Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.76 g/cc | 0.0636 lb/in³ | |
Park Electrochemical Nelcote® S-860 Silicone Prepreg, 1581-112NPH E-Glass Reinforced Nelcote® S-860 is a MIL-P-25518 type silicone resin with a good combination of electrical and high temperature properties. GMS4001 qualified specificationsKey Features and Benefits:500°F maximum s.. |
|||
Density | 1.76 g/cc | 0.0636 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP KONDUIT OX11315 PPS (Asia Pacific) Thermally conductive electrically insulative mineral filled PPS FR compound. |
|||
Density | 1.76 g/cc | 0.0636 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP KONDUIT PX11311 PA 6 (Europe-Africa-Middle East) Thermally conductive mineral and glass fiber filled PA6 Eco-FR compound |
|||
Density | 1.76 g/cc | 0.0636 lb/in³ | ISO 1183 |
Solvay Specialty Polymers Solef® 31008 PVDF Copolymer
(discontinued **) Key features of this grade: High Flexibility/ High Elongation/Cold Impact Resistance, Wire & Cable, Plenum, Formulated. Recommended processing is extrusion. Available as powder & granules.General .. |
|||
Density | 1.76 g/cc | 0.0637 lb/in³ | |
Garlock 5507 Compressed Inorganic Fiber Gasketing, EPDM Binder Inorganic fibers with an EPDM binder.Inorganic fiber gasketing offers excellent thermal stability with minimal weight lossReduced creep relaxation and improved torque retention provide optimal seala.. |
|||
Density | 1.76 g/cc | 0.0637 lb/in³ | |
Garlock 9900 Compressed Graphite Fiber Gasketing, Nitrile Binder Graphite fibers with a nitrile binder.Graphite fiber gasketing withstands extreme temperatures and pressures, as well as many chemicalsPassed Garlock Fire tests, and is ABS Fire Safe Type ApprovedLo.. |
|||
Density | 1.76 g/cc | 0.0636 lb/in³ | |
LATI Laticonther 62 GR/70 PA 6, 70% Graphite Reinforced High thermal conductivity product based on Polyamide 6 (PA6). Graphite.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Te.. |
|||
Density | 1.76 g/cc | 0.0636 lb/in³ | Relative Density; ASTM D792 |
Sumitomo Bakelite North America RX® 3-2-530-P Long-Glass Reinforced Diallyl Phthalate Long glass fiber reinforced, flame retardant, diallyl meta-phthalate molding compound which meets the requirements of ASTM D5948 Type GII-30F.Information provided by Vyncolit, a Sumitomo Bak Group |
|||
Density | 1.76 g/cc | 0.0636 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP Thermocomp 5C003 LNP THERMOCOMP* 5C003 is a compound based on Polyvinylidene Fluoride resin containing Carbon Fiber. Added features of this material include: Electrically Conductive. Also known as THERMOCOMP* FP-VC.. |
|||
Density | 1.76 g/cc | 0.0636 lb/in³ | ASTM D792 |
Techmer ES HiFill® TPX-HTN-02028 A 60% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 60% Filler by WeightAdditive: Heat StabilizerFeatures: Heat Stabilized and High Temperature StrengthInformat.. |
|||
Density | 1.76 g/cc | 0.0636 lb/in³ | |
UCAR Carbon UCAR® ATJ Isostatic Molded Graphite Isostatically molded ATJ has been an industry standard for many years. It is a fine grain, high strength material which can be machined to precise tolerances and a fine surface finish. Grade ATJ has.. |
|||
Density | 1.76 g/cc | 0.0636 lb/in³ | |
UCAR Carbon UCAR® CHV Extruded Graphite Typical uses for extruded grades are in the production of molds and crucibles, heating elements and furnace furniture, liquid metal processing equipment and chemical process equipment.Tabular proper.. |
|||
Density | 1.76 g/cc | 0.0636 lb/in³ | |
Cosmic Plastics K31 Short Glass Fiber Filled Iso Diallyl Phthalate Molding Compound Data provided by the manufacturer. |
|||
Density | 1.76 g/cc | 0.0636 lb/in³ | ASTM D792 |
Plenco 6401 Phenolic, Briquette, Transfer Molded PLENCO 06401 is a glass fiber and mineral filled two-stage phenolic molding compound. UL recognized under component file E40654. 06401 is available in black.Information supplied by Plenco. |
|||
Density | 1.76 g/cc | 0.0636 lb/in³ | |
Toho Tenax Besfight® G30-500 12K HTA-7C EP01 Continuous Filament Carbon Fiber Standard Modulus; Collimated; Polyacrylonitrile (PAN) based fiberTypical values; measured by Toho Strand Test Method based on JIS R7601 for fiber selection purposes. Information provided by Toho Car.. |
|||
Density | 1.76 g/cc | 0.0636 lb/in³ | (DAM); ISO 1183 |
DSM Stanyl® TW241F12 (COND) Nylon 46 60% Glass Reinforced, Heat Stabilized, High Flow (North America) Information provided by DSM Engineering Plastics. |
|||
Density | 1.76 g/cc | 0.0636 lb/in³ | ISO 1183 |
DSM Stanyl® TW241F12 (DAM) Nylon 46 60% Glass Reinforced, Heat Stabilized, High Flow (North America) Information provided by DSM Engineering Plastics. |
|||
Density | 1.76 g/cc | 0.0636 lb/in³ | (DAM); ISO 1183 |
DSM Stanyl® TW241F12 Nylon 46-60% Glass Reinforced (European and Asian Grade) (Cond) Stanyl is a high performance polyamide providing unmatched performance and value across an amazingly broad range of automotive and electronic applications. Stanyl offers:Highest mechanical propertie.. |
|||
Density | 1.76 g/cc | 0.0636 lb/in³ | ISO 1183 |
DSM Stanyl® TW241F12 Nylon 46-60% Glass Reinforced (European and Asian Grade) (Dry) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Density | 1.76 g/cc | 0.0636 lb/in³ | |
Cytec Thornel® T-300 3K Carbon Fiber, Polyacrylonitrile (PAN) Precursor Data provided by the manufacturer, Amoco Performance Products, Inc.Continuous length, high strength, high modulus fiber made from a polyacrylonitrile precursor. The fiber surface has been treated t.. |
|||
Density | 1.76 g/cc | 0.0636 lb/in³ | |
Cytec Thornel® T-300 6K Carbon Fiber, Polyacrylonitrile (PAN) Precursor Data provided by the manufacturer, Amoco Performance Products, Inc.Continuous length, high strength, high modulus fiber made from a polyacrylonitrile precursor. The fiber surface has been treated t.. |
|||
Density | 1.76 g/cc | 0.0636 lb/in³ | DAM; ISO 1183 |
DuPont Performance Polymers Zytel® HTN FR52G45BL BK337 Polyphthalamide (PPA)
(Unverified Data**) 45% Glass Reinforced Flame Retardant PPA High Performance Polyamide Zytel HTNFR52G45BL BK337 is a 45% glass reinforced flame retardant lubricated high performance polyamide resin that has been devel.. |
|||
Density | 1.76 g/cc | 0.0636 lb/in³ | ASTM D792 |
Applied Composites 8049 Polyester SMC Industry Application: High StrengthProduct Application: MilitaryDistinct Features: High Impact Low Profile; Paintable/In Mold Coatable; Low Shrink; Low Moisture Absorption; Bondable; Formulated for .. |
|||
Density | 1.76 g/cc | 0.0636 lb/in³ | ISO 1183 |
3M Dyneon™ PVDF 31508/0001 Polyvinylidene Fluoride
(discontinued **) Copolymer of VF2 and CTFEUltra-flexibleVery low shrinkage ratesWide operating temperature windowProcessable using a variety of thermoplastic conversation techniquesInformation provided by Dyneon, A .. |
|||
Density | 1.76 g/cc | 0.0636 lb/in³ | ISO 1183 |
3M Dyneon™ PVDF 32008/0003 Polyvinylidene Fluoride
(discontinued **) Copolymer of VF2 and CTFEUltra-flexibleVery low shrinkage ratesWide operating temperature windowProcessable using a variety of thermoplastic conversion techniquesExcellent low flame and low smoke pe.. |
|||
Density | 1.76 g/cc | 0.0636 lb/in³ | DAM; ISO 1183 |
DuPont Performance Polymers Zytel® HTN FR52G45BL BK337 Polyphthalamide (PPA)
(Unverified Data**) Zytel® HTNFR52G45BL BK337 is a 45% glass reinforced, flame retardant, lubricated high performance polyamide resin that has been developed for connector applications.Information provided by DuPont .. |