Physical Properties Metric English Comments
Density 0.970 - 1.03 g/cc
0.0350 - 0.0372 lb/in³
ASTM D792
Multibase Multi-Flex® TPE A 8502 BLK
The fogging test value is 90% according to ASTM SAE-J275. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase.
Density 1.03 - 1.03 g/cc

@Temperature 270 - 270 °C
0.0372 - 0.0372 lb/in³

@Temperature 518 - 518 °F
Average value: 1.03 g/cc Grade Count:1
Overview of materials for Polycarbonate/PET Polyester Blend
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/PET Polyester Blend". Each property range of values reported is minimum and maximum values..
Density 1.02 - 1.03 g/cc

@Temperature 260 - 260 °C
0.0368 - 0.0372 lb/in³

@Temperature 500 - 500 °F
Average value: 1.02 g/cc Grade Count:15
Overview of materials for Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced". Each property range of values repor..
Density 1.03 - 1.03 g/cc

@Temperature 290 - 290 °C
0.0372 - 0.0372 lb/in³

@Temperature 554 - 554 °F
Average value: 1.03 g/cc Grade Count:1
Overview of materials for Nylon 66, Unreinforced, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Unreinforced, Flame Retardant". Each property range of values reported is minimum and maximum ..
Density 1.03 - 1.03 g/cc

@Temperature 295 - 295 °C
0.0372 - 0.0372 lb/in³

@Temperature 563 - 563 °F
Average value: 1.03 g/cc Grade Count:1
Overview of materials for Nylon 66, 10% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 10% Glass Fiber Filled". Specific grades with glass content between 5% and 14% are included. ..
Density 0.971 - 1.03 g/cc
0.0351 - 0.0372 lb/in³
Lord Adhesives 521 Medium Viscosity, Slow Cure Acrylic Adhesive
Lord 500 SeriesLord 500 Series Acrylic Adhesives bond plastics and prepared metals; they offer excellent adhesion to both thermoplastics and thermoset plastics. They are available with varying handi..
Density 0.990 - 1.03 g/cc
0.0358 - 0.0372 lb/in³
AV15
Solvay Duraphos Octyl Acid Phosphate Surfactant
Identification: DI(N-OCTYL) PHOSPHORIC ACID, N-OCTYL PHOSPHORIC ACID, PHOSPHORIC ACID CAS: 3115-39-7; 3991-73-9; 7664-38-2Solublility: Soluble in common organic solvents and slightly soluble in wate..
Density 0.990 - 1.03 g/cc
0.0358 - 0.0372 lb/in³
RP-17617
Solvay RHODOLINE® DF-988 Surfactant
Description: Silicone free and mineral oil free defoamer for high gloss paints.Identification: DEFOAMERAvailable in: North AmericaApplications: RHODOLINE© DF-988 is a silicone-free, mineral oil-f..
Density 1.00 - 1.03 g/cc
0.0361 - 0.0372 lb/in³
RP-0549
Solvay RHODISOLV® INFINITY Solvent
Description: Rhodiasolv INFINITY is a blend of dibasic ester solvent and proprietary surfactantsChemical Name: Microemulsion concentrate based on dimethyl-2-methyl glutarateSolubility in water: 100%..