Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.17 - 1.23 g/cc | 0.0423 - 0.0444 lb/in³ | ASTM D792 |
Multibase Multi-Flex® TPE A 6221 M BLK The burn rate is 1 in/min (25 mm/min) based on ASTM FM VSS 302. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase. |
|||
Density | 1.19 - 1.23 g/cc | 0.0430 - 0.0444 lb/in³ | Average value: 1.21 g/cc Grade Count:19 |
Overview of materials for PCTG Copolyester This property data is a summary of similar materials in the MatWeb database for the category "PCTG Copolyester". Each property range of values reported is minimum and maximum values of appropriate M.. |
|||
Density | 1.17 - 1.23 g/cc | 0.0423 - 0.0444 lb/in³ | RPG24 |
Solvay MIRACARE® P IS-C Surfactant Description: Water soluble preservative, suitable for rinse-off products. Highly effective at low concentration.I.N.C.I. Name: METHYLCHLOROISOTHIAZOLINONE ; METHYLISOTHIAZOLINONE ; MAGNESIUM NITRATE.. |
|||
Density | 1.19 - 1.23 g/cc | 0.0430 - 0.0444 lb/in³ | ISO R 1183 |
Fainplast Compounds FAINGUM 6510 Flexible PVC, Injection Molding for Footwear Soles with rubber |
|||
Density | 1.19 - 1.23 g/cc | 0.0430 - 0.0444 lb/in³ | ISO R 1183 |
Fainplast Compounds GS 64/70 Flexible PVC, Injection Molding for Footwear Soles for cold climates |
|||
Density | 1.19 - 1.23 g/cc | 0.0430 - 0.0444 lb/in³ | ISO R 1183 |
Fainplast Compounds GS 66/F Flexible PVC, Injection Molding for Footwear Fluorescent sandals |
|||
Density | 1.19 - 1.23 g/cc | 0.0430 - 0.0444 lb/in³ | ISO R 1183 |
Fainplast Compounds GS 69/T Flexible PVC, Injection Molding for Footwear Crystal sandals |
|||
Density | 1.19 - 1.23 g/cc | 0.0430 - 0.0444 lb/in³ | ISO R 1183 |
Fainplast Compounds GS 70/AT Flexible PVC, Injection Molding for Transparent Technical Items Toys |
|||
Density | 1.19 - 1.23 g/cc | 0.0430 - 0.0444 lb/in³ | ISO R 1183 |
Fainplast Compounds GS 7005/BT Flexible PVC, Injection Molding for Footwear Soles for cold climates |
|||
Density | 1.19 - 1.23 g/cc | 0.0430 - 0.0444 lb/in³ | ISO R 1183 |
Fainplast Compounds GS 74/BT Flexible PVC, Injection Molding for Footwear Soles for cold climates |
|||
Density | 1.19 - 1.23 g/cc | 0.0430 - 0.0444 lb/in³ | ISO R 1183 |
Fainplast Compounds GS 75/T Flexible PVC, Injection Molding for Footwear Crystal sandals |
|||
Density | 1.19 - 1.23 g/cc | 0.0430 - 0.0444 lb/in³ | ISO R 1184 |
Fainplast Compounds MPH 69 Medical Flexible PVC, Extrusion Tubolar apparatus |
|||
Density | 1.19 - 1.23 g/cc | 0.0430 - 0.0444 lb/in³ | ISO R 1184 |
Fainplast Compounds MPH 78/OP Medical Flexible PVC, Extrusion Tubolar apparatus anti bend |
|||
Density | 1.19 - 1.23 g/cc | 0.0430 - 0.0444 lb/in³ | ISO R 1183 |
Fainplast Compounds PG 58/K1-UV Flexible PVC, Extrusion Modified with Rubber Gaskets mat finish UV-Resistant |
|||
Density | 1.19 - 1.23 g/cc | 0.0430 - 0.0444 lb/in³ | ISO 1183 |
Austin Novel Materials Texalan® 290A Polyester-based TPU Description: Good abrasion resistance, tensile strength, oil resistance and transparency which can meet different demands in various industryInformation from Dawnentech |
|||
Density | 1.19 - 1.23 g/cc | 0.0430 - 0.0444 lb/in³ | ISO 1183 |
Austin Novel Materials Texalan® 295A Polyester-based TPU Description: Good abrasion resistance, tensile strength, oil resistance and transparency which can meet different demands in various industryInformation from Dawnentech |
|||
Density | 1.19 - 1.23 g/cc | 0.0430 - 0.0444 lb/in³ | ISO 1183 |
Austin Novel Materials Texalan® 390A Polyester-based TPU Description: Good abrasion resistance, tensile strength, oil resistance which can be used in injection, extrusion purpose.Information from Dawnentech |
|||
Density | 1.19 - 1.23 g/cc | 0.0430 - 0.0444 lb/in³ | ISO 1183 |
Austin Novel Materials Texalan® 490A Polyester-based TPU Description: Can be considered as custom-made products which use different raw materials to meet customers special requirementsInformation from Dawnentech |
|||
Density | 1.19 - 1.23 g/cc | 0.0430 - 0.0444 lb/in³ | ISO 1183 |
Austin Novel Materials Texalan® 495A Polyester-based TPU Description: Can be considered as custom-made products which use different raw materials to meet customers special requirementsInformation from Dawnentech |
|||
Density | 1.19 - 1.23 g/cc | 0.0430 - 0.0444 lb/in³ | ISO 1183 |
Austin Novel Materials Texalan® 690A Polyester and Polyether based TPU Description: A kind of custom-made products which use different raw materials to meet customers special requirementsInformation from Dawnentech |
|||
Density | 1.19 - 1.23 g/cc | 0.0430 - 0.0444 lb/in³ | ISO 1183 |
Austin Novel Materials Texalan® 395A Polyester-based TPU Description: Good abrasion resistance, tensile strength, oil resistance which can be used in injection, extrusion purpose.Information from Dawnentech |
|||
Density | 1.19 - 1.23 g/cc | 0.0430 - 0.0444 lb/in³ | ISO R 1184 |
Fainplast Compounds KLT 75/G Flexible PVC, Sheathing Transparent Cables Lead Free Transparent sheathing |
|||
Density | 1.19 - 1.23 g/cc | 0.0430 - 0.0444 lb/in³ | ISO R 1183 |
Fainplast Compounds PG 60/C Flexible PVC, Extrusion Modified with Rubber Gaskets modified with rubber |
|||
Density | 1.19 - 1.23 g/cc | 0.0430 - 0.0444 lb/in³ | ISO R 1183 |
Fainplast Compounds PH 68/A Flexible PVC, Transparent Extrusion Profiles, UL Class V1 |
|||
Density | 1.19 - 1.23 g/cc | 0.0430 - 0.0444 lb/in³ | ISO 1183 |
Austin Novel Materials Texalan® 695A Polyester and Polyether based TPU Description: A kind of custom-made products which use different raw materials to meet customers special requirementsInformation from Dawnentech |
|||
Density | 1.19 - 1.23 g/cc | 0.0430 - 0.0444 lb/in³ | ISO 1183 |
Austin Novel Materials Texalan® 798A PCL TPU Description: Good abrasion resistance, tensile strength, oil resistance and heat resistance which can be used in mechanic parts and various industry parts.Information from Dawnentech |
|||
Density | 1.19 - 1.23 g/cc | 0.0430 - 0.0444 lb/in³ | ISO R 1183 |
Fainplast Compounds PMP 77 Flexible PVC, Extrusion Modified with PU Various profiles |
|||
Density | 1.04 - 1.23 g/cc | 0.0376 - 0.0444 lb/in³ | Average value: 1.17 g/cc Grade Count:9 |
Overview of materials for Polypropylene with Glass Fiber + Bead Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with Glass Fiber + Bead Filler". Each property range of values reported is minimum and max.. |
|||
Density | 1.19 - 1.23 g/cc | 0.0430 - 0.0444 lb/in³ | ISO R 1183 |
Fainplast Compounds PMP 338 Flexible PVC, Extrusion Modified with PU Sheath PVC/PU for low temperatures |
|||
Density | 0.872 - 1.23 g/cc | 0.0315 - 0.0444 lb/in³ | Average value: 1.02 g/cc Grade Count:19 |
Overview of materials for Polypropylene, Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Carbon Fiber 10%". Each property range of values reported is minimum and maximum values o.. |