Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

API Megol AM SV/PS SEBS Adhesion Modified Overmolding for PS

Category Polymer , Thermoplastic , Elastomer, TPE , Styrenic TPE
Manufacturer A.P.I. SpA
Trade Name Megol AM
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF API Megol AM SV/PS SEBS Adhesion Modified Overmolding for PS.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Over-molding allows for the creation of composite finished products in a single phase, removing the need for successive gluing or mechanical fixing steps. This also reduces environmental impact as there are no VOC emissions from adhesives and, as the components are not made from a range of incompatible materials, they are more easily recycled at the end of their useful life. The over-molding process can be used in highly technical applications such as components for the automotive industry, shells and casings for power tools, parts for domestic appliances, and seals which can be molded directly onto the frame.Information provided by A.P.I. SpA
Physical Properties Metric English Comments
Density 0.970 - 1.05 g/cc
0.0350 - 0.0379 lb/in³
ASTM D 792
Mechanical Properties Metric English Comments
Hardness, Shore A 50 - 80

@Time 15.0 sec
50 - 80

@Time 0.00417 hour
ASTM D 2240
Tensile Strength 3.50 - 7.00 MPa
508 - 1020 psi
ASTM D 638
Elongation at Break 320 - 420 %
320 - 420 %
ASTM D 638
100% Modulus 0.00140 - 0.00400 GPa
0.203 - 0.580 ksi
ASTM D 638
300% Modulus 0.00300 - 0.00600 GPa
0.435 - 0.870 ksi
ASTM D 638
Tear Strength 18.0 - 35.0 kN/m
103 - 200 pli
ASTM D 624
Descriptive Properties Value Comments
Compatibility HIPS
PS
Food contact On Request
Hygroscopicity No
Main Features Easy Processability
Ozone Aging Resistance Excellent
72h, 40°C, 200 ppcm, Tension = 20%
Processing Injection Molding
Weathering Good