Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 2.66 - 2.94 g/cc | 0.0961 - 0.106 lb/in³ | |
PEAK Werkstoff DISPAL S690 Aluminum Alloy, AlCu4MgAg, Condition T4 High stiffness and elongation at rupture. Property data for Condition T4 (Quench in water at RT).Information provided by PEAK Werkstoff GmbH |
|||
Density | 2.66 - 2.94 g/cc | 0.0961 - 0.106 lb/in³ | |
PEAK Werkstoff DISPAL S690 Aluminum Alloy, AlCu4MgAg, Condition T6 High stiffness and elongation at rupture. Property data for Condition T6 (Quench in water at RT).Information provided by PEAK Werkstoff GmbH |
|||
Density | 2.66 g/cc | 0.0961 lb/in³ | |
Lucas-Milhaupt AL 718 Aluminum Brazing Filler Metal Applications:AL 718 filler metal is generally used to join aluminum and aluminum alloys. It can be used to join titanium or aluminum to dissimilar metals. When joining to dissimilar metals thought.. |
|||
Density | 2.66 g/cc | 0.0961 lb/in³ | |
Schott BG4 Band Pass Filter Ionically colored glass. Data provided by the manufacturer, Schott Glas Mainz. |
|||
Density | 2.66 g/cc @Temperature 25.0 °C |
0.0961 lb/in³ @Temperature 77.0 °F |
|
Schott Glass 8360 Lead-Free Soft Glass Soft glass, lead-free Encapsulation of semiconductor components at low temperature (diodes) The heavy metal content for the elements lead, mercury, cadmium, and hexavalent chromium is less than 10.. |
|||
Density | 2.66 g/cc | 0.0961 lb/in³ | ASTM D792 |
Techmer ES HiFill® PA6 0266 B Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/ReinforFeatures: High Specific GravityInformation provided by TP Composites, Inc. |
|||
Density | 2.66 g/cc | 0.0961 lb/in³ | ASTM D792 |
Techmer ES HiFill® TPU 0266 A Availability: North AmericaForms: PelletsFeatures: High Density and High Specific GravityInformation provided by TP Composites, Inc. |
|||
Density | 2.66 g/cc | 0.0960 lb/in³ | |
PCP-Canada ALCA 5® 5083 Cast Aluminum Mold Plate ALCA5® cast precision plate product has an excellent dimensional stability. The low level of internal stress reduces the plate deformation during and after machining. This high stability leads to c.. |
|||
Density | 2.66 g/cc | 0.0960 lb/in³ | |
Vista Metals ATP-5™ Precision Cast Aluminum Plate Used where flatness and dimensional control are critical, such as: computer & electronics, pharmaceuticals, medical testing equipment, packaging machinery, printing machinery, thermoforming tools, m.. |
|||
Density | 2.66 g/cc | 0.0960 lb/in³ | |
Vista Metals Duramold-5™ Cast Aluminum Mold Plate Used for molds for the automotive industry, blow molds, structural foam molds, rubber molds, low pressure injection molds, Thermoforming molds, R.I.M. and R.T.M. molding.Features: Excellent Machinab.. |
|||
Density | 2.66 g/cc | 0.0961 lb/in³ | |
Constellium Alumold® 110 Aluminum Cast Sliced Plate Alumold®-110 has been specifically developed for low–pressure processing (thermoforming, RTM) of plastics and their composites. The material can also be used for prototype injection moulds. The ma.. |
|||
Density | 2.66 g/cc | 0.0961 lb/in³ | |
Constellium Fibral® Cast Aluminum Sliced Plate Fibral® has been specifically developed for low–pressure processing (thermoforming, RTM) of plastics and their composites. The material can also be used for prototype injection moulds. The materia.. |
|||
Density | 2.66 g/cc | 0.0961 lb/in³ | |
Constellium PLAN 5083 Aluminum Rolled Plate Rolled plates in 5083 PLAN are optimized for minimum residual stress and improved dimensional tolerances. 5083 PLAN is mainly used for low stressed mechanical components, manufactured by intensive m.. |
|||
Density | 2.66 g/cc | 0.0961 lb/in³ | |
Constellium Planoxal® 50 Aluminum plate Planoxal®-50 plates differ from other standard EN-AW 5083 alloy products by their low level of residual stress. This specialty plate is also suitable for decorative anodizing. Planoxal®-50 is main.. |
|||
Density | 2.66 g/cc | 0.0961 lb/in³ | |
Constellium ALPLAN® 5083 Rolled Precision Aluminum Plate, Milled Both Sides ALPLAN® 5083 precision plates exhibit good dimensional stability. Their low internal stresses reduces the effects of plate deformation during machining, thus saving on extra operations such as roug.. |
|||
Density | 2.66 g/cc | 0.0961 lb/in³ | Aluminum 5083 |
Aleris Alustar Aluminum Alloy, H321/H116; 2 - 20 mm thickness At least 20% stronger than AA 5083 before and after welding. Bendability and weldability similar to AA 5083. High corrosion resistance. Provides options for ship design and building.Composition d.. |
|||
Density | 2.66 g/cc | 0.0961 lb/in³ | Aluminum 5083 |
Aleris Alustar Aluminum Alloy, MIG-welded At least 20% stronger than AA 5083 before and after welding. Bendability and weldability similar to AA 5083. High corrosion resistance. Provides options for ship design and building.Composition d.. |
|||
Density | 2.66 g/cc | 0.0961 lb/in³ | Aluminum 5083 |
Aleris Alustar H131 Aluminum Alloy Close in composition to AA5059. Used in defense and mining shielding applications for protection against ballistics and blasts. |
|||
Density | 2.66 g/cc | 0.0960 lb/in³ | |
Alpase K100-S™ Aluminum Plate K100-S™ features and benefits include: Dimensional stability, fully weldable, anodizable, high elongation, consistent properties - regardless of size, close flatness and tolerances, superior corros.. |
|||
Density | 2.66 g/cc | 0.0960 lb/in³ | |
Alpase M-5™ Aluminum Mold Plate Excellent weldabilitySurface Condition - Machined top and bottom to reduce costly handling and machining stepsDimensional Stability - High dimensional stability during and after machiningPolishing -.. |
|||
Density | 2.66 g/cc | 0.0961 lb/in³ | Aluminum 5083 |
Aleris Alustar Aluminum Alloy, H321/H116; 20 - 40 mm thickness At least 20% stronger than AA 5083 before and after welding. Bendability and weldability similar to AA 5083. High corrosion resistance. Provides options for ship design and building.Composition d.. |
|||
Density | 2.66 g/cc | 0.0961 lb/in³ | Aluminum 5083 |
Aleris Alustar Aluminum Alloy, O/H111 At least 20% stronger than AA 5083 before and after welding. Bendability and weldability similar to AA 5083. High corrosion resistance. Provides options for ship design and building.Composition d.. |
|||
Density | 2.66 g/cc | 0.0961 lb/in³ | Aluminum 5083 |
Aleris Alustar H136 Aluminum Alloy Close in composition to AA5059. Used in defense and mining shielding applications for protection against ballistics and blasts. H136 has a higher elongation than H131 and so provides better protec.. |
|||
Density | 2.66 g/cc | 0.0960 lb/in³ | |
ALIMEX 5083 O/H111Aluminum Alloy Rolled Rolled aluminium material according to DIN EN standard. Information provided by ALIMEX GmbHAnnealed and slightly strain-hardened |
|||
Density | 2.66 g/cc | 0.0960 lb/in³ | |
ALIMEX ACP 5080 Aluminum Cast Plate ACP 5080 is a 5xxx series precision aluminum cast plate. Thickness, flatness and surface finish offer very tight tolerances.Material stability and excellent processing characteristics make this alum.. |
|||
Density | 2.66 g/cc | 0.0960 lb/in³ | |
ALIMEX PLANAL 5083 O/H111 Aluminum Alloy Aluminium rolled plates which have been machined on both sides. Has a precise surface finish and high tensile strength. The temper values and the material conditions are not changed by surface-machi.. |
|||
Density | 2.66 g/cc | 0.0961 lb/in³ | AA 5083 |
Aleris HOGAL 5558 Aluminum 5026 H14/H34 HOGAL 5558 is produced according to EN AW-5026.Information provided by Aleris. |
|||
Density | 2.66 g/cc | 0.0960 lb/in³ | |
ALIMEX ACP 5080R Aluminum Cast Material Sizes range availability along with good mechanical and physical properties of ACP 5080R provide the Mold Tool Industry tooling materials solutions for the most challenging applications.Information .. |
|||
Density | 2.66 g/cc | 0.0960 lb/in³ | |
PCP-Canada Max 5® 5083 Cast Aluminum Mold Block Max 5® is characterized by an excellent dimensional stability. It is a 5083 alloy which provides strength, good hard anodizing response, weldability, and machinability (with sintered carbide materi.. |
|||
Density | 2.66 g/cc | 0.0961 lb/in³ | |
Indium Corp. Indalloy 188 Aluminum Solder Alloy Information Provided by Indium Corporation |