| Category | Ceramic , Metal , Electronic/Magnetic Alloy | 
| Manufacturer | Alliance LLC | 
| Trade Name | |
| Port | Shanghai port,China | 
| Trade Terms | FOB, CFR, CIF | 
| Payment Terms | L/C, T/T, Western Union | 
| Download PDF | Alliance BIN-26 Bonded (Composite) Magnetic Material.pdf  | 
          
| Price | EMAIL US sales@lookpolymers.com | 
| Physical Properties | Metric | English | Comments | 
|---|---|---|---|
| Density | 4.50 - 5.50 g/cc | 0.163 - 0.199 lb/in³ | 
| Mechanical Properties | Metric | English | Comments | 
|---|---|---|---|
| Tensile Strength, Ultimate | 25.0 - 40.0 MPa | 3630 - 5800 psi | |
| Flexural Strength | 60.0 - 80.0 MPa | 8700 - 11600 psi | 
| Thermal Properties | Metric | English | Comments | 
|---|---|---|---|
| CTE, linear |           60.0 - 80.0           µm/m-°C           @Temperature 20.0 °C  | 
                  33.3 - 44.4           µin/in-°F           @Temperature 68.0 °F  | 
        Parallel DOM | 
| Maximum Service Temperature, Air | 100 °C | 212 °F | 
| Electrical Properties | Metric | English | Comments | 
|---|---|---|---|
| Electrical Resistivity | 0.00400 - 0.00700 ohm-cm | 0.00400 - 0.00700 ohm-cm | |
| Magnetic Coercive Force, Hc | 3500 Oe | 3500 Oe | |
| 8480 Oe | 8480 Oe | Intrinsic | |
| Magnetic Remanence, Br | 4000 Gauss | 4000 Gauss | |
| Magnetic Maximum Energy Product, BH | 3.6 MGOe | 3.6 MGOe | |
| Curie Temperature | 300 - 470 °C | 572 - 878 °F | 
| Descriptive Properties | Value | Comments | 
|---|---|---|
| Reversible Temp Coef., Bd | -0.105 %/°C | |
| Reversible Temp Coef., Hd | -0.40 %/°C | |
| Temperature Coefficient, Br | -0.1 %/°C | (20-100°C) | 
| Temperature Coefficient, Hci | -0.4 %/°C | (20-100°C) |