, variable ratio, .. |
|||
Density | 0.935 g/cc | 0.0338 lb/in³ | AboCure 7804-4 |
Abatron AboCast 7802-1/AboCure 7804-4 (40 pbw) Epoxy AboCast 7802-1 is a clear resin with low viscosity (600-800 cps.) and a weight of 9.1 lbs/gallon. AboCure 7804-4 a clear, more accelerated converter for lower rigidity. It has an HDT of 60°C, varia.. |
|||
Density | 0.935 g/cc | 0.0338 lb/in³ | |
3M Scotch-Weld™ Hi-Strength Postforming 94 CA Spray Adhesive A low VOC, high performance, postformable grade spray adhesive with a unique low telegraphing pebble spray pattern.Features:Bonds to a variety of demanding substrates like decorative laminate, metal.. |
|||
Density | 0.936 g/cc | 0.0338 lb/in³ | ASTM D1505 |
Huntsman Rexell® M3107 Blown Film Extrusion LLDPE
(discontinued **) Linear-low medium density copolymer, cast film extrusion, FDA compliantFeatures: Excellent combination of stiffness, heat resistance, and impermeability to water vapor.Applications: Food packaging, .. |
|||
Density | 0.935 g/cc | 0.0338 lb/in³ | ExxonMobil Method |
ExxonMobil Escorene® LD 728.61 Molding, extrusion and compounding resin Escorene Ultra LD 728.61 is a high vinyl acetate copolymer with low melting temperature and excellent strength properties and toughness.Availability: Latin America, North America and South America A.. |
|||
Density | 0.936 g/cc | 0.0338 lb/in³ | compound; ISO 1872-2/ISO 1183 |
Borealis Borstar® LE8707 Black Bimodal LLDPE Jacketing Compound for Energy and Communication Cables Borstar® LE8707 is a black linear low density (LLD) jacketing compound, which is produced with the Borealis proprietary Borstar® bimodal process technology. Borstar® technology allows the manufa.. |
|||
Density | 0.935 g/cc | 0.0338 lb/in³ | ASTM D792 |
Rochling Engineered Plastics Polystone® Reprocessed (UHMW-PE) Polystone® M is a highly versatile polymer that features: Low coefficient of friction Excellent abrasion resistance High-impact strength Chemical resistance Complies with FDA regulations under the .. |
|||
Density | 0.936 g/cc | 0.0338 lb/in³ | ASTM D792 |
DuPont Bynel® 3933 Anhydride-Modified Ethylene Vinyl Acetate Adhesive Resin
(discontinued **) Bynel® Series 3900 resins are anhydride-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process p.. |