Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 4.50 g/cc | 0.163 lb/in³ | |
Kobe Steel KS100 Commercially Pure Titanium, Annealed Nominal Composition: Ti-Fe-OApplications: Wrist watches, cutlery, golf club heads.Features: Scratch resistant, easy to polish, high strength. Information provided by Kobe Steel |
|||
Density | 4.50 g/cc | 0.163 lb/in³ | |
Kobe Steel KS120SI Titanium alloy with low alloying elements, Annealed Nominal Composition: Ti-Fe-O-Si Applications: Wrist watches, cutlery, golf club heads.Features: Scratch resistant, easy to polish, high strength. Information provided by Kobe Steel |
|||
Density | 4.50 g/cc | 0.163 lb/in³ | |
Kobe Steel KS40 Commercially Pure Titanium, ASTM Gr. 1, Annealed Nominal Composition: Ti-Fe-OApplications: PHE, press formed parts, roofs, walls Features: Excellent formability, Excellent corrosion resistanceInformation provided by Kobe Steel |
|||
Density | 4.50 g/cc | 0.163 lb/in³ | |
Kobe Steel KS40PDA Titanium alloy with low alloying elements, ASTM Gr. 11, Annealed Nominal Composition: Ti-0.15 Pd Applications: Condenser tubes, heat transfer tubes, piping, linings, electrolysis vessels, chemical use.Features: Super corrosion resistant. Information provided by .. |
|||
Density | 4.50 g/cc | 0.163 lb/in³ | |
Kobe Steel KS40S Commercially Pure Titanium, ASTM Gr. 1, Annealed Nominal Composition: Ti-Fe-OApplications: PHE, press formed parts, roofs, walls Features: Excellent formability, Excellent corrosion resistanceInformation provided by Kobe Steel |
|||
Density | 4.50 g/cc | 0.163 lb/in³ | |
Kobe Steel KS60AKOT Titanium alloy with low alloying elements, ASTM Gr. 33, Annealed Nominal Composition: Ti-0.4 Ni-0.015 Pd-0.025 Ru-0.14 Cr Applications: Condenser tubes, heat transfer tubes, piping, linings, electrolysis vessels, chemical use.Features: Super corrosion resistant... |
|||
Density | 4.50 g/cc | 0.163 lb/in³ | |
Kobe Steel KS70 Commercially Pure Titanium, ASTM Gr. 3, Annealed Nominal Composition: Ti-Fe-OApplications: Tube sheets.Features: Relatively high strength, excellent corrosion resistance.Information provided by Kobe Steel |
|||
Density | 4.50 g/cc | 0.163 lb/in³ | |
Kobe Steel Titanium alloy with low alloying elements, ASTM Gr. 7, Annealed Nominal Composition: Ti-0.15 Pd Applications: Condenser tubes, heat transfer tubes, piping, linings, electrolysis vessels, chemical use.Features: Super corrosion resistant. Information provided by .. |
|||
Density | 4.50 g/cc | 0.163 lb/in³ | |
LATI Latamid 12 H 90FE03 PA 12, Heat Stabilized Polyamide 12 (PA12) based compound. Heat stabilized. Magnetizable filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria.. |
|||
Density | 4.50 g/cc | 0.163 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP TH0450C PU LNP* Thermocomp* TH0450C is a compound based on Polyurethane resin containing High Specific Gravity Filler. Added features of this material include: High Specific Gravity. |
|||
Density | 4.50 g/cc | 0.163 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP THERMOCOMP TH0450C PU LNP* Thermocomp* TH0450C is a compound based on Polyurethane resin containing High Specific Gravity Filler. Added features of this material include: High Specific Gravity. |
|||
Density | 4.50 g/cc | 0.163 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP TH0450C PUR (Asia Pacific) LNP* Thermocomp* TH0450C is a compound based on Polyurethane resin containing High Specific Gravity Filler. Added features of this material include: High Specific Gravity. |
|||
Density | 4.50 g/cc | 0.163 lb/in³ | ASTM D 792 |
SABIC Innovative Plastics LNP Thermocomp TH0450D LNP* Thermocomp* TH0450D is a compound based on Polyurethane resin containing High Specific Gravity Filler. Added features of this material include: High Specific Gravity.This data was supplied by .. |
|||
Density | 4.50 g/cc | 0.163 lb/in³ | ASTM D 792 |
SABIC Innovative Plastics LNP Thermocomp TH0450D PUR (Asia Pacific) LNP* Thermocomp* TH0450D is a compound based on Polyurethane resin containing High Specific Gravity Filler. Added features of this material include: High Specific Gravity.This data was supplied by .. |
|||
Density | 4.50 g/cc | 0.163 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP THERMOCOMP WH0450E PBT LNP* Thermocomp* WH0450E is a compound based on Polybutylene Terephalate resin containing High Specific Gravity Filler. Added features of this material include: High Specific Gravity. |
|||
Density | 4.50 g/cc | 0.163 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP WH0450EX PBT (Asia Pacific) LNP* Thermocomp* WH0450EX is a compound based on Polybutylene Terephalate resin containing High Specific Gravity Filler. Added features of this material include: High Specific Gravity. |
|||
Density | 4.50 g/cc | 0.163 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP WH0450E PBT (Asia Pacific) LNP* Thermocomp* WH0450E is a compound based on Polybutylene Terephalate resin containing High Specific Gravity Filler. Added features of this material include: High Specific Gravity. |
|||
Density | 4.50 g/cc | 0.163 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP THERMOCOMP WH0450E PBT (Asia Pacific) LNP* Thermocomp* WH0450E is a compound based on Polybutylene Terephalate resin containing High Specific Gravity Filler. Added features of this material include: High Specific Gravity. |
|||
Density | 4.50 g/cc | 0.163 lb/in³ | Typical |
TIMET TIMETAL® 1100 Titanium Alloy (Ti-6Al-2.7Sn-4Zr-0.4Mo-0.45Si) Features: A near alpha, high temperature creep resistant alloy developed for elevated temperature use in the range of 600°C that offers the highest combination of strength, creep resistance, fractu.. |
|||
Density | 4.50 g/cc | 0.163 lb/in³ | |
BASF Sicotan® Red L 2817 Color Additive Description: Transparent red iron oxideChemical Structure: Iron-III-OxideSuitable for: Baking System, Waterborn systems, Acrylic-isocyanate systems, Acid curing system, Amine curing system and Airdr.. |
|||
Density | 4.50 g/cc | 0.163 lb/in³ | |
BASF Sicotan® Red L 2818 Color Additive Description: Transparent red iron oxideChemical Structure: Iron-III-OxideSuitable for: Baking System, Waterborn systems, Acrylic-isocyanate systems, Acid curing system, Amine curing system and Airdr.. |
|||
Density | 4.50 g/cc | 0.163 lb/in³ | |
BASF Sicotan® Yellow K 1010 Color Additive Chemical Structure: Ni/Sb/Ti-oxideApplication: Colourant for plastics; PVC-p, PVC-u, LD-PE, HD-PE, PP, PS, SB, SAN, ABS/ASA, PMMA, PC, PA, PETP, CA/CAB and UPRecommendations for food applications: B.. |
|||
Density | 4.50 g/cc | 0.163 lb/in³ | |
BASF Sicotan® Yellow K 2011 Color Additive Chemical Structure: Cr/Sb/Ti-oxideApplication: Colourant for plastics; PVC-p, PVC-u, LD-PE, HD-PE, PP, PS, SB, SAN, ABS/ASA, PMMA, PC, PA, PETP, CA/CAB and UPRecommendations for food applications: B.. |
|||
Density | 4.50 g/cc | 0.163 lb/in³ | |
BASF Sicotan® Yellow L 1910 Color Additive Description: Mixed-phase pigment with maximum fastness properties. Suitable for all coatings systemsChemical Structure: Cr/Sb/Ti-OxideSuitable for: Baking System, Waterborn systems, Acrylic-isocyana.. |
|||
Density | 4.50 g/cc | 0.163 lb/in³ | |
BASF Sicotan® Yellow L 1912 Color Additive Description: Mixed-phase pigment with maximum fastness properties. Suitable for all coatings systemsChemical Structure: Cr/Sb/Ti-OxideSuitable for: Baking System, Waterborn systems, Acrylic-isocyana.. |
|||
Density | 4.50 - 5.50 g/cc | 0.163 - 0.199 lb/in³ | |
Alliance BIN-26 Bonded (Composite) Magnetic Material |
|||
Density | 4.50 - 5.50 g/cc | 0.163 - 0.199 lb/in³ | |
Alliance BIN-45 Bonded (Composite) Magnetic Material |
|||
Density | 4.50 - 5.50 g/cc | 0.163 - 0.199 lb/in³ | |
Alliance BIN-48 Bonded (Composite) Magnetic Material |
|||
Density | 4.50 - 5.50 g/cc | 0.163 - 0.199 lb/in³ | |
Alliance BIN-72 Bonded (Composite) Magnetic Material |
|||
Density | 4.50 g/cc | 0.163 lb/in³ | |
BASF Sicopal® Blue K 6310 Color Additive Chemical Structure: Co/Al-oxideApplication: Colourant for plastics; PVC-p, PVC-u, PUR, LD-PE, HD-PE, PP, PS, SB, SAN, ABS/ASA, PMMA, PC, PA PETP, CA/CAB and UPRecommendations for food applications: .. |