Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Density = 1.49 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 1.29 - 1.49 g/cc

@Temperature 250 - 250 °C
0.0466 - 0.0538 lb/in³

@Temperature 482 - 482 °F
Average value: 1.40 g/cc Grade Count:6
Overview of materials for Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled". Specific grades with glass content between 25..
Density 1.37 - 1.49 g/cc
0.0495 - 0.0538 lb/in³
Average value: 1.43 g/cc Grade Count:3
Overview of materials for Polyarylsulfone (PAS), Molded/Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Polyarylsulfone; Molded/Extruded". Each property range of values reported is minimum and maximum values ..
Density 1.25 - 1.49 g/cc
0.0452 - 0.0538 lb/in³
Average value: 1.36 g/cc Grade Count:34
Overview of materials for PVC/Acrylic Alloy
This property data is a summary of similar materials in the MatWeb database for the category "PVC/Acrylic Alloy". Each property range of values reported is minimum and maximum values of appropriate ..
Density 1.29 - 1.49 g/cc
0.0466 - 0.0538 lb/in³
Average value: 1.38 g/cc Grade Count:48
Overview of materials for Polyetherimide (PEI), Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide, Carbon Fiber Filled". Each property range of values reported is minimum and maximum valu..
Density 1.27 - 1.49 g/cc
0.0459 - 0.0538 lb/in³
Average value: 1.34 g/cc Grade Count:14
Overview of materials for Polysulfone, 10% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polysulfone, 10% Glass Fiber Reinforced". Specific grades with glass content between 5% and 14% are incl..
Density 1.45 - 1.49 g/cc
0.0524 - 0.0538 lb/in³
ISO R 1184
Fainplast Compounds RH 210/W Rigid PVC, Antishock Extrusion
Various antishock profiles
Density 1.45 - 1.49 g/cc
0.0524 - 0.0538 lb/in³
ISO R 1184
Fainplast Compounds RH 4410 Rigid PVC, Antishock Extrusion
Antishock spiral pipes
Density 1.45 - 1.49 g/cc
0.0524 - 0.0538 lb/in³
ISO R 1184
Fainplast Compounds RKS 218/W Rigid PVC, Antishock Extrusion Lead Free
Antishock profiles
Density 1.46 - 1.49 g/cc
0.0527 - 0.0538 lb/in³
ASTM D792
KYDEX® 6565 Acrylic/PVC Thermoplastic Sheet
Low heat release aviation gradeApplications: Airducts, seat parts, bulkhead laminates, escape slide packboards, gallery parts, instrument panels, laboratory floorplans, sidewall panels, life vest sh..
Density 1.475 - 1.49 g/cc
0.05329 - 0.0538 lb/in³
ISO 1183
Tisan TISMOSET®
Properties:Flame retardantHigh gloss surfaceImproved thermal and electircal strengthHigh impact strengthMinimized shrinkage at the presence of moldingHigh melting flow indexReduced moisture absorpti..
Density 1.45 - 1.49 g/cc
0.0524 - 0.0538 lb/in³
ISO R 1183
Fainplast Compounds FR 80 Flexible PVC, Insulation
General purposes
Density 1.45 - 1.49 g/cc
0.0524 - 0.0538 lb/in³
ISO R 1183
Fainplast Compounds GA 0179 Flexible PVC, Flame Retardant Sheathing
Hydrocarbon resistant sheathing
Density 1.45 - 1.49 g/cc
0.0524 - 0.0538 lb/in³
ISO 1183
Fainplast Compounds Hax™ HFX 500 Crosslinkable HFFR Cable Compound
Polyolefin based HFFR silane grafted compound; cross-linkable by heat and moisture and by addition of suitable catalystGrade description:• Standard sheathingInformation provided by Fainplast Compou..
Density 1.45 - 1.49 g/cc
0.0524 - 0.0538 lb/in³
ISO 1183
Fainplast Compounds Hax™ HFX 500S Crosslinkable HFFR Cable Compound
Polyolefin based HFFR silane grafted compound; cross-linkable by heat and moisture and by addition of suitable catalystGrade description:• Sheathing for solar cablesInformation provided by Fainplas..
Density 1.45 - 1.49 g/cc
0.0524 - 0.0538 lb/in³
ISO R 1183
Fainplast Compounds HL 90/4 Flexible PVC, Insulation for High Temperatures
Operating temperature 105°C
Density 1.45 - 1.49 g/cc
0.0524 - 0.0538 lb/in³
ISO R 1183
Fainplast Compounds CL 70 Flexible PVC, Sheathing
General purposes
Density 1.12 - 1.49 g/cc
0.0405 - 0.0538 lb/in³
Average value: 1.26 g/cc Grade Count:31
Overview of materials for Nylon 6, PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, PTFE Filled". Each property range of values reported is minimum and maximum values of appropria..
Density 1.19 - 1.49 g/cc
0.0430 - 0.0538 lb/in³
Average value: 1.30 g/cc Grade Count:11
Overview of materials for Acrylic/Polycarbonate Alloy, Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic/Polycarbonate Alloy, Glass Fiber Filler". Each property range of values reported is minimum and ..
Density 1.45 - 1.49 g/cc
0.0524 - 0.0538 lb/in³
ISO 1183
Fainplast Compounds Hax™ HF 223F Flame Retardant Polyolefin Cable Compound
Thermoplastic halogen free flame retardant compound based on polyolefins and mineral fillersGrade description:High flexibility, good stress crack resistanceInformation provided by Fainplast Compound..
Density 1.08 - 1.49 g/cc
0.0390 - 0.0538 lb/in³
Average value: 1.13 g/cc Grade Count:26
Overview of materials for Polypropylene with 30% Mica Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 30% Mica Filler". Specific grades with primary filler content between 25% and 34% are..