Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 2.20 g/cc | 0.0795 lb/in³ | Green |
Nabaltec NABALOX® NO 613-10 Reactive Alumina NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula.. |
|||
Density | 2.20 g/cc | 0.0795 lb/in³ | ASTM D792 |
Rogers Corporation RT/duroid® 6035HTC Ceramic Filled PTFE Composite, High Power RF and Microwave Features & Benefits:High thermal conductivity - Improved dielectric heat dissipation, enabling lower operating temperatures for high power applicationsLow loss tangent - Excellent high frequency per.. |
|||
Density | 2.20 g/cc | 0.0795 lb/in³ | ISO 1183 |
LNP Konduit® OTF-212-11 Polyphenylene Sulfide, Proprietary Filler
(discontinued **) Features: Thermally ConductiveForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades ar.. |
|||
Density | 2.20 g/cc | 0.0795 lb/in³ | ASTM D4894 |
3M Dyneon™ CC603 PTFE, 15% Fiberglass Filled
(discontinued **) Product Form: White, pelletized free-flowing powder. Applications include bearings, valve seats, seals.Data provided by Dyneon. |
|||
Density | 2.20 g/cc | 0.0795 lb/in³ | |
Ferro IX 2693 Dental Glass Glass Type: Fused Silica Typical Application: Low Expansion Filler Ferro's Dental Glasses are standard x-ray opaque glass powders and inorganic fillers for use in dental restorations. Ferro also m.. |
|||
Density | 2.20 g/cc | 0.0795 lb/in³ | Apparent |
Gouda Vuurvast B Sp Dense Refractory Brick Description: A very dense brick, high resistance against slag penetration. Application: in rotary kilns (cement) and incinerators.Remarks: This data represents average values, obtained from samples .. |
|||
Density | 2.20 g/cc | 0.0795 lb/in³ | |
Mo-Sci Corporation GL-0179 Borosilicate Glass Spheres Appearance: Solid clear borosilicate glass microspheres with white color in powder form.Typical applications of GL0179 beads include: calibration, high temperature spacer material for gauge control,.. |
|||
Density | 2.20 g/cc | 0.0795 lb/in³ | |
Mo-Sci Corporation GL-0201 Silica Glass Spheres Appearance: Solid clear amorphous silica microspheres with white color in powder form.Typical applications of GL0201 beads include: calibration, high temperature spacer material for gauge control, c.. |
|||
Density | 2.20 - 2.30 g/cc | 0.0795 - 0.0831 lb/in³ | |
Mo-Sci Corporation GL-0261 Ni Coated Borosilicate Glass Spheres Appearance: Solid borosilicate glass microspheres with metallic nickel coatingTypical applications of GL-0261 glass microspheres include: conductive filler for plastic, pigment, and etc.Information .. |
|||
Density | 2.20 - 2.30 g/cc | 0.0795 - 0.0831 lb/in³ | |
Mo-Sci Corporation GL-0263 Cu Coated Borosilicate Glass Spheres Appearance: Solid borosilicate glass microspheres with metallic copper coatingTypical applications of GL-0263 glass microspheres include: conductive filler for plastic, pigment, and etc.Information .. |
|||
Density | 2.20 g/cc | 0.0795 lb/in³ | |
Momentive Performance Materials Type 214 Fused Quartz Tubing Used for clear fused quartz lamp tubing. GE 214 is a high purity, high transmittance, high temperature material with a low hydroxyl (OH-) content. It is suitable for a broad range of mercury, halo.. |
|||
Density | 2.20 g/cc | 0.0795 lb/in³ | theoretical |
Gwent Electronic Materials P2121112P1 Acid Vapor Plasma Modified Graphene Nanoplatelets Production Method: Plasma Exfoliation of Natural GraphiteColor: Black/Grey Trial product which has not yet been extensively tested.Information provided by Gwent Electronic Materials Ltd. |
|||
Density | 2.20 g/cc | 0.0795 lb/in³ | theoretical |
Gwent Electronic Materials P2121112P2 Argon Plasma Modified Graphene Nanoplatelets Production Method: Plasma Exfoliation of Natural GraphiteColor: Black/Grey Trial product which has not yet been extensively tested.Information provided by Gwent Electronic Materials Ltd. |
|||
Density | 2.20 g/cc | 0.0795 lb/in³ | theoretical |
Gwent Electronic Materials P2121112P4 Nitrogen Plasma Modified Graphene Nanoplatelets Production Method: Plasma Exfoliation of Natural GraphiteColor: Black/Grey Trial product which has not yet been extensively tested.Information provided by Gwent Electronic Materials Ltd. |
|||
Density | 2.20 g/cc | 0.0795 lb/in³ | theoretical |
Gwent Electronic Materials P2121112P5 Ammonia Plasma Modified Graphene Nanoplatelets Production Method: Plasma Exfoliation of Natural GraphiteColor: Black/Grey Trial product which has not yet been extensively tested.Information provided by Gwent Electronic Materials Ltd. |
|||
Density | 2.20 - 2.60 g/cc | 0.0795 - 0.0939 lb/in³ | ASTM B212 |
H.C. Starck Amperit® 827.054 Zirconium Oxide-Yttrium Oxide 93-7 (ZrO2-Y2O3) |
|||
Density | 2.20 - 2.40 g/cc | 0.0795 - 0.0867 lb/in³ | ASTM B212 |
H.C. Starck Amperit® 827.6 Zirconium Oxide-Yttrium Oxide 93-7 (ZrO2-Y2O3) |
|||
Density | 2.20 - 2.60 g/cc | 0.0795 - 0.0939 lb/in³ | ASTM B212 |
H.C. Starck Amperit® 832.054 Zirconium Oxide-Yttrium Oxide 93-7 (ZrO2-Y2O3) |
|||
Density | 2.20 - 2.60 g/cc | 0.0795 - 0.0939 lb/in³ | ASTM B212 |
H.C. Starck Amperit® 832.7 Zirconium Oxide-Yttrium Oxide 93-7 (ZrO2-Y2O3) |
|||
Density | 2.20 g/cc | 0.0795 lb/in³ | |
Momentive Performance Materials Pyrolytic Graphite (PG) Coating PG is a popular coating for sealing machined graphite hardware which does not require oxidation protection. It is the most anisotropic commercially available material and is therefore useful where .. |
|||
Density | 2.20 - 2.60 g/cc | 0.0795 - 0.0939 lb/in³ | ASTM B212 |
H.C. Starck Amperit® 832.6 Zirconium Oxide-Yttrium Oxide 93-7 (ZrO2-Y2O3) |
|||
Density | 2.20 g/cc | 0.0795 lb/in³ | |
Schott LITHOSIL-Q Glass Information Provided by SCHOTT North America, Inc. |
|||
Density | 2.20 g/cc | 0.0795 lb/in³ | |
SGL Carbon Group EK 3245 Carbon Graphite Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and.. |
|||
Density | 2.20 g/cc | 0.0795 lb/in³ | |
Trelleborg Emerson & Cuming Stycast® 4952/25 Two-Component Silicone High Service Temp Encapsulant Features and Typical ApplicationsAbility to withstand high temperatures, thermal shock, and chemical exposure. These products are designed for heat generating electronic devices which operate in har.. |
|||
Density | 2.20 g/cc | 0.0795 lb/in³ | DIN 53479 |
Polyram RamOfin PPC371B73 Polypropylene, 73% Mineral Filled 73% mineral filled polypropylene for heavy density injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Density | 2.20 g/cc | 0.0795 lb/in³ | Cured |
Chesterton ARC BX1 Sliding Wear Compound Description: An advanced contractor grade ceramic composite for the repair and protection of all metal surfaces subjected to severe erosion, corrosion, and chemical attack. It is normally applied at.. |
|||
Density | 2.20 g/cc | 0.0795 lb/in³ | Cured |
Chesterton ARC BX2 Contractor Grade Fine Sliding Wear Compound Description: ARC BX2 is an advanced contractor grade ceramic reinforced composite for the repair and protection of all metal surfaces subjected to severe erosion, corrosion, and chemical attack. It .. |
|||
Density | 2.20 g/cc | 0.0795 lb/in³ | |
Corning Vycor® 7907 UV-Blocking Glass Vycor-UV™ is cerium-doped and provides homogeneous absorption of UV-B and UV-C.Special Features:Superior optical qualityTight dimensional controlThermal and chemical properties ideally suited to hi.. |
|||
Density | 2.20 g/cc | 0.0795 lb/in³ | |
Anderman Ceramics EC90P Mullite-Bonded Porous Silicon Carbide (90%) Excellent thermal shock properties and thermal conductivity when in contact with molten metal. Available as tube, sheath, or rod up to 6 ft (1.9 m) long with diameters 0.6" to 3.75".Information pro.. |
|||
Density | 2.20 g/cc | 0.0795 lb/in³ | ISO 1183 |
LNP Konduit® OTF-212-11 BK8-115 Polyphenylene Sulfide, Proprietary Filler
(discontinued **) Features: Thermally ConductiveForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades ar.. |