Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Schott Glass 8360 Lead-Free Soft Glass

Category Ceramic , Glass
Manufacturer Schott North America
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Schott Glass 8360 Lead-Free Soft Glass.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Soft glass, lead-free Encapsulation of semiconductor components at low temperature (diodes) The heavy metal content for the elements lead, mercury, cadmium, and hexavalent chromium is less than 100 ppmInformation provided by SCHOTT AG.
Physical Properties Metric English Comments
Density 2.66 g/cc

@Temperature 25.0 °C
0.0961 lb/in³

@Temperature 77.0 °F
Mechanical Properties Metric English Comments
Modulus of Elasticity 85.0 GPa
12300 ksi
Poissons Ratio 0.24
0.24
Thermal Properties Metric English Comments
CTE, linear 9.10 µm/m-°C

@Temperature 20.0 - 300 °C
5.06 µin/in-°F

@Temperature 68.0 - 572 °F
ISO 7991
Transformation Temperature, Tg 465 °C
869 °F
ISO 7884-8
Softening Point 575 °C
1070 °F
Viscosity 10<sup>7.6</sup> dPa s; ISO 7884-3
Working Point 745 °C
1370 °F
Viscosity 10<sup>4</sup> dPa s; ISO 7884-2
Annealing Point 470 °C
878 °F
Viscosity 10<sup>13</sup> dPa s; ISO 7884-4
Optical Properties Metric English Comments
Refractive Index 1.566

@Wavelength 587.6 nm
1.566

@Wavelength 587.6 nm
Electrical Properties Metric English Comments
Volume Resistivity 5.00e+6 ohm-cm

@Temperature 350 °C
5.00e+6 ohm-cm

@Temperature 662 °F
3.20e+8 ohm-cm

@Temperature 250 °C
3.20e+8 ohm-cm

@Temperature 482 °F
Dielectric Constant 7.3

@Frequency 1.00e+6 Hz,
Temperature 25.0 °C
7.3

@Frequency 1.00e+6 Hz,
Temperature 77.0 °F
Dielectric Loss Index 0.0024

@Frequency 1.00e+6 Hz,
Temperature 25.0 °C
0.0024

@Frequency 1.00e+6 Hz,
Temperature 77.0 °F
Chemical Properties Metric English Comments
Acid Class, SR 4
4
DIN 12116
Alkali Class, AR 3
3
ISO 695
Descriptive Properties Value Comments
Hydrolytic Resistance Class HGB 3
ISO 719
Stress-optical Coefficient K (10-6mm2N-1) 2.9
DIN 52314
tk100(°C) 275