Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.45 - 1.55 g/cc | 0.0524 - 0.0560 lb/in³ | wet density (as supplied) |
Pyrotek Insural® 85 MASTIC Insulating Mastic for Aluminum contact Applications Insural® 85 MASTIC is an asbestos-free, durable and insulating refractory composition designed for the fabrication of launders and jointing, bedding and patching of precast refractory shapes.Advant.. |
|||
Density | 1.45 - 1.55 g/cc | 0.0524 - 0.0560 lb/in³ | wet density (as supplied) |
Pyrotek Insural® GP MASTIC Insulating mastic for general-purpose refractory applications Insural® GP Mastic is an asbestos-free, durable and insulating refractory fiber composition designed for general-purpose patching and veneering applications that are not exposed to contact with mol.. |
|||
Density | 1.11 - 1.55 g/cc | 0.0401 - 0.0560 lb/in³ | Average value: 1.39 g/cc Grade Count:88 |
Overview of materials for Polybutylene Terephthalate (PBT), 10% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 10% Glass Fiber Filled".Specific grades with glass content between 5% .. |
|||
Density | 1.00 - 1.55 g/cc | 0.0361 - 0.0560 lb/in³ | Average value: 1.21 g/cc Grade Count:282 |
Overview of materials for Polycarbonate, Unreinforced, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Unreinforced, Flame Retardant". Each property range of values reported is minimum and max.. |
|||
Density | 1.50 - 1.55 g/cc | 0.0542 - 0.0560 lb/in³ | Average value: 1.52 g/cc Grade Count:4 |
Overview of materials for PVC, 20% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "PVC, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% are included. E.. |
|||
Density | 1.31 - 1.55 g/cc | 0.0473 - 0.0560 lb/in³ | Average value: 1.42 g/cc Grade Count:8 |
Overview of materials for Phenolic, Carbon Fiber Composite This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Carbon Fiber Composite". Each property range of values reported is minimum and maximum values .. |
|||
Density | 1.51 - 1.55 g/cc | 0.0546 - 0.0560 lb/in³ | ISO R 1184 |
Fainplast Compounds RE 520/1 Rigid PVC, Extrusion Electric pipes |
|||
Density | 1.46 - 1.55 g/cc | 0.0527 - 0.0560 lb/in³ | Fusor 2001 |
Lord Adhesives Fusor® 2001 / 2002 Urethane Adhesive Fusor® 2001/2002 is a two-part urethane adhesive system used to bond fiberglass reinforced plastics, sheet molded compound, and bulk molded compound to themselves as well as to primed metals.All .. |
|||
Density | 1.45 - 1.55 g/cc | 0.0524 - 0.0560 lb/in³ | |
Sibur 1030-13 Compound OMN Polyvinyl Chloride (PVC) Shall correspond to control sample, approved in accordance with the established procedure. Pores, which can be seen by eyes, are not allowed. Plastic shall no burn at stop of worm extruder for a p.. |
|||
Density | 1.53 - 1.55 g/cc | 0.0553 - 0.0560 lb/in³ | Laminate |
Hexcel® HexPly® F652 Bismaleimide Resin, Carbon Fabric Form Material Description: F3G584-60; Fiber: T300-3K; T300/13.5 mils (0.343 mm) per plyInformation provided by HexCel |
|||
Density | 1.52 - 1.55 g/cc | 0.0549 - 0.0560 lb/in³ | |
Chengdu Polyster RPM440 Flame Retardant Masterbatch RPM 440 is a flame retardant phosphorus based additive designed for use in reinforced polyamide resins. It is halogen-free and has good flame retardant performance. Red pellet form. Used for electri.. |
|||
Density | 1.52 - 1.55 g/cc | 0.0549 - 0.0560 lb/in³ | |
Chengdu Polyster RPM540B Flame Retardant Masterbatch RPM540B is a red phosphorus based additive flame retardant designed for PBT resins. It is halogen-free and has good flame retardant performance. Red pellet form. Used for electrical componentsInform.. |
|||
Density | 1.51 - 1.55 g/cc | 0.0546 - 0.0560 lb/in³ | ISO R 1183 |
Fainplast Compounds FKA 89 Flexible PVC, Flame Retardant Insulation Lead Free Power cables |
|||
Density | 1.51 - 1.55 g/cc | 0.0546 - 0.0560 lb/in³ | ISO R 1183 |
Fainplast Compounds GA 025/12 Flexible PVC, Flame Retardant Sheathing Sheathing low smoke opacity |
|||
Density | 1.51 - 1.55 g/cc | 0.0546 - 0.0560 lb/in³ | ISO R 1183 |
Fainplast Compounds GK 90 Flexible PVC, Flame Retardant Sheathing Lead Free General purposes |
|||
Density | 1.51 - 1.55 g/cc | 0.0546 - 0.0560 lb/in³ | IEC 60811 |
Fainplast Compounds HAX HF 018/9 Halogen Free PVC General purpose |
|||
Density | 1.51 - 1.55 g/cc | 0.0546 - 0.0560 lb/in³ | IEC 60811 |
Fainplast Compounds HAX HF 029/47 Halogen Free PVC General purpose |
|||
Density | 1.51 - 1.55 g/cc | 0.0546 - 0.0560 lb/in³ | IEC 60811 |
Fainplast Compounds HAX HF 4021/TC Halogen Free PVC Improved flame retardancy |
|||
Density | 1.51 - 1.55 g/cc | 0.0546 - 0.0560 lb/in³ | ISO R 1184 |
Fainplast Compounds HGA 40 Flexible PVC, Sheathing for High Temperatures Sheath high L.O.I. |
|||
Density | 1.51 - 1.55 g/cc | 0.0546 - 0.0560 lb/in³ | ISO R 1184 |
Fainplast Compounds HGKA 0183 Flexible PVC, Sheathing for High Temperatures Lead Free Sheathing high LOI |
|||
Density | 1.51 - 1.55 g/cc | 0.0546 - 0.0560 lb/in³ | ISO R 1184 |
Fainplast Compounds R 316/AS Rigid PVC, Extrusion Antistatic profiles |
|||
Density | 1.51 - 1.55 g/cc | 0.0546 - 0.0560 lb/in³ | ISO 1183 |
Fainplast Compounds Hax™ HF 4021/TC Flame Retardant Polyolefin Cable Compound Thermoplastic halogen free flame retardant compound based on polyolefins and mineral fillersGrade description:Improved flame retardancyInformation provided by Fainplast Compounds |
|||
Density | 1.52 - 1.55 g/cc | 0.0549 - 0.0560 lb/in³ | MIL-PRF-81733D |
3M AC-665 Class C-12 Aerospace Sealant 3M Aerospace Sealant AC-665 Class C are two-part, manganese-cured, chromate containing, corrosion inhabiting sealants. These Sealants provide an effective barrier against the common causes of corros.. |
|||
Density | 1.52 - 1.55 g/cc | 0.0549 - 0.0560 lb/in³ | MIL-PRF-81733D |
3M AC-665 Class C-24 Aerospace Sealant 3M Aerospace Sealant AC-665 Class C are two-part, manganese-cured, chromate containing, corrosion inhabiting sealants. These Sealants provide an effective barrier against the common causes of corros.. |
|||
Density | 1.45 - 1.55 g/cc | 0.0524 - 0.0560 lb/in³ | Molding; IS 867-1963 |
Amity Thermosets ATI 172 Phenolic Molding Organic and inorganic Filler, Injection Molded Characteristics:Heat resistant ( asbestos free )Good electric insulationLow shrinkageLow water absorptionMedium mechanical strengthNot suitable for high mechanical tensionColor-blackVery soft flow .. |
|||
Density | 1.45 - 1.55 g/cc | 0.0524 - 0.0560 lb/in³ | Molding; IS 867-1963 |
Amity Thermosets ATS 1613-G Phenolic Molding Nylon and inorganic Filler, Compression Molded Characteristics:High dielectric & mechanical strengthWeather resistant Good electric insulationLow water absorption Good mechanical tension bearing capacityColor-blackSoft/Medium flow Applications:R.. |
|||
Density | 1.42 - 1.55 g/cc | 0.0513 - 0.0560 lb/in³ | Average value: 1.49 g/cc Grade Count:31 |
Overview of materials for Acetal Homopolymer, PTFE-Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Homopolymer, PTFE-Filled". Each property range of values reported is minimum and maximum values o.. |
|||
Density | 1.08 - 1.55 g/cc | 0.0390 - 0.0560 lb/in³ | Average value: 1.28 g/cc Grade Count:77 |
Overview of materials for Polycarbonate, PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, PTFE Filled". Each property range of values reported is minimum and maximum values of app.. |
|||
Density | 1.51 - 1.55 g/cc | 0.0546 - 0.0560 lb/in³ | ISO R 1184 |
Fainplast Compounds R 244 Rigid PVC, Extrusion Shutters high modulus low curving |
|||
Density | 1.13 - 1.55 g/cc | 0.0408 - 0.0560 lb/in³ | Average value: 1.31 g/cc Grade Count:7 |
Overview of materials for Polyphenylene Ether, Glass/Graphite Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, Glass/Graphite Reinforced". Each property range of values reported is minimum and m.. |