Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.23 - 1.62 g/cc | 0.0444 - 0.0585 lb/in³ | Average value: 1.34 g/cc Grade Count:5 |
Overview of materials for Polyphenylene Ether, Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, Mineral Filled". Each property range of values reported is minimum and maximum valu.. |
|||
Density | 1.29 - 1.62 g/cc | 0.0466 - 0.0585 lb/in³ | Average value: 1.41 g/cc Grade Count:17 |
Overview of materials for Acetal Copolymer, Silicone Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Silicone Filled". Each property range of values reported is minimum and maximum values.. |
|||
Density | 0.880 - 1.62 g/cc | 0.0318 - 0.0585 lb/in³ | Average value: 1.34 g/cc Grade Count:85 |
Overview of materials for PVC, Uncompounded This property data is a summary of similar materials in the MatWeb database for the category "PVC, Uncompounded". Each property range of values reported is minimum and maximum values of appropriate .. |
|||
Density | 1.08 - 1.62 g/cc | 0.0390 - 0.0585 lb/in³ | Average value: 1.48 g/cc Grade Count:18 |
Overview of materials for Polyphenylene Sulfide (PPS) with Carbon Fiber + PTFE Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with Carbon Fiber + PTFE Filler". Each property range of values reported is .. |
|||
Density | 1.20 - 1.62 g/cc | 0.0434 - 0.0585 lb/in³ | Average value: 1.38 g/cc Grade Count:81 |
Overview of materials for Nylon 6, 30% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 30% Mineral Filled". Specific grades with primary filler content between 25% and 34% are includ.. |
|||
Density | 1.39 - 1.62 g/cc | 0.0502 - 0.0585 lb/in³ | Average value: 1.51 g/cc Grade Count:45 |
Overview of materials for Nylon 66/6, 40% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 40% Glass Fiber Reinforced". Specific grades with glass content between 35% and 44% are incl.. |
|||
Density | 1.23 - 1.62 g/cc | 0.0444 - 0.0585 lb/in³ | Average value: 1.39 g/cc Grade Count:45 |
Overview of materials for Nylon 66, 30% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 30% Mineral Filled". Specific grades with primary filler content between 25% and 34% are inclu.. |
|||
Density | 1.58 - 1.62 g/cc | 0.0571 - 0.0585 lb/in³ | ISO R 1184 |
Fainplast Compounds RE 240 Rigid PVC, Extrusion Electric channels |
|||
Density | 1.58 - 1.62 g/cc | 0.0571 - 0.0585 lb/in³ | IEC 60811 |
Fainplast Compounds HAX HF 019/HT6 Halogen Free PVC High fire performances, good flexibility |
|||
Density | 1.60 - 1.62 g/cc | 0.0578 - 0.0585 lb/in³ | |
Beijing Evergrow Resources CFC-DD-1000 Carbon Fiber Cloth The viscose yarn(cloth) are converted into carbon fiber(cloth) by the special process of weaving, preoxidization, carbonization aftertreatment etc. It has the good high temperature resistance, corro.. |
|||
Density | 1.60 - 1.62 g/cc | 0.0578 - 0.0585 lb/in³ | |
Beijing Evergrow Resources CFC-DD-1000S Carbon Fiber Cloth The viscose yarn(cloth) are converted into carbon fiber(cloth) by the special process of weaving, preoxidization, carbonization aftertreatment etc. It has the good high temperature resistance, corro.. |
|||
Density | 1.60 - 1.62 g/cc | 0.0578 - 0.0585 lb/in³ | |
Beijing Evergrow Resources CFC-DDX-1000S Carbon Fiber Cloth The viscose yarn(cloth) are converted into carbon fiber(cloth) by the special process of weaving, preoxidization, carbonization aftertreatment etc. It has the good high temperature resistance, corro.. |
|||
Density | 1.55 - 1.62 g/cc | 0.0560 - 0.0585 lb/in³ | Molding; IS 867-1963 |
Amity Thermosets ATS 131 Phenolic Molding Organic and graphite Filler, Compression Molded Characteristics:Self lubricating ( graphite modified )Good glide propertiesGood sealing propertiesMedium or low mechanical strengthUnsuitable for electrical applicationGlossy surfaceThermal conducti.. |
|||
Density | 1.60 - 1.62 g/cc | 0.0578 - 0.0585 lb/in³ | |
Beijing Evergrow Resources CFC-DDX-1000 Carbon Fiber Cloth The viscose yarn(cloth) are converted into carbon fiber(cloth) by the special process of weaving, preoxidization, carbonization aftertreatment etc. It has the good high temperature resistance, corro.. |
|||
Density | 1.58 - 1.62 g/cc | 0.0571 - 0.0585 lb/in³ | ISO R 1184 |
Fainplast Compounds RE 224 Rigid PVC, Extrusion Various profiles |
|||
Density | 1.58 - 1.62 g/cc | 0.0571 - 0.0585 lb/in³ | ISO R 1184 |
Fainplast Compounds RE 430 Rigid PVC, Extrusion Electric channels |
|||
Density | 1.47 - 1.62 g/cc | 0.0531 - 0.0585 lb/in³ | Average value: 1.51 g/cc Grade Count:27 |
Overview of materials for Polyethersulfone (PES), 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone (PES), 20% Glass Fiber Filled". Each property range of values reported is minimum and m.. |
|||
Density | 1.58 - 1.62 g/cc | 0.0571 - 0.0585 lb/in³ | ISO R 1184 |
Fainplast Compounds RE 230/D Rigid PVC, Extrusion Electric channels |