Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.04 - 1.05 g/cc | 0.0376 - 0.0379 lb/in³ | Polymerized; ASTM D792 |
Proto3000 Objet VeroClear FullCure810 Information provided by Proto3000 for their protoyping engineering services. |
|||
Density | 0.995 - 1.05 g/cc | 0.0359 - 0.0381 lb/in³ | |
Lord Adhesives 506 Semi-Flexible, Medium Cure, Medium Viscosity Acrylic Adhesive Lord 500 SeriesLord 500 Series Acrylic Adhesives bond plastics and prepared metals; they offer excellent adhesion to both thermoplastics and thermoset plastics. They are available with varying handi.. |
|||
Density | 0.995 - 1.05 g/cc | 0.0359 - 0.0381 lb/in³ | |
Lord Adhesives 510 Fast Cure Acrylic Adhesive Lord 500 SeriesLord 500 Series Acrylic Adhesives bond plastics and prepared metals; they offer excellent adhesion to both thermoplastics and thermoset plastics. They are available with varying handi.. |
|||
Density | 1.04 - 1.05 g/cc | 0.0376 - 0.0379 lb/in³ | |
Solvay ALKAMULS® EL 620 Surfactant Description: Castor oil ethoxylate (30 EO) Emulsifier for fats, oils fatty acids and solvents. Maintains stability of oil-in-water emulsions over a wide temperature range as co-emulsifier with an HL.. |
|||
Density | 1.01 - 1.05 g/cc | 0.0365 - 0.0379 lb/in³ | |
3M 32661 Heavy Duty Performance Coating - Part B 3M™ HD (Heavy Duty) Performance Coating is 100% solids elastomeric lining especially developed for high abrasion and tear resistance with thick build up characteristics. It has good durability and .. |
|||
Density | 1.03 - 1.05 g/cc | 0.0372 - 0.0379 lb/in³ | Typical; ISO 1183-1 |
Axion Polymers Axpoly® PS01 Impact Modified Polystyrene 100% post-consumer recycled polymer (recovered from refrigerators)93% less CO2 impact compared with virgin*Successfully replaces virgin grade resinISO9000 quality certifiedAvailable in a range of co.. |
|||
Density | 1.02 - 1.05 g/cc | 0.0368 - 0.0379 lb/in³ | |
BASF Neopor® 2300 Expandable Polystyrene Description: Expandable polystyrene (EPS) containing uniformly distributed flame retardant (blowing agent: pentane).Remarks: For the production of flame-retardant silver-gray foams having a consider.. |
|||
Density | 1.02 - 1.05 g/cc | 0.0368 - 0.0379 lb/in³ | |
BASF Neopor® 2400 Expandable Polystyrene Description: Expandable polystyrene (EPS) containing uniformly distributed flame retardant (blowing agent: pentane).Remarks: For the production of flame-retardant silver-gray foams having a consider.. |
|||
Density | 1.02 - 1.05 g/cc | 0.0368 - 0.0379 lb/in³ | |
BASF Neopor® 5300 Plus Expandable Polystyrene Description: Expandable polystyrene (EPS) containing uniformly distributed flame retardant (blowing agent: pentane).Remarks: For the production of flame-retardant silver-gray foams having a consider.. |
|||
Density | 1.02 - 1.05 g/cc | 0.0368 - 0.0379 lb/in³ | |
BASF Peripor® 200 Expandable Polystyrene Description: Expandable polystyrene (EPS) with uniformly distributed flame retardant (blowing agent: pentane)Remarks: Low-pentane products for the production of flame-retardant foams displaying low .. |
|||
Density | 1.02 - 1.05 g/cc | 0.0368 - 0.0379 lb/in³ | |
BASF Styropor® F 215 N Expandable Polystyrene Description: Expandable polystyrene (EPS) containing a uniformly distributed ?ame retardant (blowing agent: pentane)Remarks: For the manufacture of flame-retardant foams.Applications: Blocks, insula.. |
|||
Density | 1.02 - 1.05 g/cc | 0.0368 - 0.0379 lb/in³ | |
BASF Styropor® F 215 T-N Expandable Polystyrene Use: Expanding-agent containing plastic for the production of foam plasticInformation provided by BASF |
|||
Density | 1.02 - 1.05 g/cc | 0.0368 - 0.0379 lb/in³ | |
BASF Styropor® F 315 T-N Expandable Polystyrene Use: Expanding-agent containing plastic for the production of foam plasticsInformation provided by BASF |
|||
Density | 1.02 - 1.05 g/cc | 0.0368 - 0.0379 lb/in³ | |
BASF Styropor® F 395 -N Expandable Polystyrene Description: Expandable polystyrene (EPS) containing uniformly distributed flame retardant (blowing agent: pentane)Remarks: Production of flame-retardant foams displaying low post-shrinkage.Applicat.. |
|||
Density | 1.02 - 1.05 g/cc | 0.0368 - 0.0379 lb/in³ | |
BASF Styropor® F 415-N Expandable Polystyrene Description: Expandable polystyrene (EPS) containing uniformly distributed flame retardant (blowing agent: pentane)Remarks: For the manufacture of flame-retardant foamsApplications: Visible cover pa.. |
|||
Density | 1.02 - 1.05 g/cc | 0.0368 - 0.0379 lb/in³ | |
BASF Styropor® P 326 M Expandable Polystyrene Description: Expandable polystyrene (EPS) (blowing agent: pentane).Remarks: Good foaming capacity, energy-saving processing and short cycle time.Applications: Molded parts with very good mechanical .. |
|||
Density | 1.02 - 1.05 g/cc | 0.0368 - 0.0379 lb/in³ | |
BASF Styropor® P 570 Expandable Polystyrene Additive Description: Expandable polystyrene (EPS) (blowing agent: pentane).Remarks: Only foamed particles, good foaming capacity.Applications: For the production of expanded particles as a filling material .. |
|||
Density | 0.970 - 1.05 g/cc | 0.0350 - 0.0379 lb/in³ | ASTM D 792 |
API Megol AM SV/PS SEBS Adhesion Modified Overmolding for PS Over-molding allows for the creation of composite finished products in a single phase, removing the need for successive gluing or mechanical fixing steps. This also reduces environmental impact as .. |
|||
Density | 1.02 - 1.05 g/cc | 0.0368 - 0.0379 lb/in³ | |
BASF Peripor® 300 Expandable Polystyrene Description: Expandable polystyrene (EPS) with uniformly distributed flame retardant (blowing agent: pentane)Remarks: Low-pentane products for the production of flame-retardant foams displaying low .. |
|||
Density | 1.02 - 1.05 g/cc | 0.0368 - 0.0379 lb/in³ | |
BASF Styropor® F 215 L-N Expandable Polystyrene Description: Expandable polystyrene (EPS) containing a uniformly distributed came retardant (blowing agent: pentane)Remarks: For the manufacture of flame-retardant foams.Applications: Low-density bl.. |
|||
Density | 1.02 - 1.05 g/cc | 0.0368 - 0.0379 lb/in³ | |
BASF Styropor® F 295-N Expandable Polystyrene Description: Expandable polystyrene (EPS) containing uniformly distributed flame retardant (blowing agent: pentane)Remarks: Production of flame-retardant foams displaying low post-shrinkageApplicati.. |
|||
Density | 1.02 - 1.05 g/cc | 0.0368 - 0.0379 lb/in³ | |
BASF Styropor® F 495-N Expandable Polystyrene Description: Expandable polystyrene (EPS) containing uniformly distributed flame retardant (blowing agent: pentane)Remarks: Production of flame-retardant foams displaying low post-shrinkage.Applicat.. |
|||
Density | 1.02 - 1.05 g/cc | 0.0368 - 0.0379 lb/in³ | |
BASF Styropor® P 226 C Expandable Polystyrene Description: Expandable polystyrene (EPS) (blowing agent: pentane).Remarks: Good foaming capacity, energy-saving processing and short cycle time.Applications: Blocks with very short cycle times.Info.. |
|||
Density | 1.02 - 1.05 g/cc | 0.0368 - 0.0379 lb/in³ | |
BASF Styropor® P 326 Expandable Polystyrene Description: Expandable polystyrene (EPS) (blowing agent: pentane).Remarks: Good foaming capacity, energy-saving processing and short cycle time.Applications: Molded partsInformation provided by BAS.. |
|||
Density | 1.02 - 1.05 g/cc | 0.0368 - 0.0379 lb/in³ | |
BASF Styropor® P 426 Expandable Polystyrene Description: Expandable polystyrene (EPS) (blowing agent: pentane).Remarks: Good foaming capacity, energy-saving processing and short cycle time.Applications: Thin-walled molded parts.Information pr.. |
|||
Density | 1.02 - 1.05 g/cc | 0.0368 - 0.0379 lb/in³ | |
BASF Styropor® P 656 Expandable Polystyrene Additive Description: Expandable polystyrene (EPS) (blowing agent: pentane).Remarks: Only foamed particles, good foaming capacity.Applications: Filling material for lightweight plasters.Information provided .. |
|||
Density | 0.930 - 1.05 g/cc | 0.0336 - 0.0379 lb/in³ | Average value: 0.945 g/cc Grade Count:22 |
Overview of materials for Medium Density Polyethylene (MDPE), Extruded This property data is a summary of similar materials in the MatWeb database for the category "Medium Density Polyethylene (MDPE), Extruded". Each property range of values reported is minimum and max.. |
|||
Density | 1.00 - 1.05 g/cc | 0.0361 - 0.0379 lb/in³ | Average value: 1.03 g/cc Grade Count:36 |
Overview of materials for Nylon 11, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11, Unreinforced". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Density | 1.02 - 1.05 g/cc | 0.0368 - 0.0379 lb/in³ | |
BASF Neopor® 2200 Expandable Polystyrene Description: Expandable polystyrene (EPS) containing uniformly distributed flame retardant (blowing agent: pentane).Remarks: For the production of flame-retardant silver-gray foams having a consider.. |
|||
Density | 1.02 - 1.05 g/cc | 0.0368 - 0.0379 lb/in³ | |
BASF Neopor® P 5200 Expandable Polystyrene Description: Expandable polystyrene (EPS) containing uniformly distributed flame retardant (blowing agent: pentane).Remarks: For the production of silver-gray foams having a considerably higher ther.. |