| Category | Ceramic , Glass , Filter , Optical |
| Manufacturer | Schott Glas Mainz |
| Trade Name | |
| Port | Ningbo port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | Schott BG4 Band Pass Filter.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 2.66 g/cc | 0.0961 lb/in³ |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 7.70 µm/m-°C @Temperature -30.0 - 70.0 °C |
4.28 µin/in-°F @Temperature -22.0 - 158 °F |
|
| 9.00 µm/m-°C @Temperature 20.0 - 300 °C |
5.00 µin/in-°F @Temperature 68.0 - 572 °F |
||
| Transformation Temperature, Tg | 536 °C | 997 °F |
| Optical Properties | Metric | English | Comments |
|---|---|---|---|
| Refractive Index | 1.52 @Wavelength 1014 nm |
1.52 @Wavelength 1014 nm |
Hg |
| 1.53 @Wavelength 587.6 nm |
1.53 @Wavelength 587.6 nm |
He | |
| 1.54 @Wavelength 435.8 nm |
1.54 @Wavelength 435.8 nm |
Hg | |
| 1.57 @Wavelength 302.1 nm |
1.57 @Wavelength 302.1 nm |
Hg | |
| Transmission, Visible | <= 1.0 % @Wavelength 490 - 690 nm |
<= 1.0 % @Wavelength 490 - 690 nm |
|
| 87 % @Wavelength 400 nm |
87 % @Wavelength 400 nm |
Internal transmittance of 95% at 400 nm | |
| IR Transmittance | 91 % @Wavelength 760 - 800 nm |
91 % @Wavelength 760 - 800 nm |
Internal transmittance of 99% from 760-800 nm. |
| UV Transmittance | <= 0.020 % @Wavelength 200 - 270 nm |
<= 0.020 % @Wavelength 200 - 270 nm |
|
| 91 % @Wavelength 340 - 380 nm |
91 % @Wavelength 340 - 380 nm |
Internal transmittance of 99% from 340-380 nm | |
| Reflection Coefficient, Visible (0-1) | 0.92 | 0.92 |
| Chemical Properties | Metric | English | Comments |
|---|---|---|---|
| Acid Class, SR | 1 | 1 | |
| Alkali Class, AR | 1 | 1 | |
| Stain Resistance Class, FR | 0.0 | 0.0 |